Influence of Inclusions on Initiation Of Hydrogen Blister in Iron
REN Xuechong; CHU Wuyang; LI Jinxu; SU Yanjing; QIAO Lijie
Department of Materials Physics; University of Science and Technology Beijing
Cite this article: 

REN Xuechong; CHU Wuyang; LI Jinxu; SU Yanjing; QIAO Lijie. Influence of Inclusions on Initiation Of Hydrogen Blister in Iron. Acta Metall Sin, 2007, 43(7): 673-.

Download:  PDF(812KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:  inclusion      second phase      hydrogen blister      nucleation      iron      
Received:  30 October 2006     
ZTFLH:  TB383  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I7/673

[1]Zaffe C A,Sims C E.Trans AIME,1941;145:225
[2]Hirth J P.Metall Trans,1980;11A:861
[3]Chen L,Xu Y B,Yin W Q.Acta Metall Sin,1978;14: 253 (陈廉,徐永波,尹万全.金属学报,1978;14:253)
[4]Garofalo F,Chou Y T,Ambegaokar V.Aeta Metall,1960; 8:504
[5]Tetelman A S,Robertson W D.Acta Metall,1963;11: 415
[6]Matsui H,Kimura H,Kimura A.Mater Sci Eng,1979;40: 227
[7]Li X G,Dong C F,Li M.J Univ Sci Technol Beijing, 2002;9:130
[8]Wilde B E,Kim C D,Phelps E H.Corrosion,1980;36: 625
[9]Domizzi G,Anteri G,Ovejero-Garcia J.Corros Sci,2001; 43:325
[10]Chu W Y,Gao K W,Huang Y Z,Qiao L J.Corrosion, 2000;56:1046
[11]McLellan R B,Xu Z R.Scr Mater,1997;36:1201
[12]Gavriljuk V G,Bugaev V N,Petrov Y N,Yanchitski B Z. Scr Mater,1996;34:903
[13]Iida T,Yamazaki Y,Kobayashi T,Iijima Y,Fukai Y.Acta Mater,2005;53:3083
[14]Fukai Y,Okuma N.Phys Rev Lett,1994;73:1640
[15]Morishita K,Sugano R,Wirth B D.J Nucl Mater,2003; 323:243
[16]Daw M S,Baskes M I.Phys Rev,1984,29B:6443
[17]Garet M,BraSs A M,Haut C.Corros Sci,1998;40:1073
[1] CHEN Runnong, LI Zhaodong, CAO Yanguang, ZHANG Qifu, LI Xiaogang. Initial Corrosion Behavior and Local Corrosion Origin of 9%Cr Alloy Steel in Cl-Containing Environment[J]. 金属学报, 2023, 59(7): 926-938.
[2] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[3] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[4] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[5] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[6] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[7] SUN Yangting, LI Yiwei, WU Wenbo, JIANG Yiming, LI Jin. Effect of Inclusions on Pitting Corrosion of C70S6 Non-Quenched and Tempered Steel Doped with Ca and Mg[J]. 金属学报, 2022, 58(7): 895-904.
[8] LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun. Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics[J]. 金属学报, 2022, 58(4): 473-485.
[9] LIU Jie, XU Le, SHI Chao, YANG Shaopeng, HE Xiaofei, WANG Maoqiu, SHI Jie. Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel[J]. 金属学报, 2022, 58(3): 365-374.
[10] ZHU Miaoyong, DENG Zhiyin. Evolution and Control of Non-Metallic Inclusions in Steel During Secondary Refining Process[J]. 金属学报, 2022, 58(1): 28-44.
[11] WANG Youde, ZHOU Xiaodong, MA Rui, XU Shanhua. Stochastic Model for Surface Characterization of Structural Steel Corroded in Simulated Offshore Atmosphere[J]. 金属学报, 2021, 57(6): 811-821.
[12] TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan. Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control[J]. 金属学报, 2021, 57(10): 1229-1245.
[13] ZHOU Hongwei, BAI Fengmei, YANG Lei, CHEN Yan, FANG Junfei, ZHANG Liqiang, YI Hailong, HE Yizhu. Low-Cycle Fatigue Behavior of 1100 MPa Grade High-Strength Steel[J]. 金属学报, 2020, 56(7): 937-948.
[14] SUN Feilong, GENG Ke, YU Feng, LUO Haiwen. Relationship of Inclusions and Rolling Contact Fatigue Life for Ultra-Clean Bearing Steel[J]. 金属学报, 2020, 56(5): 693-703.
[15] WEI Shizhong, XU Liujie. Review on Research Progress of Steel and Iron Wear-Resistant Materials[J]. 金属学报, 2020, 56(4): 523-538.
No Suggested Reading articles found!