SYNTHESIS OF NANOMETER ALUMINIUM NITRIDE POWDER BY MICROWAVE METHOD
DAI Changhong; ZHANG Xianpeng(Notheastern University;Shenyang 110006);ZHANG Jinsong; YANG Youjin; CAO Lihua; XIA Fei(Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

DAI Changhong; ZHANG Xianpeng(Notheastern University;Shenyang 110006);ZHANG Jinsong; YANG Youjin; CAO Lihua; XIA Fei(Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015). SYNTHESIS OF NANOMETER ALUMINIUM NITRIDE POWDER BY MICROWAVE METHOD. Acta Metall Sin, 1996, 32(11): 1221-1226.

Download:  PDF(464KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Nanometer aluminum nitride powder synthesized by microwave heating is described in this paper. Aluminum nitride powder which purity is higher than 98% has been obtained by microwave heating the mixture of Al(OH)3 and carbon powder. The character of the nanometer powder is determined by means of XRD, TEM. The effects of temperature and carbon type on the fomiation of nanometer powder are discussed. Correspondent: DAI Changhong, Advanced Ceramics Department, Qingdao Institute of Chemical Technology, Qingdao 266042
Key words:  microwave method      AlN      nanometer powder     
Received:  18 November 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I11/1221

1SheppardLM.AmCeramSocBull,1990;69:18012李凝芳,周毅,材料导报,1994;2:383PatilDS,MutsuddyBC,GavulicJ,DahimeneM.CeramTrans,1991;21:3014黄莉萍,黄熊璋,符锡仁,沈宝珍.硅酸盐学报,1986,14:3325ForslundB,ZhengJ.JMaterSci,1993;28:3125
[1] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[2] Zhengguan LU,Jie WU,Lei XU,Xiaoxiao CUI,Rui YANG. Ring Rolling Forming and Properties of Ti2AlNb Special Shaped Ring Prepared by Powder Metallurgy[J]. 金属学报, 2019, 55(6): 729-740.
[3] Yongyong GONG, Shumin CHENG, Yuyi ZHONG, Yunhu ZHANG, Qijie ZHAI. The Solidification Technology of Pulsed Magneto Oscillation[J]. 金属学报, 2018, 54(5): 757-765.
[4] Xiaoyi ZHANG, Hailong SHANG, Bingyang MA, Rongbin LI, Geyang LI. Brazing of Coated Al Foil Filler to AlN Ceramic[J]. 金属学报, 2018, 54(4): 575-580.
[5] Baiyang LOU,Yuxing WANG. EFFECTS OF Mo CONTENT ON THE MICRO-STRUCTURE AND TRIBOLOGICAL PROPERTIES OF CrMoAlN FILMS[J]. 金属学报, 2016, 52(6): 727-733.
[6] PAN Tao, WANG Xiaoyong, SU Hang, YANG Caifu. EFFECT OF ALLOYING ELEMENT Al ON HARDENABILITITY AND MECHANICAL PROPERTIES OF MICRO-B TREATED ULTRA-HEAVY PLATE STEELS[J]. 金属学报, 2014, 50(4): 431-438.
[7] SHEN Jun, FENG Aihan. RECENT ADVANCES ON MICROSTRUCTURAL CONTROLLING AND HOT FORMING OF Ti2AlNb-BASED ALLOYS[J]. 金属学报, 2013, 49(11): 1286-1294.
[8] . HIGH TEMPERATURE OXIDATION RESISTANCE AND MECHANICAL PROPERTIES OF NiCrAlY/Al--Al2O3 COATINGS ON AN ORTHORHOMBIC Ti2AlNb ALLOY[J]. 金属学报, 2012, 48(5): 579-586.
[9] DONG Yuliang YAN Xubo ZHAO Shengsheng GONG Jun SUN Chao. PREPARATION OF (Ti, Al)N/Ti2AlN COATINGS[J]. 金属学报, 2010, 46(6): 743-747.
[10] YANG Rui HAO Yulin Obbard E G DONG Limin LU Bin. ORTHORHOMBIC PHASE TRANSFORMATIONS IN TITANIUM ALLOYS AND THEIR APPLICATIONS[J]. 金属学报, 2010, 46(11): 1443-1449.
[11] YANG Mocong LIN Xin XU Xiaojing CHEN Jing HUANG Weidong. MICROSTRUCTURE AND PHASE EVOLUTION IN Ti60--Ti2AlNb GRADIENT MATERIAL PREPARED BY LASER SOLID FORMING[J]. 金属学报, 2009, 45(6): 729-736.
[12] LIN Xin; LV Xiaowei LV; Jing Chen; Weidong Huang. RESEARCH ON LASER SOLID FORMING OF A FUNCTIONALLY GRADED TI-TI2ALNB ALLOY[J]. 金属学报, 2008, 44(8): 1006-1012 .
[13] CUI Chunxiang; WU Renjie; YANG Chunsheng(Shanghai Jiaotong University.Shanghai 200030)(Manuscript received 1 995-07- 1 7; in revised form 1 995-10-04). IN SITU FORMATION AND DISTRIBUTION OF TiC WHISKERS IN TiC_w-AlN_p/ AI COMPOSITE[J]. 金属学报, 1996, 32(3): 323-327.
[14] YU Xifeng; CHENG Lizhi; HU Huosheng; LIU Xiang; HU Zhuangqi (State Key Laboratory for RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)( Northeastern University; Shenyang 110006)(Manuscript received 1995-04-12; in revised form 1995-09-11). PREPARATION OF NANOMETER POWDER BY ELECTROHYDRODYNAMIC TECHNIQUE[J]. 金属学报, 1996, 32(1): 75-79.
[15] LIAO Bo; WANG Tiansheng; YANG Ke; YUAN Hui; XIAO Furen;LI Yiyi(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Yanshan University; Qinhuangdao 066004). EFFECT OF THERMOCHEMICAL PROCESSING WITH HYDROGEN ON MICROSTRUCTURE OF SUPER-α2 ALLOY[J]. 金属学报, 1995, 31(5): 223-228.
No Suggested Reading articles found!