| Influence of Inclusions on Initiation Of Hydrogen Blister in Iron |
| REN Xuechong; CHU Wuyang; LI Jinxu; SU Yanjing; QIAO Lijie |
| Department of Materials Physics; University of Science and Technology Beijing |
|
Cite this article:
REN Xuechong; CHU Wuyang; LI Jinxu; SU Yanjing; QIAO Lijie. Influence of Inclusions on Initiation Of Hydrogen Blister in Iron. Acta Metall Sin, 2007, 43(7): 673-.
|
|
|
|
|
Received: 30 October 2006
|
|
|
[1]Zaffe C A,Sims C E.Trans AIME,1941;145:225 [2]Hirth J P.Metall Trans,1980;11A:861 [3]Chen L,Xu Y B,Yin W Q.Acta Metall Sin,1978;14: 253 (陈廉,徐永波,尹万全.金属学报,1978;14:253) [4]Garofalo F,Chou Y T,Ambegaokar V.Aeta Metall,1960; 8:504 [5]Tetelman A S,Robertson W D.Acta Metall,1963;11: 415 [6]Matsui H,Kimura H,Kimura A.Mater Sci Eng,1979;40: 227 [7]Li X G,Dong C F,Li M.J Univ Sci Technol Beijing, 2002;9:130 [8]Wilde B E,Kim C D,Phelps E H.Corrosion,1980;36: 625 [9]Domizzi G,Anteri G,Ovejero-Garcia J.Corros Sci,2001; 43:325 [10]Chu W Y,Gao K W,Huang Y Z,Qiao L J.Corrosion, 2000;56:1046 [11]McLellan R B,Xu Z R.Scr Mater,1997;36:1201 [12]Gavriljuk V G,Bugaev V N,Petrov Y N,Yanchitski B Z. Scr Mater,1996;34:903 [13]Iida T,Yamazaki Y,Kobayashi T,Iijima Y,Fukai Y.Acta Mater,2005;53:3083 [14]Fukai Y,Okuma N.Phys Rev Lett,1994;73:1640 [15]Morishita K,Sugano R,Wirth B D.J Nucl Mater,2003; 323:243 [16]Daw M S,Baskes M I.Phys Rev,1984,29B:6443 [17]Garet M,BraSs A M,Haut C.Corros Sci,1998;40:1073 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|