MORPHOLOGIES OF (Al,Ag)_3Ti AND Ti_3AlC PRECIPITATES IN Ll_0-TiAl INTERMETALLIC COMPOUND
TIAN Wenhuai;YANG Haichun (Universily of Science and Technology Beijing; Beij ing 100083); NEMOTO Minoru (Kyushu University; Japan)
Cite this article:
TIAN Wenhuai;YANG Haichun (Universily of Science and Technology Beijing; Beij ing 100083); NEMOTO Minoru (Kyushu University; Japan). MORPHOLOGIES OF (Al,Ag)_3Ti AND Ti_3AlC PRECIPITATES IN Ll_0-TiAl INTERMETALLIC COMPOUND. Acta Metall Sin, 1997, 33(7): 677-682.
Abstract A trasmission electron microscopy (TEM) investigation has been performed on the moerphologies of Ll2-(Al,Ag),Ti and Ti3AIC precipitates in Ll0-ordered TiAl(Ag). During aging at temperatures around 1073 K after quenching from 1473 K, TiAl(Ag) hardens by the precipitation of (Al,Ag)3Ti and Ti3AIC. TEM observations revealed that plate-like precipitates (Al,Ag)3Ti lie on (001) plane of TiAl(Ag) matrix and needle--like pricipitates Ti3AlC, which lie only in one direction parallel to the [001] axis of the TiAl(Ag) matrix, appear after longer period aging or higher temperature aging. The anisotropic misfits between TiAl matrix and Ll2-(Al,Ag)3Ti and Ti3AIC can be considered to explain the morphologies of (Ag,Al)3Ti and Ti3AIC precipitates.
1 Kim Y W,DimidukDM.In:HosoiY,YoshlnagaH,Oikawa H,Maruyama K eds,Aspects of High Temperature De formation and Fracture in Crystalline Materials, Proc 7th JIM Int Symp, TheJapan Institute of Metals,Sendal,1993:373 2 DahmsM,Seeger J,SmarslyW,Wildhagen B.ISIJ Int,1991;31:1093 3结城 勇,天野宪 鱼住 稔,乾 晴行,山口正治.日本金属学会志,1994;58:564 4Mabuchi H,Hirukawa K,KatayamaK,TsudaH,Nakayama Y.Scr Metall Mater ,1990224:1553 5田文怀,原田浩介,中岛玲司,佐野毅,根本 .日本金属学会志1993;57:1235 6Tian W H,sano T,Nemoto M.Phils Mag 1993;A68:965 7 Keily A, Nlchoson R B. In: Churners B ed, Progress In Malerlals Science, Vol.10, Oxford:Pergamollg 1963: 149 8von Hornbogen E, Roth M. Z Metallk, 1967; 58: 842 9Loomls W T, Freeman J W, Sponseller D J. Metall Trans, 1972; 3: 989 10 SchusterJC,NowotnyH,VaccaroC.JSolidstateChem,1980;32:213