| SOLIDIFICATION PHASE SELECTION IN DIRECTION-ALLY SOLIDIFIED Ti–(44%—54%)Al ALLOYS |
| LI Xinzhong 1; SUN Tao 2; YU Caixia 1; SU Yanqing 2; CAO Yongzhi 2; GUO Jingjie 1; FU Hengzhi 1 |
1. School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001
2. School of Mechatronics Engineering; Harbin Institute of Technology; Harbin 150001 |
|
Cite this article:
LI Xinzhong SUN Tao YU Caixia SU Yanqing CAO Yongzhi GUO Jingjie FU Hengzhi . SOLIDIFICATION PHASE SELECTION IN DIRECTION-ALLY SOLIDIFIED Ti–(44%—54%)Al ALLOYS. Acta Metall Sin, 2009, 45(12): 1479-1486.
|
|
|
Abstract Directional solidification experiments were conducted for Ti–(44%—54%)Al (atomic fraction) alloys in a wide range of ratios between temperature gradients and growth rates. Interfacial morphology evolution, microstructure formation and the final lamellar orientatios were investigated undedifferent solidification conditions. Nucleation and compositional undercooling citerion were used to clculate the phase selection map for Ti–Al alloys which gives phases and corresponding microstructures at different initial compositions and solidification parameters. The map is in good agreement with the experimental results and gives important criteria for determing phase compositions and solidification parameters in lamellar orientation control of Ti–Al alloys.
|
|
Received: 09 June 2009
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.50771041 and 50801019), China Postdoctoral Science Foundation (No.20080430909), Financial Assistance Under Heilongjiang Postdoctorial Fund (No.LBH–Z08127) and Development Programme for Outstanding Young Teachers in Harbin Institute of Technology (No.HITQNJS.2008.018)
|
| [1] Loria E A. Intermetallics, 2000; 8: 1339
[2] Kim Y W. JOM, 1994; 4: 14
[3] Oliver B F, Kad B. J Less–Comon Met, 1991; 168: 81
[4] Ramanujan R V, Bi Y J, Xu Q, Abell J S. Scr Metall Mater, 1994; 30: 719
[5] Bi Y J, Abell J S. Scr Metall Mater, 1994; 31: 751
[6] Johnson D R, Inui H, Yamaguchi M. Acta Mater, 1996; 44: 2523
[7] Kim M C, Oh M H, Lee J H, Inui H, Yamaguchi M, Wee D M. Mater Sci Eng, 1997; A239–240: 570
[8] Johnson D R, Inui H, Muto S, Omiya Y, Yamanaka T. Acta Mater, 2006; 54: 1077
[9] Liu Y C. PhD Thesis, Northwestern Polytechnical University, Xi’an, 2000
(刘永长. 西北工业大学博士论文, 西安, 2000)
[10] Liu C. PhD Thesis, Harbin Institute of Technology, 2006
(刘 畅. 哈尔滨工业大学博士论文, 2006)
[11] Luo W Z, Shen J, Min Z X, Fu H Z. J Cryst Growth, 2008; 310: 5441
[12] Boettinger W J. Metall Trans, 1974; 24: 2023
[13] Lo T S, Dobler S, Plapp M, Karma A, Kurz W. Acta Mater, 2003; 51: 599
[14] Karma A, Rappel W J, Fuh B C, Trivedi R. Metall Mater Trans, 1998; 29A: 1457
[15] Dobler S, Lo T S, Plapp M, Karma A, Kurz W. Acta Mater, 2004; 52: 2795
[16] Umeda T, Okane T, Kurz W. Acta Mater, 1996; 44: 4209
[17] Hunziker O, Vandyoussefi M, Kurz W. Acta Mater, 1998; 46: 6325
[18] Guo J J, Li X Z, Su Y Q, Fu H Z. Acta Metall Sin, 2005; 41: 599
(郭景杰, 李新中, 苏彦庆, 吴士平, 傅恒志. 金属学报, 2005; 41: 599)
[19] XiaoW. PhD Thesis, Harbin Institute of Technology, 2008
(肖伟. 哈尔滨工业大学硕士论文, 2008)
[20] Lapin J, Ondrus L, Nazmy M. Intermetallics, 2002; 10: 1019
[21] Lu H Y. Master Disseration, Northwestern Polytechnical University, Xi’an, 2004
(吕海燕. 西北工业大学硕士论文, 西安 2004) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|