Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (11): 1227-1232    DOI:
Current Issue | Archive | Adv Search |
THERMAL DIFFUSIVITY OF SELF-BAKING CARBON BLOCK WITH DIFFERENT GRAPHITIZATION DEGREES
XUE Xiangxin (Northeastern University; Shenyang 110006); HUANG Xiaoyu (Ironmaking Works; Anshan Iron and Steel Complex; Anshan 114021); DU Yingmin(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015); ZHANG Dianyou(Ironmaking Works; Anshan Iron and Steel Complex;Anshan 114021)
Cite this article: 

XUE Xiangxin (Northeastern University; Shenyang 110006); HUANG Xiaoyu (Ironmaking Works; Anshan Iron and Steel Complex; Anshan 114021); DU Yingmin(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015); ZHANG Dianyou(Ironmaking Works; Anshan Iron and Steel Complex;Anshan 114021). THERMAL DIFFUSIVITY OF SELF-BAKING CARBON BLOCK WITH DIFFERENT GRAPHITIZATION DEGREES. Acta Metall Sin, 1996, 32(11): 1227-1232.

Download:  PDF(359KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Thermal diffusivity, α, of self-baking carbon block with different graphitization degrees was determined experimentally by means of laser-pulse within temperature range of 200—1100℃. The results show that the higher is the graphitization degree of carbon blocks, the higher is thermal diffusivity, α, at a given temperature; and α is decreased with the increment of temperature at a given graphitization degree. Resistance to thermal shock, R, of the carbon blocks was discussed from the experimental results. Correspondent: XUE Xiangxin, associate professor, Post Box 313, Department of Metallurgy, NortheasternUniversity, Shenyang 110006
Key words:  thermal diffusivity      self-baking carbon block      graphitization degree      resistance to thermal shock      laser pulse     
Received:  18 November 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I11/1227

1郝运中,陈前婉.炼铁,1994;13(增刊):72HaoYZ,ChenQW.Chian'sRefractories,1994;1:93张殿有,肖亦芹,郝运中,陈前婉.炼铁,1994;13(增刊):284何冠虎,叶庆和,邸忠起,周本濂.工程热物理学报,1981,2:2835何冠虎,叶庆和,董淑清,邸忠起,周本濂.工程热物理学报,1983;4:1686黄晓煜.东北大学硕士学位论文,19957薛向欣,段培宁,黄晓煜,张殿有.中国科协第二届青年学术年会卫星会议、辽宁省第二届青年学术会议文集,工科分册,大连:大连理工大学出版社,1995:908姚广春.冶金炭素材料性能及生产工艺.北京:冶金工业出版社,1992:1999CarslawHS,JeagerJC.ConductionofHeatinSolids.2nded.,London:OxfordPress,1959:101
[1] CAI Hui WANG Fei WANG Yaping SONG Xiaoping DING Bingjun. FABRICATION OF Cu/Si COMPOSITES ON SOL–GEL PRETREATED Si POWDERS[J]. 金属学报, 2009, 45(10): 1261-1266.
[2] HU Xiaojun (Department of Physicochemistry; University of Science and Technology; Beijing 100083)XUE Xiangxin; DUAN Peining (School of Materials and Metallurgy; Northeastern University; Shenyang 110006)HUANG Xiaoyu(Ironmaking Work; Anshan Iron & Steel Company; Anshan 114021). PERMEATION PROCESS OF MOLTEN IRON IN A SELF-BAKING CARBON BLOCK[J]. 金属学报, 1998, 34(4): 384-387.
[3] XUE Xiangxin; CHE Yinchang (Northeastern University; Shenyang 110006)DU Yingmin (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)HUANG Hiaoyu (Ironmaking Works; Anshan Iron and Steel Company; Anshan 114012). DETERMINATION OF ENTHALPY AND MASSIC HEAT CAPACITY OF SELF-BAKING CARBON BLOCK[J]. 金属学报, 1996, 32(6): 669-672.