| EFFECT OF IMPURITIES AND Ce ADDITION ON INTRINSIC AND EXTRINSIC TOUGHENING LEVELS OF 8090 Al-Li ALLOY |
| MENG Liang; ZHENG Xiulin (Northwestern Polytechnical University; Xi'an 710072) (Manuscript received 1996-08-26; in revised form 1996-12-02) |
|
Cite this article:
MENG Liang; ZHENG Xiulin (Northwestern Polytechnical University; Xi'an 710072) (Manuscript received 1996-08-26; in revised form 1996-12-02). EFFECT OF IMPURITIES AND Ce ADDITION ON INTRINSIC AND EXTRINSIC TOUGHENING LEVELS OF 8090 Al-Li ALLOY. Acta Metall Sin, 1997, 33(8): 802-806.
|
|
|
Abstract The variability of intrinsic and extrinsic toughening levels has been derived for 8090 Al-Li alloy. The tensile properties and plane stress fracture toughness have been deter-mined for alloy 8090 sheets with various contents of impurities and Ce addition. Impurities Fe, Si and Na, K show an evident behavior to decrease the intrinsic toughening level and the fracture toughness even though the impurities could produce the extrinsic toughening effi-ciency to a certain degree. The intrinsic toughening level could be enhanced but the extrinsic toughening level is reduced by adding minor Ce element into alloy 8090 containing higher concentration of impurities. The intrinsic and extrinsic toughening levels are increased and the fracture toughness improved when the alloy containing higher concentration of impurities is modified by a fixed Ce content.
|
|
Received: 18 August 1997
|
1 Lynch S P. Mater Sci Eng, 1991, A136: 45 2 Blankenship C P, Starke E A. Metall Trans, 1993; 24A: 833 3孟亮,张宝昌,梁英,张卫中,田普科.金属学报,1992;28:A121 4孟亮,耿东生,郑修麟.金属学报,1995;31:A40 5 Meng L, Zheng X L. Scr Metall Mater, 1995; 33: 27 6 Meng L, Zheng X L, Tian L. Mater Sci Eng, 1995, A 196: 191 7孟亮.西北工业大学学报, 1993;11: 389 8 Zheng X L. Eng Fract Mech, 1989; 33: 685 9 Liu Y L, Hu Z Q, Zhang Y, Shi C X. Metall Trans, 1993; 24B: 857 10 Webster D. Metall Trans, 1987, 18A: 2181 |