Refinement of Grain and Enhancement of Impact Energy Absorption for Low-Alloy Ultra-High Strength Bainite Steels Containing Silicon
Cite this article: 

. Refinement of Grain and Enhancement of Impact Energy Absorption for Low-Alloy Ultra-High Strength Bainite Steels Containing Silicon. Acta Metall Sin, 2007, 43(3): 315-320 .

Download:  PDF(974KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Through judiciously using the silicon, manganese and nickel as the alloying elements and effectively controlling the transformation temperature, cooling and tempering parameters for a series of low alloy ultrahigh strength bainitic steels (LUHSBS), the combination of strength and toughness are very excellent and the impact energy absorption (AKV ≥185 J) has been tripled compared to the previously advanced martensitic steel 23MnNiCrMo with the same strength level (>1500 MPa). The basic reasons giving rise to the enhancement of strength and toughness consist in the increase of carbon content and the refinement of sublaths in the bainitic ferrite (BF) and the very thin films of retained austenite (AR). It is confirmed by the atomicforce microscope (AFM) and scanning tunneling microscope (STM) that there was no any large bulky areas of AR in the structure which is less stable and will reduce the impact toughness of bainitic steels. Not only is the sublaths is significantly refined, but also the average size of subgrains is less than 20 nm and the average thickness of shear units in a BF lath is only about 1.6 nm. The refinement of microstructure, the enrichment of interstitial atom carbon in BF and the increase of both the dislocation density and the volume fraction of AR are some critical factors that affect the ultimate tensile strength, the stability of AR and the impact energy absorption. Furthermore, the physical mechanism on the improvement of the combination of strength and toughness is in depth discussed.
Key words:  bainitic ferrite      bainitic laths      sub-units      refined microstructure      
Received:  29 June 2006     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I3/315

[1]Hammond R I,Proud W G.Proc R Soc Lond,2004;460A: 2959
[2]Bhadeshia H K D H.Ironmaking Steelmaking,2005;32: 405
[3]Caballero F G,Bhadeshia H K D H,Mawella K J A,Jones D G,Brown P.Mater Sci Technol,2001;17:517
[4]Miihkinen V T T,Edmonds D V.Mater Sci Technol,1987; 3:422
[5]Miihkinen V T T,Edmonds D V.Mater Sci Technol,1987; 3:432
[6]Miihkinen V T T,Edmonds D V.Mater Sci Technol,1987; 3:441
[7]Caballero F G,Bhadeshia H K D H,Mawella K J A,Jones D G,Brown P.Mater Sci Technol,2001;17:512
[8]Tomita Y,Okawa T.Mater Sci Technol,1995;11:245
[9]Tomita Y.Mater Sci Technol,1995;11:259
[10]Bhadeshia H K D H.Mater Sci Technol,2005;21:1293
[11]Kang M K,Sun J L,Yang Q M.Metall Trans,1990;21 A:853
[12]Wang L D,Zhu M,Zhou W M,Chen J D,Shi Y J,Chen G D,Zhang W.Mater Sci Forum,2007;539—543:4562
[13]Toshiki N,Koichi G,Hiroazu T,Kazumasa Y.NIPPON Steel Technol Rep,No.88,2003
[14]Arif Basuki,Etienne Aernoudt.J Mater Process Technol, 1999;89—90:37
[15]Zhou W L,Guo J T,Chen R S,Zhou J Y.Acta Metall Sin,2000;36:798 (周文龙,郭建亭,陈荣石,周继扬.金属学报,2000;36:798)
[16]Gacrcia C,Peet M,Caballero F G,Bhadeshia H K D H. Mater Sci Technol,2004;20:814
[17]Peer M,Babu S S,Miller M K,Bhadeshia H K D H.Scr Mater,2004;50:1227
[18]Wang L D,Jiang L Z,Zhu M,Liu X,Zhou W M,Li Y.J Phys D:Appl Phys,2004;37:2151
[19]Wang L D,Jiang L Z,Zhu M,Liu X,Zhou W M.J Mater Sci Technol,2005;21:710
[20]Caballero F G,Bhadeshia H K D H,Mawella K J A,Jones D G,Brown P.Mater Sci Technol,2002;18:279
[21]Kang Y,Bhadeshia H K D H.Mater Sci Technol,2006; 22:650
[22]Fang H S,Bai B Z,Xu P G,Zhang C,Yang Z G,Liu D Y.Heat Treat Met,2002;27(11):1 (方鸿生,白秉哲,徐平光,张弛,杨志刚,刘东雨.金属热处理,2002;27(11):1)
[23]Hsu T Y(Xu Z Y).Martensitic Transformation and Martensite.Beijing:Science Press,1999:568 (徐祖耀.马氏体相变与马氏体.北京:科学出版社,1999:568)
[1] WANG Xixia, GUO Hui, WANG Ding, BAI Yin, YANG Shanwu, HE Xinlai. INFLUENCE OF COHERENT AUSTENITE TWIN BOUNDARIES ON THE VARIANT SELECTION OF BAINITIC FERRITE IN Fe-C-Mn-Si STEELS[J]. 金属学报, 2012, 48(4): 385-392.
[2] LI Fengzhao; AO Qing; GU Yingni; JIANG Jiang; SUN Dongsheng (Shandong University of Technology; Jinan 250061)DAI Jiyan; PENG Hongying (Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015). TEM OBSERVATION OF THE FINE STRUCTURE OF BAINITE[J]. 金属学报, 1997, 33(3): 241-247.
[3] YANG Liu; ZHU Degui; ZHANG Jun; CHEN Jian (Southwestern Jiaotong University; Chengdu). IN SITU OBSERVATION OF GROWTH OF BAINITE IN Fe-Ni ALLOY[J]. 金属学报, 1994, 30(8): 344-347.
[4] JIN Qiang;FANG Hongsheng;CAO Jianjun;ZHENG Yankang;CHEN Xiuyun Tsinghua University; Beijing. LEDGE STRUCTURE AT BROAD FACES OF FERRITE PLATES IN LOWER BAINITE[J]. 金属学报, 1990, 26(6): 5-9.
No Suggested Reading articles found!