| INVESTIGATION OF HYPERFINE STRUCTURE OF LASER CLADDING Fe-Si COATING |
| DONG Dan-Yang;Changsheng LIU |
| 辽宁省沈阳市东北大学材料与冶金学院 |
|
Cite this article:
DONG Dan-Yang; Changsheng LIU. INVESTIGATION OF HYPERFINE STRUCTURE OF LASER CLADDING Fe-Si COATING. Acta Metall Sin, 2008, 44(2): 188-192 .
|
|
|
Abstract Fe-Si coating with high silicon content was prepared by laser cladding method on low silicon steel surface. Microstructure, hyperfine structure and structural transformation at RT of laser cladding coating were investigated by scanning electron microscopy, transmission electron microscopy,Mossbauer spectroscopy and X-ray diffraction. The results show that there forms metallurgical bonding at the interface between Fe-Si coating and substrate and there exist planar, columnar and dendritic microstructures from the interface to the top surface of the coating. In the laser cladding coating, six different atom configurations of Fe atom are observed. The primary phase containing Si atom is corresponding to the α-Fe type phase of disorderd solid solution structure whose relative content is 24.6 %. The isomer shift increases and the hyperfine magnetic field decreases as the number of nearest- neighbour Si atoms increases in the α-Fe type phase.
|
|
Received: 17 May 2007
|
[1]Haiji H,Okada K,Hiratani T,Abe M,Ninomiya M.J Magn Magn Mater,1996;160:109 [2]Ushigami Y,Mizokami M,Fujikura M,Kubota T,Fujii H, Murakami K.J Magn Magn Mater,2003;254-255:307 [3]Dong D Y,Liu C S,Zhang B,Miao J.Chin J Mater Res, 2007;21:364 (董丹阳,刘常升,张滨,苗隽.材料研究学报,2007;21:364) [4]Dong D Y,Liu C S,Zhang B,Miao J.J Univ Sci Technol Beijing,2007;14:321 [5]Pelletier J M,Renaud L,Fouquet F.Mater Sci Eng,1991; A134:1283 [6]Yang S,Su Y P,Liu W J,Huang W D,Zhou Y H.Acta Phys Sin,2003;52:81 (杨森,苏云鹏,刘文今,黄卫东,周尧和.物理学报,2003;52:81) [7]Su Y P,Lin X,Wang M,Xue L,Huang W D.Chin Phys, 2006;15:1631 [8]Song J L,Deng Q L,Hu D J,Chen C Y.Chin J Lasers, 2005;32:1441 (宋建丽,邓琦林,胡德金,陈畅源.中国激光,2005;32:1441) [9]Zhao Y,Sheng Q,Wang C B,Zhang L M.Powder Metall Technol,2006;24:407 (赵媛,沈强,王传彬,张联盟.粉末冶金技术,2006;24:407) [10]Li T,Li Y Z,Zhang Y H.J Phys Condens Matter,1997; 9:1381 [11]Li X N,Nie D,Dong C,Ma T C,Jin X,Zhang Z.Acta Phys Sin,2002;51:115 (李晓娜,聂冬,董闯,马腾才,金星,张泽.物理学报,2002;51:115) [12]Yuan X G,Xu D M,Zhang W D,Li Q C.Acta Metall Sin,1996;32:1034 (袁晓光,徐达鸣,张卫方,李庆春.金属学报,1996;32:1034) [13]Chen S Y,Liu C S,Fu G Q,Zhang J L,Cai Q K.Chin J Laser,2003;30:1049 (陈岁元,刘常升,付贵勤,张继良,才庆魁.中国激光,2003;30:1049) [14]Stearns M B.Phys Rev,1963;129:1136 [15]Ma R Z,Xu Y T.The Theory of M(?)ssbauer Spectra.Bei- jing:Science Press,1996:438 (马如璋,徐英庭.穆斯堡尔谱学.北京:科学出版社,1996:438) [16]Teng G Q,Chao Y S.Chin or Nonferrous Met,2000;10: 27 (滕功清,晁月盛.中国有色金属学报,2000;10:27) [17]Bai K C,Jiang Z Y,He K Y,Cheng L Z,Zhi J.Acta Metall Sin,1994;30:67 (白魁昌,江自应,何开元,程力智,智靖.金属学报,1994;30:67) [18]Chao Y S,Zeng F W,Yang Y L,Dong L Q,Chen S Y. Acta Metall Sin,2000;36:235 (晁月盛,曾繁武,杨玉玲,董立秋,陈岁元.金属学报,2000;36:235) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|