Acta Metall Sin  2007, Vol. 43 Issue (3): 321-326     DOI:
Research Articles Current Issue | Archive | Adv Search |
EFFECT OF WELDING PARAMETERS ON MIXTURE OF MATERIALS IN NUGGET ZONE IN FRICTION STIR WELDS
Cite this article: 

. EFFECT OF WELDING PARAMETERS ON MIXTURE OF MATERIALS IN NUGGET ZONE IN FRICTION STIR WELDS. Acta Metall Sin, 2007, 43(3): 321-326 .

Download:  PDF(824KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Rate dependent constitutive model is used to simulate the friction stir welding process. The effect of the process parameters on the material deformation on the transverse section of the friction stir weld is investigated. The mixture of the materials on the both sides of the welding line in the nugget zone and thermo-mechanical zone is studied by means of the research on the equivalent plastic strain distributions under different process parameters. The effect of the process parameters on the weld quality is herein judged from the material deformations. Results indicate that mixture of the material can be improved when the angular velocity of the pin is increased or the welding speed is decreased. But flaws may occur when the angular velocity is too high.
Key words:  friction stir welding      finite element method      weld quality      
Received:  21 June 2006     
ZTFLH:  TG404  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I3/321

[1]Mishra R S,Ma Z Y.Mater Sci Eng,2005;R50:1
[2]Liu H J,Chen Y C,Feng J C.Scr Mater,2006;55:231
[3]Feng J C,Chen Y C,Liu H J.Mater Sci Technol,2006; 22:86
[4]Zeng W M,Wu H L,Zhang J.Acta Metall Sin(Engl Lett), 2006;19:9
[5]Ma Z Y,Mishra R S,Mahoney M W.Acta Mater,2002; 50:4419
[6]Ma Z Y,Mishra R S.Scr Mater,2005;53:75
[7]Ma Z Y,Sharma S R,Mishra R S.Sct Mater,2006;54: 1623
[8]Xu S W,Deng X M,Reynolds A P,Seidel T U.Sci Technol Weld Joining,2001;6:191
[9]Deng X M,Xu S W.J Manuf Process,2004;6:125
[10]Fonda R W,Lambrakos S G.Sci Technol Weld Joining, 2002,7:177
[11]Schmidt H,Hattel J.Sci Technol Weld doining,2005;10: 176
[12]Khandkar M Z H,Khan J A,Reynolds A P,Sutton M A. J Mater Process Technol,2006;174:195
[13]Zhang H W,Zhang Z,Chen J T.Acta Metall Sin,2005; 41:853 (张洪武,张昭,陈金涛.金属学报,2005;41:853)
[14]Zhang H W,Zhang Z,Chen J T.Mater Sci Eng,2005; A403:340
[15]Zhang z,Chen J T,Zhang H W.J Aeronaut Mater,2005; 25(6):33 (张昭,陈金涛,张洪武.航空材料学报,2005;25(6):33)
[16]Zhang Z,Chen J T,Zhang H W.J Mater Eng,2006;(1): 19 (张昭,陈金涛,张洪武.材料工程,2006;(1):19)
[17]Zhang H W,Zhang Z,Chen J T.Chin Mech Eng,2006; 17(7):719 (张洪武,张昭,陈金涛.中国机械工程,2006;17:719)
[18]Zhang Z,Zhang H W.Ord Mater Sci Eng,2006;29(3): 61 (张昭,张洪武.兵器材料科学与工程,2006;29(3):61)
[19]Zhang H W,Zhang Z,Chen J T.Trans Chin Weld Inst, 2005;26(9):13 (张洪武,张昭,陈金涛.焊接学报,2005;26(9):13)
[20]Zhang Z,Zhang H W.Acta Metall Sin,2006;42:998 (张昭,张洪武.金属学报,2006;42:998)
[21]Ponthot J P.J Mater Process Technol,1998,80-81:628
[22]Belytschko T,Liu W K,Moran B.Nonlinear Finite El- ??ements for Continua and Structures.New York:John Wiley & Sons Ltd,2000:131
[23]HKS Inc.ABAQUS Theory Manual,V6.4,Hibbt,Karls- son and Sorensen Inc.,2003
[24]Simo J C,Hughes T J R.Computational Inelasticity,New York:Springer,1998:153
[25]Potdar Y K,Zehnder A T.J Manuf Sci Eng,2003;125: 645
[26]Chen C M,Kovacevic R.Int J Mach Tools Manuf,2004; 44:1205
[27]Tang W,Guo X,McClure J C,Numes L E.J Mater Pro- cess Manuf Sci,1998;7:163
[28]Colegrove P,Painter M,Graham D,Miller T.Proc 2nd Int Syrup on Friction Stir Welding.Gothenburg:TWI Center,2000:162
[29]Fratini L,Buffa G.Int J Mach Tools Manuf,2005;45: 1188
[30]Marzoli L M,Strombeck A V,Dos Santos J F,Gambaro C,Volpone L M.Compos Sci Technol,2006;66:363Z
[1] LI Shaojie, JIN Jianfeng, SONG Yuhao, WANG Mingtao, TANG Shuai, ZONG Yaping, QIN Gaowu. Multimodal Microstructure of Mg-Gd-Y Alloy Through an Integrated Simulation of “Process-Structure-Property”[J]. 金属学报, 2022, 58(1): 114-128.
[2] HE Changshu, QIE Mofan, ZHANG Zhiqiang, ZHAO Xiang. Effect of Axial Ultrasonic Vibration on Metal Flow Behavior During Friction Stir Welding[J]. 金属学报, 2021, 57(12): 1614-1626.
[3] LIU Chenxi, MAO Chunliang, CUI Lei, ZHOU Xiaosheng, YU Liming, LIU Yongchang. Recent Progress in Microstructural Control and Solid-State Welding of Reduced Activation Ferritic/Martensitic Steels[J]. 金属学报, 2021, 57(11): 1521-1538.
[4] Xuexiong LI,Dongsheng XU,Rui YANG. Crystal Plasticity Finite Element Method Investigation of the High Temperature Deformation Consistency in Dual-Phase Titanium Alloy[J]. 金属学报, 2019, 55(7): 928-938.
[5] Chen WANG, Beibei WANG, Peng XUE, Dong WANG, Dingrui NI, Liqing CHEN, Bolü XIAO, Zongyi MA. Fatigue Behavior of Friction Stir Welded SiCp/6092Al Composite[J]. 金属学报, 2019, 55(1): 149-159.
[6] Chuansong WU, Hao SU, Lei SHI. Numerical Simulation of Heat Generation, Heat Transfer and Material Flow in Friction Stir Welding[J]. 金属学报, 2018, 54(2): 265-277.
[7] Zongyi MA, Qiao SHANG, Dingrui NI, Bolv XIAO. Friction Stir Welding of Magnesium Alloys: A Review[J]. 金属学报, 2018, 54(11): 1597-1617.
[8] Jianhai YANG,Yuxiang ZHANG,Liling GE,Xiao CHENG,Jiazhao CHEN,Yang GAO. Effect of Hybrid Surface Nanocrystallization Before Welding on Microstructure and Mechanical Properties of Friction Stir Welded 2A14 Aluminum Alloy Joints[J]. 金属学报, 2017, 53(7): 842-850.
[9] Ju KANG,Suying LIANG,Aiping WU,Quan LI,Guoqing WANG. Local Liquation Phenomenon and Its Effect on Mechanical Properties of Joint in Friction Stir Welded 2219 Al Alloy[J]. 金属学报, 2017, 53(3): 358-368.
[10] Fenjun LIU, Li FU, Haiyan CHEN. Microstructures and Mechanical Properties of Thin Plate Aluminium Alloy Joint Prepared by High Rotational Speed Friction Stir Welding[J]. 金属学报, 2017, 53(12): 1651-1658.
[11] Guannan CHU,Yanli LIN,Weining SONG,Lin ZHANG. Forming Limit of FSW Aluminum Alloy Blank Based on a New Constitutive Model[J]. 金属学报, 2017, 53(1): 114-122.
[12] Yongkui LI, Chunyi QUAN, Shanping LU, Qingyang JIAO, Shijian LI, Zhonghai SUN. STUDY ON SHAPE CORRECTION OF THE THIN PLATE OF TA15 TITANIUM ALLOY BY POST WELD HEAT TREATMENT[J]. 金属学报, 2016, 52(3): 281-288.
[13] Peng XUE, Xingxing ZHANG, Lihui WU, Zongyi MA. RESEARCH PROGRESS ON FRICTION STIR WELDING AND PROCESSING[J]. 金属学报, 2016, 52(10): 1222-1238.
[14] Ju KANG,Jichao LI,Zhicao FENG,Guisheng ZOU,Guoqing WANG,Aiping WU. INVESTIGATION ON MECHANICAL AND STRESS CORROSION CRACKING PROPERTIES OF WEAKNESS ZONE IN FRICTION STIR WELDED 2219-T8 Al ALLOY[J]. 金属学报, 2016, 52(1): 60-70.
[15] LIU Fenjun, FU Li, ZHANG Wenyuan, MENG Qiang, DONG Chunlin, LUAN Guohong. INTERFACE STRUCTURE AND MECHANICAL PRO-PERTIES OF FRICTION STIR WELDING JOINT OF 2099-T83/2060-T8 DISSIMILAR Al-Li ALLOYS[J]. 金属学报, 2015, 51(3): 281-288.
No Suggested Reading articles found!