| 3D TOPOGRAPHY OF FRACTURED SURFACES AND MECHANICAL PROPERTIES UNDER INSTRUMENTED IMPACT LOADING |
| ZHU Ping;CHEN Bingsen (Department of Mechanical Engineering; Tsinghua University; Beijing 100084) |
|
Cite this article:
ZHU Ping;CHEN Bingsen (Department of Mechanical Engineering; Tsinghua University; Beijing 100084). 3D TOPOGRAPHY OF FRACTURED SURFACES AND MECHANICAL PROPERTIES UNDER INSTRUMENTED IMPACT LOADING. Acta Metall Sin, 1998, 34(1): 63-69.
|
|
|
Abstract The dynamic fracture properties of P460NLl steel were tested under instrumented impact loading at different test temperatures. The 3D topography of fractured surfaces was reconstructed and quantified by the means of SEM stereo pairs, image processing and analysis, and computer vision. It was shown that measured 3D roughness indexes Rs, Rq and Rmax have good positive relations to the crack propagation part of absorbed impact energy. Although fractal behavior had been checked out on the fractured surfaces, the fractal dimension was found nonsensitive to the fracture mode and mechanical properties. The geometric characteristics of fractal fractured surfaces should be quantified in fractal dimension together with absolute parameters.
|
|
Received: 18 January 1998
|
1 Coster M,Chermant J L.Int Metals Rev,1983;28:228 2 朱平,陈丙森.电子显微学报,19972 16(1):49(Zhu Ping,Chen Bingsen.J Chin Electron Microsc Soc,1997; 16(1): 49) 3 Pande C S,Richards L E,Dempsey B D,Schwoeble A J.Acta Metall,1987; 35: 1633 4 朱平.陈丙森,唐伟中国体视学与图像分析,1997;2(1):1(Zhu Ping,Chen Bingsen,Tang Wei.Chin J Sterol Imag Analys,1997;2(1):1) 5 Davidson D L J Mater Sci,1989;24:681 6 Russ J C Fractal Surfaces.New York:Plenum Press,994:73 |
| No Suggested Reading articles found! |
|
|