Please wait a minute...
金属学报    DOI: 10.11900/0412.1961.2025.00110
  本期目录 | 过刊浏览 |
合金元素对 Co-Ti 基高温合金相界面行为的影响
王俊儒1,2,马庆爽1,2,朱洪涛3,李会军3,高傲雪1,2,宫明龙1,2,高秋志1,2

1 东北大学 材料科学与工程学院  沈阳 110819

2 东北大学秦皇岛分校 资源与材料学院  秦皇岛066004

3 Faculty of Engineering and Information Sciences, University of Wollongong, Wollongong, NSW 2522, Australia

Effect of alloying elements on phase interface behavior in Co-Ti based superalloys

WANG Junru 1,2, MA Qinshuang 1,2, ZHU Hongtao 3, LI Huijun 3, GAO Aoxue 1,2, GONG Minglong 1,2, GAO Qiuzhi 1,2

1 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China

2 School of Resources and Materials, Northeastern University at Qinhuangdao, Qinhuangdao 066004, China

3 Faculty of Engineering and Information Sciences, University of Wollongong, Wollongong, NSW 2522, Australia

引用本文:

王俊儒 马庆爽 朱洪涛 李会军 高傲雪 宫明龙 高秋志. 合金元素对 Co-Ti 基高温合金相界面行为的影响[J]. 金属学报, DOI: 10.11900/0412.1961.2025.00110.

全文: PDF(7664 KB)  
摘要: 新型钴基高温合金的力学性能和高温稳定性在很大程度上依赖于析出相与基体之间的界面特性。本文通过第一性原理计算,系统研究了合金元素对L12-γ′/γ 和 D019-χ/γ 两类相界面演化行为的影响。明确了了合金元素在相界面附近的优先析出位置,并全面评估了其对析出相成核与生长的影响。研究结果表明,Mo 和 Ta 能显著增强析出相与基体之间界面的稳定性。相比之下,Al 和 Ni 的添加则倾向于削弱界面强度,抑制D019-χ相形核。电荷分析结果显示,合金元素掺杂对界面强度的增强主要源于其提高了界面金属键的强度。此外,研究还考察了不同合金元素对扩散行为的影响,并通过实验加以验证。上述研究成果为开发具有优异性能的新型钴基高温合金提供了重要理论依据。
关键词 钴基高温合金γ′相χ相界面稳定性元素扩散    
Abstract:The mechanical properties and thermal stability of novel Co-based superalloys are critically dependent on the interface characteristics between precipitates and matrix. The influence of alloying elements on the evolutions of L12-γ′/γ and D019-χ/γ interfaces was systematically investigated by first-principles calculations. The preferred precipitation sites of alloying elements near the phase interface were identified, and their effects on nucleation and growth of precipitates were comprehensively evaluated. The results demonstrate that Mo and Ta significantly enhance the stability of interface between precipitates and matrix. In contrast, the addition of Al and Ni tends to weaken the stability of interface and inhibit D019-χ phase nucleation. The charge analysis reveals that the strengthening effect of alloying element doping on interfacial strength is primarily attributed to the enhancement of metal bond strength across the interface. Furthermore, the impact of various alloying elements on diffusion behavior was also examined and experimentally verified. These findings provide valuable insights for the development of novel Co-based superalloys with superior performance.
Key wordsCo-based superalloys    γ′ phase    χ phase    interfacial stability    elements diffusion
收稿日期: 2025-04-14     
ZTFLH:  TG132.3  
基金资助:国家自然科学基金;国家自然科学基金;国家自然科学基金;驻冀高校与石家庄市产学研合作项目;中央高校基本科研业务费
[1] 郭星星, 帅美荣, 楚志兵, 李玉贵, 谢广明. 不锈钢复合钢筋近界面微观组织演变及元素扩散动力学[J]. 金属学报, 2025, 61(2): 336-348.
[2] 冯强, 路松, 李文道, 张晓瑞, 李龙飞, 邹敏, 庄晓黎. γ' 相强化钴基高温合金成分设计与蠕变机理研究进展[J]. 金属学报, 2023, 59(9): 1125-1143.
[3] 陈佳, 郭敏, 杨敏, 刘林, 张军. 新型钴基高温合金中W元素对蠕变组织和性能的影响[J]. 金属学报, 2023, 59(9): 1209-1220.
[4] 刘兴军, 魏振帮, 卢勇, 韩佳甲, 施荣沛, 王翠萍. 新型钴基与Nb-Si基高温合金扩散动力学研究进展[J]. 金属学报, 2023, 59(8): 969-985.
[5] 李赛, 杨泽南, 张弛, 杨志刚. 珠光体-奥氏体相变中扩散通道的相场法研究[J]. 金属学报, 2023, 59(10): 1376-1388.
[6] 沈莹莹, 张国兴, 贾清, 王玉敏, 崔玉友, 杨锐. SiCf/TiAl复合材料界面反应及热稳定性[J]. 金属学报, 2022, 58(9): 1150-1158.
[7] 王超, 张旭, 王玉敏, 杨青, 杨丽娜, 张国兴, 吴颖, 孔旭, 杨锐. SiCf/Ti65复合材料界面反应与基体相变机理[J]. 金属学报, 2020, 56(9): 1275-1285.
[8] 濮晟, 王莉, 谢光, 丁贤飞, 楼琅洪, 冯强. 缺口取向和再结晶对一种定向凝固钴基高温合金热疲劳性能的影响[J]. 金属学报, 2015, 51(4): 449-457.
[9] 吴铭方, 匡泓锦, 王凤江, 林红香, 胥国祥. Zr/Cu/Zr部分瞬间液相焊扩散连接Ti(C, N)-Al2O3陶瓷基复合材料*[J]. 金属学报, 2014, 50(5): 619-625.
[10] 张旭 王玉敏 雷家峰 杨锐. SiCf/TC17复合材料界面热稳定性及元素扩散机理[J]. 金属学报, 2012, 48(11): 1306-1314.
[11] 杨富民; 孙晓峰; 管恒荣; 胡壮麒 . K40S钻基高温合金的高温低周疲劳行为Ⅰ.疲劳性能[J]. 金属学报, 2002, 38(10): 1047-1052 .
[12] 杨富民; 孙晓峰; 管恒荣; 胡壮麒 . K40S钻基高温合金的高温低周疲劳行为Ⅱ.疲劳断口分析[J]. 金属学报, 2002, 38(10): 1053-1056 .
[13] 杨富民; 孙晓峰; 康煜平; 管恒荣; 胡壮麒 . K40S合金高温时效过程中二次碳化物的沉淀析出行为[J]. 金属学报, 2001, 37(3): 253-257 .
[14] 袁超; 王铁利 . 返回料添加比例对铸造钴基高温合金K640S组织与性能的影响[J]. 金属学报, 2000, 36(9): 961-965 .
[15] 姜文辉;姚向东;管恒荣;胡壮麒. DZ40M合金高温低周疲劳性能及其断口分析[J]. 金属学报, 1998, 34(4): 378-383.