INFLUENCE OF CARBIDE STABILITY ON WEAR RESISTANCE OF ALLOY AT ELEVATED TEMPERATURE
WU Wenzhong; XING Jiandong;SU Junyi(Xi'an Jiaotong University; Xi'an 710049)
Cite this article: 

WU Wenzhong; XING Jiandong;SU Junyi(Xi'an Jiaotong University; Xi'an 710049). INFLUENCE OF CARBIDE STABILITY ON WEAR RESISTANCE OF ALLOY AT ELEVATED TEMPERATURE. Acta Metall Sin, 1997, 33(10): 1075-1078.

Download:  PDF(884KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of the stability of eutectic carbide in high Cr-Ni cast iron on abrasive wear resistance has been investigated on a high temperature abrasive wear tester, in which atmosphere can be controlled. The obtained results show that the carbide can not act as a resistant to wear if its chemical stability at elevated temperature is too bad, and the wear resistance of the alloy is decreased rapidly.
Key words:  high temperature abrasive wear      carbide      chemical stability     
Received:  18 October 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I10/1075

1邢建东,周庆德,赵学增.磨擦学学报,1993;13(2):153
2Tien J K, ansell G S. alloy and Microstructural Design. London: academic press INC LTD 1983:379
3张安峰,邢建东,陆文华.金属学报,1993;28:B263
4解荣军,武文忠,邢建东,王恩泽.机械工程学报.1997;33
5武文忠,邢建东,苏俊义磨炼学学报(待发表)
[1] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[2] LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong. Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel[J]. 金属学报, 2022, 58(8): 1024-1034.
[3] HE Shuwen, WANG Minghua, BAI Qin, XIA Shuang, ZHOU Bangxin. Effect of TaC Content on Microstructure and Mechanical Properties of WC-TiC-TaC-Co Cemented Carbide[J]. 金属学报, 2020, 56(7): 1015-1024.
[4] YANG Ke,LIANG Ye,YAN Wei,SHAN Yiyin. Preferential Distribution of Boron and its Effect on Microstructure and Mechanical Properties of (9~12)%Cr Martensitic Heat Resistant Steels[J]. 金属学报, 2020, 56(1): 53-65.
[5] LI Jiarong,XIE Hongji,HAN Mei,LIU Shizhong. High Cycle Fatigue Behavior of Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1195-1203.
[6] Futao DONG,Fei XUE,Yaqiang TIAN,Liansheng CHEN,Linxiu DU,Xianghua LIU. Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel[J]. 金属学报, 2019, 55(6): 792-800.
[7] HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. 金属学报, 2019, 55(12): 1487-1494.
[8] Tao ZHANG, Wei YAN, Zhuoming XIE, Shu MIAO, Junfeng YANG, Xianping WANG, Qianfeng FANG, Changsong LIU. Recent Progress of Oxide/Carbide Dispersion Strengthened W-Based Materials[J]. 金属学报, 2018, 54(6): 831-843.
[9] Xirong LIU, Kai ZHANG, Shuang XIA, Wenqing LIU, Hui LI. Effects of Triple Junction and Grain Boundary Characters on the Morphology of Carbide Precipitation in Alloy 690[J]. 金属学报, 2018, 54(3): 404-410.
[10] Shenghu CHEN, Lijian RONG. Microstructure Evolution During Solution Treatment and Its Effects on the Properties of Ni-Fe-Cr Alloy[J]. 金属学报, 2018, 54(3): 385-392.
[11] Yubin DU, Xiaofeng HU, Haichang JIANG, Desheng YAN, Lijian RONG. Effect of Tempering Time on Carbide Evolution and Mechanical Properties in a Fe-Cr-Ni-Mo High-Strength Steel[J]. 金属学报, 2018, 54(1): 11-20.
[12] Bo CHEN, Xianchao HAO, Yingche MA, Xiangdong CHA, Kui LIU. Effects of Nitrogen Addition on Microstructure and Grain Boundary Microchemistry of Inconel Alloy 690[J]. 金属学报, 2017, 53(8): 983-990.
[13] Dawei WANG,Shichao XIU. Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint[J]. 金属学报, 2017, 53(5): 567-574.
[14] Dexin MA, Fu WANG, Xuhui WEN, Dejian SUN, Lin LIU. Influence of MC Carbides on the Formation of γ/γ′ Eutectics in Single Crystal Superalloy CM247LC[J]. 金属学报, 2017, 53(12): 1603-1610.
[15] Yingche MA,Shuo LI,Xianchao HAO,Xiangdong ZHA,Ming GAO,Kui LIU. RESEARCH ON THE CARBIDE PRECIPITATION AND CHROMIUM DEPLETION IN THE GRAIN BOUNDARY OF ALLOY 690 CONTAINING DIFFERENT CONTENTS OF NITROGEN[J]. 金属学报, 2016, 52(8): 980-986.
No Suggested Reading articles found!