THREE DIMENSIONAL MORPHOLOGY AND MICROSTRUCTURAL EVOLUTION OF BAINITE
FANG Hongsheng; BO Xiangzheng; WANG Jiajun; XU Ning(Deperment of Materials Science & Engineering; Tsinghua University; Beijing 100084)Correspondent : BO Xiangzheag Fas:(010)62771160; Tel: (010)62782361;E-mail: fhsdms tsinghua edu .cn
Cite this article:
FANG Hongsheng; BO Xiangzheng; WANG Jiajun; XU Ning(Deperment of Materials Science & Engineering; Tsinghua University; Beijing 100084)Correspondent : BO Xiangzheag Fas:(010)62771160; Tel: (010)62782361;E-mail: fhsdms tsinghua edu .cn. THREE DIMENSIONAL MORPHOLOGY AND MICROSTRUCTURAL EVOLUTION OF BAINITE. Acta Metall Sin, 1998, 34(6): 579-585.
Abstract The 3--D morphologies of bainite in steels have been studied by scanning electronmicroscopy (SEM) with high resolution, based on the dual--surface observation. The subplatescomposing uPPer berate sheaf are lath-like while the whole morphology of lower bainite andits subplates are plate--shaped. The subunits in lower bainite seem to be lumpish. There is noobvious difference between upper bainite and lower bainite. Between them elms transient bainite,whose 3--D morphology proves to resemble both opper and lower bainite on some aspects. Themicrostructural evolution of three types of bainite has been interpreted when the sympatheticnucleation ledgewise growth mechanism is employed, and the evolution model has been proposed.
1 Oblak J M, Goodenow R H, Hehemann R F. Trans AIME, 1964; 230: 258 2 Stinivasan G R, Wayman C M. Acta Metall 1968; 16(6): 621 3 Fang H S, Wang J J, Yang Z G, Li C M, Deng X R, Zheng Y K, Yan J J, Yu H B, Li Z G, Huang G. Prog Nat Sci,1994; 4(2):182 4 Wang J J, Fang H S, Yang Z G, Zheng Y K. ISIJ Int, 1995; 35(8): 992 5 方鸿生,杨志刚,王家军,郑蔡康.金属学报,1995;31:A387(Fang H S, Yang Z G, Wang J J, and Zheng Y K, Acta Metall Sin, 1995; 31: A387)6 方鸿生,王家军.金属学报,1994;30:A491(Fang H S, Wang J J. Acta Metall Sin, 1994; 30: A491) 7 方鸿生,王家军.郑燕康,杨志刚.金属学报,1993;29:A445(Fang H S, Wang J J, Zheng Y K, Yang Z G. Acta Mentall Sin 1993; 29: A445) 8 方鸿生,王家军,杨志刚.钢铁研究学报,1997;9(5):45(Fang H S, Wang J J, Yang Z G.J Iron Steel Rea, 1997; 9(5): 45)