MICRO-/MACRO-SCOPIC MODELING OF SOLUTAL MASS TRANSPORT IN DENDRITE SOLIDIFICAfION WITH PARTIAL SOLID BACK DIFFUSION
XU Daming ; ZHANG Chengjun ; SI Guangju (School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001)(Engineering College; Jiamusi University; Jiamusi 154007)
Cite this article:
XU Daming ; ZHANG Chengjun ; SI Guangju (School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001)(Engineering College; Jiamusi University; Jiamusi 154007). MICRO-/MACRO-SCOPIC MODELING OF SOLUTAL MASS TRANSPORT IN DENDRITE SOLIDIFICAfION WITH PARTIAL SOLID BACK DIFFUSION. Acta Metall Sin, 1998, 34(7): 678-688.
Abstract The continuum model proposed by the present authors for macroscopic solidification transport phenomena and macrosegregation formation was extended to account for the effect of any incomplete solid back diffusion through a microscopic dendrite solidification model. A generalized coefficient for the solid back diffusion was proposed by the present microscopic/macroscopic model, which includes the growing dendrite dimension, the parameters for the dendrite geometry, the solidification rate and partition coefficient etc besides the solid diffusivity.Numerical simulation of macrosegregations in a horizontal directionally soliditied A1-4.4Cu ingot with assumed different solid diffusivities of the copper solute was performed using the extended continuum model. The computation results show that the variation of the solid back diffusion can evidently influence the macrocomposition distribution in the soliditied ingot, and the greater the solid solute diffusivity, the lighter the macrosegregation seventy.
1 Bennon W D, Incropera F P. Int J Heat Mass Transfer 1987; 30: 2161, 2171 2 Prescott P J, Incropera F P, Bennon W D. Int J Heat Maas Transfer, 1991; 34: 2351 3 Voller V R, Prakash C. Int J Heat Mass Transfer 1987; 30: 1709 4 Beckermann C. Viskanta R. Phys Chem Hydrodyn. 1988: 10: 195 5徐达鸣,李庆春,安阁英铸造,1997;(4):44 (Xu Damin., Li Qingchun, An Geying Foundry, 1997(4): 44) 6 Diao Q Z, Tsai H L. Metall Trans, 1993; 24A: 963 7顾江平清华大学博士学位论文,1995(Gu Jiangping.PhD Thesis,Tsinghua University,1995) 8 Rappaz M, Voller V. Metall Trans, 1990; 21A: 749 9 Schneider M C, Beckermann C. Int J Heat Mass Transfer, 1995; 38: 3455 10徐达鸣.哈尔滨工业大学博士学位论文,1989(Xu Daming、PhD Thesis,Harbin Institute of Technology,,1989) 11 Xu Daming, Li Qingchun. Numer Heat Transfer, 1991; 20A: 181; 203 12 Shahani H, Amberg G, Fredriksson H. Metall Trans, 1992; 23A: 2301 13陈卫德.大连理工大学博士学位论文,1994(Chen Weide.PhD Thesis,Dalian University of Science and Engineering,1994) 14徐达鸣,李庆春.金属学报,1990;26:B267(Xu Daming, Li Qingchun. Acta Metall Sin, 1990; 26: B267) 15 Gray W G. Chem Egg Sci, 1975; 30: 229 16 Ni J, Beckermann C. Metall Trans, 1991; 22B: 349 17 Flemings M C, Nereo G E. Trans Metall Soc AIME, 1967; 239: 1449 18 1980; (1): 6(Balangin G F. Cast Product, 1980; (1): 6) 19 Geiger G H, Poirier D R. Transport Phenomena in Metallurgy. Reading, Mass: Addison-Wesley, 1973:20司广琚.哈尔滨工业大学硕士学位论文,1996(Si Guangju.Master Thesis,Harbin Institute of Technology,1996) 21 Bower T F, Brody H D, Flemings M C. Trans Metall Soc AIME, 1966; 236: 624 22 Xu Daming, Si Guanaiu. In: Proc 3rd Pacific Rim Int Conf on Modeling of Casting and SolidificationPriestes 1996, Beijing: International Academic Publishers, 1996: 228