VISCOELASTIC-PLASTIC ANALYSIS OF BROADENING OF SLAB IN THE SECONDARY COOLING ZONE OF CONTINUOUS CASTING
FU Jianxun1;2); LI Jingshe1); ZHANG Hui2)
1) School of Metallurgical and Ecological Engineering; University of Science and Technology Beijing; Beijing 100083
2) National Engineering Research Center of Continuous Casting Technology; China Iron $\&$ Steel Research Institute Group; Beijing 100081
Cite this article:
FU Jianxun LI Jingshe ZHANG Hui. VISCOELASTIC-PLASTIC ANALYSIS OF BROADENING OF SLAB IN THE SECONDARY COOLING ZONE OF CONTINUOUS CASTING. Acta Metall Sin, 2010, 46(1): 91-96.
The 3D viscoelastic-plastic thermal-mechanically coupled finite element model was established by a commercial software MSC.Marc on the basis of secondary development, and used to simulate the situation of slab's broadening in the secondary cooling zone. The results showed that the slab's broadening mainly emerged in the former segments of the secondary cooling zone, and the broadening rate has a gradually increasing trend from the first segment to the sixth segment. The broadening of slab has a close relationship with bulging along the thickness direction. The results simulated by using viscoelastic-plastic model revealed that the law of the slab's broadening is excellent agreement with the actual deformation. The broadening of slab is the result of viscoelastic-plastic deformation of the slab shell under the pressure of core of molten steel.
[1] Yoshii A, Kihara S. Trans ISIJ, 1986; 26: 891
[2] Maeno S, Wada K, Itoh Y, Nagano Y. Trans ISIJ, 1983; 24: 83
[3] Siyasiya C, van Rooyen G T. Stumpf W E. J South Afr Inst Mining Metall, 2005; 105: 473
[4] Lin Q Y, Zhu M Y. Acta Metall Sin, 2007; 43: 1301
(林启勇, 朱苗勇. 金属学报, 2007; 43: 1301)
[5] Chen Z P, Cheng N L, Cui L X, Zhang J Q. Iron Steel, 2004; 39(suppl): 457
(陈志平, 程乃良, 崔立新, 张家泉. 钢铁, 2004; 39(增刊): 457
[6] Fu J X. PhD Thesis, University of Science and Technology Beijing, 2009
(付建勋. 北京科技大学博士学位论文, 2009)
[7] Kim K H, Yeo T J, Oh K H, Lee D N. ISIJ Int, 1996; 36: 284
[8] Grill A, Schwerdtfeger K. Ironmak Steelmak, 1979; 6: 131
[9] Barber B, Lewis B A, Leckenby B M. Ironmak Steelmak, 1985; 12: 171
[10] Okamura K, Kawashima H. ISIJ Int, 1989; 29: 666
[11] Sorimachi K, Brimacombe J K. Ironmak Steelmak, 1977; 4: 240
[12] Wang X C. Finite Element Method. Beijing: Tsinghua University Press, 2003: 125
(王勖成. 有限单元法. 北京: 清华大学出版社, 2003: 125)
[13] Fu J X, Li J S, Wang C L, Zhu J T. Mater Rev, 2009; 23(9): 68
(付建勋, 李京社, 汪春雷, 朱经涛. 材料导报, 2009; 29(9): 68)
[14] Uehara M, Samarasekera I V, Brimacombe J K. Iro nmak Steelmak, 1986; 13: 138
[15] Chen S Q. PhD Thesis, Central Iron and Steel Research Institute, Beijing, 2004