COMPARISON BETWEEN CYCLIC DEFORMATION BEHAVIORS OF NON-ISOAXIAL COPPER TRICRYSTAL AND BICRVSTAL
JIA Weiping; LI Shouxin; WANG Zhongguang; LI Xiaowu; LI Guangyi(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

JIA Weiping; LI Shouxin; WANG Zhongguang; LI Xiaowu; LI Guangyi(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). COMPARISON BETWEEN CYCLIC DEFORMATION BEHAVIORS OF NON-ISOAXIAL COPPER TRICRYSTAL AND BICRVSTAL. Acta Metall Sin, 1998, 34(7): 696-704.

Download:  PDF(3545KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The cyclic hardening and saturation behaviors of copper tricrystal and bicrystal were investigated by using successively increasing amplitude method. The results show that, to the inclined grain boundary bicrystal with single slip components, the cyclic stress strain curve (CSSC) ealsts a plateau or quasi-plateau region, while the CSSC of tricrystal shows no plateau.Observation of surface morphologies indicated that owing to the strain incompatibility of three grains, at lower strain amplitude the triple junction retards obviously the primary slip in grains and makes deformation near it smaller than that near bicrystal junction. The eastness of crack initiation at the same triple junction is closely related to loading direction.
Key words:  copper tricrystal      triple junction      cyclic deformation      plastic strain incompatibility     
Received:  18 July 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I7/696

1 Mughrabi H. Mater Sci Egg, 1978; 33: 207
2 Jin N Y, Winter A T. Acta Metall, 1984; 32: 989
3 Gong Bo, Wang Zhirui, Wang Zhongguang. Acta Mater, 1997; 45: 1365
4 Hu Y M, Wang Z G, Li G Y. Mater Sci Eng, 1996; A208: 260
5 Hu Y M, Wang Z G. Acta Mater, 1997; 45: 2655
6 Liu C D, You D X, Bassim M N. Acta Metall Mater, 1994; 42: 1631
7 Rasmussen K V, Pedersen O B. Acta Metall, 1980; 28: 1467
8 Winter A T, Pedersen O B, Rasmossen K V. Acta Metall, 1981; 29: 735
9 Onaka S, Tajima F, Hashimato S, Miura S. Acta Metall Mater, 1995; 43: 307
10 Randle V. Acta Metall Mater, 1995; 43: 1741
11 Sisanbaev A V, Valley R J. Acta Metall Mater, 1992, 40: 3349
12 Jia Weiping, Li Shouxin, Wang Zhongguang, Li Guangyi. In: Luitjering G, Nowack H eds., Fatigue'96,Proc 6th Int Fatigue Congress, Vol. I, Berlin: Pergamon, 1996: 161
13 Livingston J D, Chalmers B. Acta Metall, 1957; 5: 322
14 Rey C, Zaoui A. Acta Metall, 1980; 28. 687
[1] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[2] CHEN Lei, HAO Shuo, ZOU Zongyuan, HAN Shuting, ZHANG Rongqiang, GUO Baofeng. Mechanical Characteristics of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si During Cyclic Deformation[J]. 金属学报, 2019, 55(12): 1495-1502.
[3] Xirong LIU, Kai ZHANG, Shuang XIA, Wenqing LIU, Hui LI. Effects of Triple Junction and Grain Boundary Characters on the Morphology of Carbide Precipitation in Alloy 690[J]. 金属学报, 2018, 54(3): 404-410.
[4] Tingguang LIU, Shuang XIA, Qin BAI, Bangxin ZHOU, Yonghao LU. Distribution Characteristics of Twin-Boundaries in Three-Dimensional Grain Boundary Network of 316L Stainless Steel[J]. 金属学报, 2018, 54(10): 1377-1386.
[5] CHE Xin, LIANG Xingkui, CHEN Lili, CHEN Lijia, LI Feng. MICROSTRUCTURES AND LOW-CYCLE FATIGUE BEHAVIOR OF Al-9.0%Si-4.0%Cu-0.4%Mg(-0.3%Sc) ALLOY[J]. 金属学报, 2014, 50(9): 1046-1054.
[6] ZHANG Siqian, WU Wei, CHEN Lili, CHE Xin, CHEN Lijia. INFLUENCE OF HEAT TREATMENT ON LOW-CYCLE FATIGUE BEHAVIOR OF EXTRUDED Mg-7%Zn-0.6%Zr-0.5%Y ALLOY[J]. 金属学报, 2014, 50(6): 700-706.
[7] CAI Zhengxu WANG Weiguo FANG Xiaoying GUO Hong. EFFECT OF GRAIN SIZE ON THE GRAIN BOUNDARY CHARACTER DISTRIBUTIONS OF COLD ROLLED AND ANNEALED PURE COPPER[J]. 金属学报, 2010, 46(7): 769-774.
[8] JIANG Qingwei LIU Yin WANG Yao CHAO Yuesheng LI Xiaowu . MICROSTRUCTURAL INSTABILITY OF ULTRAFINE--GRAINED COPPER UNDER ANNEALING AND HIGH--TEMPERATURE DEFORMING[J]. 金属学报, 2009, 45(7): 873-879.
[9] ;. FINITE ELEMENT SIMULATION FOR CYCLIC DEFORMATION OF SiCP/6061Al ALLOY COMPOSITES[J]. 金属学报, 2006, 42(10): 1051-1055 .
[10] YANG Jihong; ZHANG Xinping; Y. W. MAI; LI Yong. Simulation Of Internal~ Stresses~ Near The Surface And Fatigue Crack Nucleation For A Copper Single Crystal In Cyclic Deformation Saturation Stage[J]. 金属学报, 2005, 41(1): 9-.
[11] ZHANG Zhefeng; WANG Zhongguang; SU Huihe(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: ZHANG Zhefeng Tel: (024)23843531-55225; Fax: (024)23891320. CYCLIC DEFORMATION BEHAVIOR OF A COPPER BICRYSTAL WITH A PERPENDICULAR GRAIN BOUNDARY[J]. 金属学报, 1998, 34(8): 841-846.
[12] (LI Xiaowu; WANG Zhongguang; SUN Shouguang; WU Shiding; LI Shouxin;LI Guangyi (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Department of Mechanical Engineering; Northern Jiaotong University; Beijing 100044). CYCLIC DEFORMATION BEHAVIOR OF [011]MULTIPLE-SLIP-ORIENTED COPPER SINGLE CRYSTALS Ⅱ. Surface Slip Features and Deformation Bands[J]. 金属学报, 1998, 34(5): 552-560.
[13] LI Xiaowu; WANG Zhongguang; SUN Shouguang; WU Shiding;LI Shouxin;LI Guangyi (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Department of Mechanical Engineering; Northern Jiaotong University; Beijing 100044). CYCLIC DEFORMATION BEHAVIOR OF [011] MULTIPLE-SLIP-ORIENTED COPPER SINGLE CRYSTALSCyclic Stress-Strain Response[J]. 金属学报, 1998, 34(5): 545-551.
[14] I. Cyclic Deformation Behavior and Slip Morphology HU Yunming; WANG Zhongguang (State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Chinese Academy ofSciences; Shenyang 110015) (Manuscript received 1996-09- 12; in revised form 1997-03-07). CYCLIC DEFORMATION BEHAVIOR AND FATIGUE CRACK INIT1ATION IN COPPER BICRYSTALS[J]. 金属学报, 1997, 33(8): 814-823.
[15] WU Jiansheng; LIN Dangling(Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1995-10-04). BEHAVIOUR OF Nb BICRYSTALS UNDER TENSION AND CYCLIC DEFORMATION[J]. 金属学报, 1996, 32(5): 527-531.
No Suggested Reading articles found!