3D TOPOGRAPHY OF FRACTURED SURFACES AND MECHANICAL PROPERTIES UNDER INSTRUMENTED IMPACT LOADING
ZHU Ping;CHEN Bingsen (Department of Mechanical Engineering; Tsinghua University; Beijing 100084)
Cite this article: 

ZHU Ping;CHEN Bingsen (Department of Mechanical Engineering; Tsinghua University; Beijing 100084). 3D TOPOGRAPHY OF FRACTURED SURFACES AND MECHANICAL PROPERTIES UNDER INSTRUMENTED IMPACT LOADING. Acta Metall Sin, 1998, 34(1): 63-69.

Download:  PDF(1128KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The dynamic fracture properties of P460NLl steel were tested under instrumented impact loading at different test temperatures. The 3D topography of fractured surfaces was reconstructed and quantified by the means of SEM stereo pairs, image processing and analysis, and computer vision. It was shown that measured 3D roughness indexes Rs, Rq and Rmax have good positive relations to the crack propagation part of absorbed impact energy. Although fractal behavior had been checked out on the fractured surfaces, the fractal dimension was found nonsensitive to the fracture mode and mechanical properties. The geometric characteristics of fractal fractured surfaces should be quantified in fractal dimension together with absolute parameters.
Key words:  quantitative fractography      instrumented impact test      3D topography      roughness      fractal      fracture property     
Received:  18 January 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I1/63

1 Coster M,Chermant J L.Int Metals Rev,1983;28:228
2 朱平,陈丙森.电子显微学报,19972 16(1):49(Zhu Ping,Chen Bingsen.J Chin Electron Microsc Soc,1997; 16(1): 49)
3 Pande C S,Richards L E,Dempsey B D,Schwoeble A J.Acta Metall,1987; 35: 1633
4 朱平.陈丙森,唐伟中国体视学与图像分析,1997;2(1):1(Zhu Ping,Chen Bingsen,Tang Wei.Chin J Sterol Imag Analys,1997;2(1):1)
5 Davidson D L J Mater Sci,1989;24:681
6 Russ J C Fractal Surfaces.New York:Plenum Press,994:73
[1] YANG Du, BAI Qin, HU Yue, ZHANG Yong, LI Zhijun, JIANG Li, XIA Shuang, ZHOU Bangxin. Fractal Analysis of the Effect of Grain Boundary Character on Te-Induced Brittle Cracking in GH3535 Alloy[J]. 金属学报, 2023, 59(2): 248-256.
[2] SONG Wenshuo, SONG Zhuman, LUO Xuemei, ZHANG Guangping, ZHANG Bin. Fatigue Life Prediction of High Strength Aluminum Alloy Conductor Wires with Rough Surface[J]. 金属学报, 2022, 58(8): 1035-1043.
[3] CAO Jianghai, HOU Zibing, GUO Zhongao, GUO Dongwei, TANG Ping. Effect of Superheat on Integral Morphology Characteristics of Solidification Structure and Permeability in Bearing Steel Billet[J]. 金属学报, 2021, 57(5): 586-594.
[4] ZHANG Conghui, RONG Hua, SONG Guodong, HU Kun. Effect of Surface Roughness by Shot Peening on Stress Corrosion Cracking Behavior of Pure Titanium Welded Joints in HCl Solution[J]. 金属学报, 2019, 55(10): 1282-1290.
[5] GUO Junli, WEN Guanghua, FU Jiaojiao, TANG Ping, HOU Zibing, GU Shaopeng. Influence of Cooling Rate on the Contraction of Peritectic Transformation During Solidification of Peritectic Steels[J]. 金属学报, 2019, 55(10): 1311-1318.
[6] Yajuan ZHANG, Haibin WANG, Xiaoyan SONG, Zuoren NIE. Preparation and Performance of Spherical Ni Powder for SLM Processing[J]. 金属学报, 2018, 54(12): 1833-1842.
[7] Zibing HOU,Jianghai CAO,Yi CHANG,Wei WANG,Han CHEN. Morphology Characteristics of Carbon Segregation in Die Steel Billet by ESR Based on Fractal Dimension[J]. 金属学报, 2017, 53(7): 769-777.
[8] Zheng LIU,Lina XU,Zhaofu YU,Yangzheng CHEN. RESEARCH ON THE MORPHOLOGY AND FRACTALDIMENSION OF PRIMARY PHASE IN SEMISOLIDA356-La ALUMINUM ALLOY BY ELECTRO-MAGNETIC STIRRING[J]. 金属学报, 2016, 52(6): 698-706.
[9] Lina ZHU,Caiyan DENG,Dongpo WANG,Shengsun HU. EFFECT OF SURFACE ROUGHNESS ON VERY HIGH CYCLE FATIGUE BEHAVIOR OF Ti-6Al-4V ALLOY[J]. 金属学报, 2016, 52(5): 583-591.
[10] Zheng LIU,Jiayi ZHANG,Haolin LUO,Keyue DENG. RESEARCH ON MORPHOLOGY EVOLUTION OF PRIMARY PHASE IN SEMISOLID A356 ALLOY UNDER CHAOTIC ADVECTION[J]. 金属学报, 2016, 52(2): 177-183.
[11] Bin WANG,Liangyin XIONG,Shi LIU. MgO SECONDARY ELECTRON EMISSION FILM PREPARED BY RADIO-FREQUENCY REACTIVE SPUTERRING[J]. 金属学报, 2016, 52(1): 10-16.
[12] WU Xiaojun CHENG Wen QIAO Shengru ZOU Wu ZHANG Peng ZHANG Xiaohu. EVOLUTION OF PORES IN C/C COMPOSITE DURING RESIN IMPREGNATION-CARBONIZATION[J]. 金属学报, 2009, 45(11): 1402-1408.
[13] ZHAO DaWen LI Jinfu. PHASE–FIELD SIMULATION OF THE EFFECT OF KINETIC ANISOTROPY ON CRYSTAL GROWTH IN UNDERCOOLED MELTS[J]. 金属学报, 2009, 45(10): 1237-1241.
[14] Jicheng He. Monte-Carlo Simulation for Fractal Growth of inclusions in the Continuous Casting Mold[J]. 金属学报, 2008, 44(6): 698-702 .
[15] . FRACTAL ANALYSIS OF TEMPERATURE-INDUCED DISCONTINUOUS LIQUID STRUCTURAL CHANGE[J]. 金属学报, 2006, 42(12): 1259-1261 .
No Suggested Reading articles found!