| ESTIMATION OF COMPONENT ACTIVITIES IN MULTICOMPONENT LIQUID ALLOYS AT GIVEN TEMPERATURES USING WILSON EQUATION |
| TAO Dongping;YANG Xianwan (Kunming University of Science and Technology;Kunming 650093) |
|
Cite this article:
TAO Dongping;YANG Xianwan (Kunming University of Science and Technology;Kunming 650093). ESTIMATION OF COMPONENT ACTIVITIES IN MULTICOMPONENT LIQUID ALLOYS AT GIVEN TEMPERATURES USING WILSON EQUATION. Acta Metall Sin, 1997, 33(10): 1079-1084.
|
|
|
Abstract Based on the relationship between the Wilson parameters and temperature,the Wilson equation can be extended to estimating activities of components of binary and multicomponent liquid alloys at given temperatures only by using the activities of components of binary liquid alloys measured at some temperatures. The results show that the estimation values of activity of multicomponent liquid alloys are in good agreement with their experimental data of activity.
|
|
Received: 18 October 1997
|
1 Wilson G M.J amer Chem Soc,1964;86:127 2陶东平.金属学报,1991;27:B380 3Tao D P. Metall Trans B 1992; 23B(4):526 4陶东平.有色金属,1993;45(3):59 5Orye R V,Prausnitz J M, Indu Eng Chem,1965;57(5 ):18 6Hultgren R Desai P D, Hawkins D T Geiser M, Kelley K K. Selected Values of the Thermodynamic Properties of Binary alloys,Metals Park,Ohio:aSM,1973:1963 7Dealy J M,Pehlke R D Trans Metall Soc aIME 1963; 227:1030 8Lucas L D.In:Rapp R a eds,Physicochemical Measurements in Metals Research New York:JohnWiley& Sons, Inc, 1970: 219 9 MoserZ,Gasior W,Panek Z.Metall Trans B,1984;B15:543 10Moser Z Zakulski W, Jedrzejek C Z Metallkde, 1979;70:293 11 Ptak W,Moser Z.Trans Metall Soc aIME,1968;242:558 12 Prausnitz J M, Lichtenthaler R N, de azevedo E G. Molecuhr Thermodynamics of Fluid-PhaseEquilibria.2nd ed,Englewood Cliffis N J:Prentice—Hall Inc,1986:234 13 Walas S M著,韩世钩等译。化工相平衡北京:中国石化出版社,1991:221 |