PREPARATION OF MELT-ATOMIZED AND SPRAY-DEPOSITED LA62AL15.7(CU0.5NI0.5)22.3 AMORPHOUS ALLOY
;;;
北京科技大学新金属材料国家重点实验室
Cite this article: 

;. PREPARATION OF MELT-ATOMIZED AND SPRAY-DEPOSITED LA62AL15.7(CU0.5NI0.5)22.3 AMORPHOUS ALLOY. Acta Metall Sin, 2008, 44(6): 659-664 .

Download:  PDF(1525KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  It is known as very difficult to prepare bulk amorphous alloys with much larger size, because the heat release will be hindered and crystallization takes place when the bulk grows larger. In view of existing the bottleneck, a full La62Al15.7(Cu0.5Ni0.5)22.3 amorphous alloy with a diameter of 340 mm and maximum thickness of 13 mm was produced by melt atomization and spray deposition. The formation mechanism of amorphous phase during the process was analyzed. The experimental results have shown that there always exist some porosity in the spray-deposited La62Al15.7(Cu0.5Ni0.5)22.3 amorphous alloy. The micropores in the La62Al15.7(Cu0.5Ni0.5)22.3 amorphous alloy can be eliminated by hot pressing in the undercooled liquid region of the amorphous alloy. The present results have indicated that spray deposition is a potential technique to prepare bulk amorphous alloys with larger size, especially for bigger plate-shaped deposit.
Key words:  melt atomization      spray deposition      La-based alloy      amorphous alloy      
Received:  18 December 2007     
ZTFLH:  TG139.8  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I6/659

[1]Wang W H,Dong C,Shek C H.Mater Sci Eng,2004;R44: 45
[2]L■ffler J F.Intermetallics,2003;11:529
[3]Song G S,Shen J,Jiang Z L,Li Q C.Mater Sci Eng,1994; A179-180:249
[4]Liu D M,Zhao J Z,Ye H Q.Acta Metall Sin,2003;39: 375 (刘东明,赵九洲,叶恒强.金属学报,2003;39:375)
[5]Afonso C R M,Bolfarini C,Botta Filho W J,Kiminami C S.Mater Sci Eng,2004;A375-377:571
[6]Afonso C R M,Bolfarini C,Botta Filho W J,Kiminami C S.Mater Sci Eng,2007;A449 451:88
[7]Zambon A,Badan B.Mater Sci Eng,2004;A375 377:638
[8]Ted Guo M L,Tsao C Y A,Huang J C,Jang J S C.Mater Sci Eng,2005;A404:49
[9]Tan H,Zhang Y,Ma D,Fcng Y P,Li Y.Acta Mater,2003; 51:45511
[10]Zhang Y,Tan H,Li Y.Mater Sci Eng,2004;A375 377: 436
[11]Liang X,Lavernia E J.Mater Sci Eng,1993:A161:221
[12]Drehman A J,Turnbull D.Scr Metall,1981:15:543
[13]Zhou Y H,Hu Z Q,Jie W Q.Solidification Technology. Beijing:China Machine Industry Press,1998:245 (周尧和,胡壮麒、介万奇.凝固技术.北京:机械工业出版社,1998:245)
[14]Szekely J,Themelis N J.Rate Phenomena in Process Met- allurgy.New York:Wiley Interscience,1971:237
[15]Liang H Y,Mao X M,Hu Z H.Foundry.Teehnol,2007; 28:367 (梁红玉,毛协民,胡志恒.铸造技术,2007:28:367)
[16]Lin X H,Johnson W L.J Appl Phys,1995:78:6514
[1] LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng. Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region[J]. 金属学报, 2022, 58(6): 807-815.
[2] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[3] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[4] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[5] HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si. Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. 金属学报, 2021, 57(4): 542-552.
[6] LIU Riping, MA Mingzhen, ZHANG Xinyu. New Development of Research on Casting of Bulk Amorphous Alloys[J]. 金属学报, 2021, 57(4): 515-528.
[7] ZHU Min, OUYANG Liuzhang. Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys[J]. 金属学报, 2021, 57(11): 1416-1428.
[8] HUANG Huogen, ZHANG Pengguo, ZHANG Pei, WANG Qinguo. Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems[J]. 金属学报, 2020, 56(6): 849-854.
[9] GENG Yaoxiang, WANG Yingmin. Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research[J]. 金属学报, 2020, 56(11): 1558-1568.
[10] XU Xiuyue, LI Yanhui, ZHANG Wei. Fabrication of Nanoporous PtRuFe by Dealloying Amorphous Fe(Pt, Ru)B Ribbons and Their Methanol Electrocatalytic Properties[J]. 金属学报, 2020, 56(10): 1393-1400.
[11] JIN Chenri, YANG Suyuan, DENG Xueyuan, WANG Yangwei, CHENG Xingwang. Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy[J]. 金属学报, 2019, 55(12): 1561-1568.
[12] Hongyang XU,Haibo KE,Huogen HUANG,Pei ZHANG,Pengguo ZHANG,Tianwei LIU. Nanoindentation Creep Behavior of U65Fe30Al5 Amorphous Alloy[J]. 金属学报, 2017, 53(7): 817-823.
[13] Dianguo MA,Yingmin WANG,Kunio YUBUTA,Yanhui LI,Wei ZHANG. Effect of Co Content on the Structure and Magnetic Properties of Melt-Spun Fe55-xCoxPt15B30 Alloys[J]. 金属学报, 2017, 53(5): 609-614.
[14] Huogen HUANG,Hongyang XU,Pengguo ZHANG,Yingmin WANG,Haibo KE,Pei ZHANG,Tianwei LIU. U-Cr Binary Alloys with Anomalous Glass-Forming Ability[J]. 金属学报, 2017, 53(2): 233-238.
[15] Yaoxiang GENG,Kaiming HAN,Yingmin WANG,Jianbing QIANG,Qing WANG,Chuang DONG,Guifeng ZHANG,O TEGUS,Peter HAÜSSLER. COMPOSITION DESIGN OF Fe-B-Si-Ta BULK AMORPHOUS ALLOYS BASED ON CLUSTER+ GLUE ATOM MODEL[J]. 金属学报, 2015, 51(8): 1017-1024.
No Suggested Reading articles found!