| SYNTHESIS OF NANOMETER ALUMINIUM NITRIDE POWDER BY MICROWAVE METHOD |
| DAI Changhong; ZHANG Xianpeng(Notheastern University;Shenyang 110006);ZHANG Jinsong; YANG Youjin; CAO Lihua; XIA Fei(Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
DAI Changhong; ZHANG Xianpeng(Notheastern University;Shenyang 110006);ZHANG Jinsong; YANG Youjin; CAO Lihua; XIA Fei(Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015). SYNTHESIS OF NANOMETER ALUMINIUM NITRIDE POWDER BY MICROWAVE METHOD. Acta Metall Sin, 1996, 32(11): 1221-1226.
|
|
|
Abstract Nanometer aluminum nitride powder synthesized by microwave heating is described in this paper. Aluminum nitride powder which purity is higher than 98% has been obtained by microwave heating the mixture of Al(OH)3 and carbon powder. The character of the nanometer powder is determined by means of XRD, TEM. The effects of temperature and carbon type on the fomiation of nanometer powder are discussed. Correspondent: DAI Changhong, Advanced Ceramics Department, Qingdao Institute of Chemical Technology, Qingdao 266042
|
|
Received: 18 November 1996
|
| 1SheppardLM.AmCeramSocBull,1990;69:18012李凝芳,周毅,材料导报,1994;2:383PatilDS,MutsuddyBC,GavulicJ,DahimeneM.CeramTrans,1991;21:3014黄莉萍,黄熊璋,符锡仁,沈宝珍.硅酸盐学报,1986,14:3325ForslundB,ZhengJ.JMaterSci,1993;28:3125 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|