| MICROSTRUCTURE AND MAGNETISM OF[Co/Ti] AND [Co/Cu(Ni)] MULTILAYERS |
| WU Ping;JIANG Enyong; WANG Cunda; BAI Haili; LIU Yuguang; WANG Heying(Tian jin University; Tianjin; 300072) |
|
Cite this article:
WU Ping;JIANG Enyong; WANG Cunda; BAI Haili; LIU Yuguang; WANG Heying(Tian jin University; Tianjin; 300072). MICROSTRUCTURE AND MAGNETISM OF[Co/Ti] AND [Co/Cu(Ni)] MULTILAYERS. Acta Metall Sin, 1997, 33(6): 625-630.
|
|
|
Abstract Two series of the multilayers with the forms of [Co/Ti]30 and[Co / Cu(Ni)]30 prepared by dual facing target sputtering at room temperature, consist ofamorphous Co magnetic layer and exhibit soft magnetic properties. The structural and magnetic properties of [Co/Cu(Ni)] and [Co/Ti] multilayers were examined as a function of thespacer layer thickness (dTi and dCu(Ni)) by XRD, TEM and VSM measurements. The saturation magnetization Ms of the [Co/Ti] multilayer was found to decrease with dTi, but for the[Co/Cu(Ni)] multilayers, the Ms was found to oscillate with dCu(Ni). The Ms approached toa constant value when dTi and dCu(Ni) thickened enough. This is the result of differentinterlayer magnetic coupling effects.
|
|
Received: 18 June 1997
|
1 Parkin S S P,More N,Roche K P.Phys Rev Lett,1990;64:2304 2Barthelemy A,Fert A,Baibich M N,HadjoudjS,Petroff F.J Appl Phys,1990;67:5908 3 Parkin S S P,Bhadra R,Roche K P.Phys Rev Lett,1991;66:2152 4 Inomata K,Yusu K,Saito Y.Mater Sci Eng,1995;B31:41 5Qiu Z Q,Pearson J,Berger A,Bader S D.Phys Rev Lett,1992;68:1398 6 Fub A,Demokritov S,Grunberg P.J Magn Magn Mater,1992:103:L221 7Liu Y H, Zhang Y M,Yan S S, Ma X D. Phys Rev, 1993; B48: 10266 8 Shi Z P and Klein B M.Phys Rev,1995;B52:12516 9Bobo J F,Hennet b,Piecuch M.J Magn Magn Mater,1995;140-144:587 10 Bruno P,Chappert C.Phys Rev Lett.1991;67:1602 11 XU Y B, Lu M, Bie Q S, Zhai Y, Jin Q Y, Zhu X B, Zhai H R. J Magn Magn Mater, 1995;140—144: 581 12 Fabian D T. Band structure spectroscopy ofmetals and alloys.London: Academic Press, 1973: 63,679 13 Leevwen R V,England C D,Dutcher J R,Falco C M.J Appp Phys,1990;67:4910F |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|