| EFFECT OF WELDING PARAMETERS ON MIXTURE OF MATERIALS IN NUGGET ZONE IN FRICTION STIR WELDS |
|
Cite this article:
. EFFECT OF WELDING PARAMETERS ON MIXTURE OF MATERIALS IN NUGGET ZONE IN FRICTION STIR WELDS. Acta Metall Sin, 2007, 43(3): 321-326 .
|
|
|
Abstract Rate dependent constitutive model is used to simulate the friction stir welding process. The effect of the process parameters on the material deformation on the transverse section of the friction stir weld is investigated. The mixture of the materials on the both sides of the welding line in the nugget zone and thermo-mechanical zone is studied by means of the research on the equivalent plastic strain distributions under different process parameters. The effect of the process parameters on the weld quality is herein judged from the material deformations. Results indicate that mixture of the material can be improved when the angular velocity of the pin is increased or the welding speed is decreased. But flaws may occur when the angular velocity is too high.
|
|
Received: 21 June 2006
|
|
|
[1]Mishra R S,Ma Z Y.Mater Sci Eng,2005;R50:1 [2]Liu H J,Chen Y C,Feng J C.Scr Mater,2006;55:231 [3]Feng J C,Chen Y C,Liu H J.Mater Sci Technol,2006; 22:86 [4]Zeng W M,Wu H L,Zhang J.Acta Metall Sin(Engl Lett), 2006;19:9 [5]Ma Z Y,Mishra R S,Mahoney M W.Acta Mater,2002; 50:4419 [6]Ma Z Y,Mishra R S.Scr Mater,2005;53:75 [7]Ma Z Y,Sharma S R,Mishra R S.Sct Mater,2006;54: 1623 [8]Xu S W,Deng X M,Reynolds A P,Seidel T U.Sci Technol Weld Joining,2001;6:191 [9]Deng X M,Xu S W.J Manuf Process,2004;6:125 [10]Fonda R W,Lambrakos S G.Sci Technol Weld Joining, 2002,7:177 [11]Schmidt H,Hattel J.Sci Technol Weld doining,2005;10: 176 [12]Khandkar M Z H,Khan J A,Reynolds A P,Sutton M A. J Mater Process Technol,2006;174:195 [13]Zhang H W,Zhang Z,Chen J T.Acta Metall Sin,2005; 41:853 (张洪武,张昭,陈金涛.金属学报,2005;41:853) [14]Zhang H W,Zhang Z,Chen J T.Mater Sci Eng,2005; A403:340 [15]Zhang z,Chen J T,Zhang H W.J Aeronaut Mater,2005; 25(6):33 (张昭,陈金涛,张洪武.航空材料学报,2005;25(6):33) [16]Zhang Z,Chen J T,Zhang H W.J Mater Eng,2006;(1): 19 (张昭,陈金涛,张洪武.材料工程,2006;(1):19) [17]Zhang H W,Zhang Z,Chen J T.Chin Mech Eng,2006; 17(7):719 (张洪武,张昭,陈金涛.中国机械工程,2006;17:719) [18]Zhang Z,Zhang H W.Ord Mater Sci Eng,2006;29(3): 61 (张昭,张洪武.兵器材料科学与工程,2006;29(3):61) [19]Zhang H W,Zhang Z,Chen J T.Trans Chin Weld Inst, 2005;26(9):13 (张洪武,张昭,陈金涛.焊接学报,2005;26(9):13) [20]Zhang Z,Zhang H W.Acta Metall Sin,2006;42:998 (张昭,张洪武.金属学报,2006;42:998) [21]Ponthot J P.J Mater Process Technol,1998,80-81:628 [22]Belytschko T,Liu W K,Moran B.Nonlinear Finite El- ??ements for Continua and Structures.New York:John Wiley & Sons Ltd,2000:131 [23]HKS Inc.ABAQUS Theory Manual,V6.4,Hibbt,Karls- son and Sorensen Inc.,2003 [24]Simo J C,Hughes T J R.Computational Inelasticity,New York:Springer,1998:153 [25]Potdar Y K,Zehnder A T.J Manuf Sci Eng,2003;125: 645 [26]Chen C M,Kovacevic R.Int J Mach Tools Manuf,2004; 44:1205 [27]Tang W,Guo X,McClure J C,Numes L E.J Mater Pro- cess Manuf Sci,1998;7:163 [28]Colegrove P,Painter M,Graham D,Miller T.Proc 2nd Int Syrup on Friction Stir Welding.Gothenburg:TWI Center,2000:162 [29]Fratini L,Buffa G.Int J Mach Tools Manuf,2005;45: 1188 [30]Marzoli L M,Strombeck A V,Dos Santos J F,Gambaro C,Volpone L M.Compos Sci Technol,2006;66:363Z |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|