Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (7): 689-695    DOI:
Current Issue | Archive | Adv Search |
THE EFFECT OF APPLIED STRESS ORIENTATION ON THE HIGH TEMPERATURE CREEP BEHAIOUR OF DIRECTIONALLY SOLIDIFIED NICKEL BASE SUPERALLOY
YUAN Chao ; GUO Jianting ; WANG Tieli ; YANG Hongcai ; WANG Shuhe ;ZHANG Hao (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Materials and Metallurgy School; Northeastern University; Shenyang 110006)
Cite this article: 

YUAN Chao ; GUO Jianting ; WANG Tieli ; YANG Hongcai ; WANG Shuhe ;ZHANG Hao (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Materials and Metallurgy School; Northeastern University; Shenyang 110006). THE EFFECT OF APPLIED STRESS ORIENTATION ON THE HIGH TEMPERATURE CREEP BEHAIOUR OF DIRECTIONALLY SOLIDIFIED NICKEL BASE SUPERALLOY. Acta Metall Sin, 1998, 34(7): 689-695.

Download:  PDF(2443KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of applied stress orientation on the creep and fracture behaviour of a directionally solidified nickel base superalloy at 980 ℃ in the stress range of 130 - 190 MPa has been studied. The results show that the creep curves of three orientation specimens, in which the grain boundaries are oriented longitudinally, transversely, and 45° to the applied stress axis, have the same shape. In terms of Dorn creep law, three orientation specimens have same creep mechanism, which is controlled by the dislocation climb process. The strain to fracture in longitudinal specimens is much higher than that in transverse and inclined specimens, the reason is the change of creep fracture mechanism from the transgranular to intergranular failure mode.
Key words:  applied stress orientation      directional solidification      nickel base superalloy      high temperature creep      creep fracture     
Received:  18 July 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I7/689

1 Duhl D N. In: Sims C T, Stoloff N S, Hagel W C eds., Superalloy II, New York: Wiley, 1987: 189
2 McLean M. Directionally Solidified Materials for High Tempemture Service. London: The Metals Society,1983: 169
3 Tien J K, Coply S M. Metall Trans, 1971; 2: 543
4 Gell M, Duhl D N. In: Alien S et al eds., Processing and Properties of Advanced High-Temperature Alloys,Metals Park, Ohio: ASM, 1986: 41
5 Caron P, Ohta Y, Nakagawa Y G, Khan T. In: Duhl D N et al eds., Superalloys 1988, Warrendale: TheMetallurgical Society, 1988: 125
6 Volki R, Glatzel U, Feller-Kniepmeier M. Scr Metall Mater, 1994; 31: 1481
7 Mishra K S, Singh S P, Sriramamuythy A M, Pandey M C. Mater Sci Technol, 1995; 11: 341
8 Mukherjee A K, Bird J E, Dorn J E. ASM Trans Q, 1969; 62: 155
9 McLean M. Acta Metall, 1985; 33: 545
10 Davies P W, Wilshire B. Scr Metall, 1971; 5. 475
11 Guo Jianting, Ranucci D, Picco E, Strocchi P M. Metall Trans, 1983; 14A: 2329
12 Williams K R, Wilshire B. Mater Sci Eng, 1977; 28: 289
13 Yuan Chao, Guo Jianting, Yang Hongcai, Wang Shuhe. J Mater Sci Technol, in press
14 Pollok T M, Argon A S. Acta Metall Mater, 1994; 42: 1859
15 Buffiere J Y, Ignet M. Acta Metall Mater, 1995; 43: 1791
[1] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[2] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[3] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[4] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[5] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[6] ZHANG Xiaoli, FENG Li, YANG Yanhong, ZHOU Yizhou, LIU Guiqun. Influence of Secondary Orientation on Competitive Grain Growth of Nickel-Based Superalloys[J]. 金属学报, 2020, 56(7): 969-978.
[7] ZHANG Jian,WANG Li,WANG Dong,XIE Guang,LU Yuzhang,SHEN Jian,LOU Langhong. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2019, 55(9): 1077-1094.
[8] XU Qingyan,YANG Cong,YAN Xuewei,LIU Baicheng. Development of Numerical Simulation in Nickel-Based Superalloy Turbine Blade Directional Solidification[J]. 金属学报, 2019, 55(9): 1175-1184.
[9] Hui FANG,Hua XUE,Qianyu TANG,Qingyu ZHANG,Shiyan PAN,Mingfang ZHU. Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification:[J]. 金属学报, 2019, 55(5): 664-672.
[10] Yan YANG, Guangyu YANG, Shifeng LUO, Lei XIAO, Wanqi JIE. Microstructures and Growth Orientation of Directionally Solidification Mg-14.61Gd Alloy[J]. 金属学报, 2019, 55(2): 202-212.
[11] JIN Hao, JIA Qing, LIU Ronghua, XIAN Quangang, CUI Yuyou, XU Dongsheng, YANG Rui. Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy[J]. 金属学报, 2019, 55(12): 1519-1526.
[12] Lin LIU, Dejian SUN, Taiwen HUANG, Yanbin ZHANG, Yafeng LI, Jun ZHANG, Hengzhi FU. Directional Solidification Under High Thermal Gradient and Its Application in Superalloys Processing[J]. 金属学报, 2018, 54(5): 615-626.
[13] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[14] Jincheng WANG, Chunwen GUO, Junjie LI, Zhijun WANG. Recent Progresses in Competitive Grain Growth During Directional Solidification[J]. 金属学报, 2018, 54(5): 657-668.
[15] Guang CHEN, Gong ZHENG, Zhixiang QI, Jinpeng ZHANG, Pei LI, Jialin CHENG, Zhongwu ZHANG. Research Progress on Controlled Solidificationand Its Applications[J]. 金属学报, 2018, 54(5): 669-681.
No Suggested Reading articles found!