Abstract A theoretical analysis has been made on the effect of deformation above Ae3 temperature to the nucleation of proeutectioid ferrite transformation in low carbon steel. There are two types of influence differentiated by strain, here mainly focuses on one that ε<0.36. The influence of deformation parameters to deformation energy is discussed. The calculation results show that transformation starting temperature and maximum nucleation temperature raises when adding deformation, nucleation rate increases at the same temperature, incubation time becomes shorter, and with increased nucleation rate, finer ferrite can be obtained if grain growth is controlled.
|
|
Received: 18 July 2006
|
|
|
[1]Umemoto M,Tamura I,Otsuka H.Tetsu Hagané,1982; 68(Suppl.):1384 (梅本实,田村今男,大冢秀幸.铁钢,1982;68(增刊): 1384) [2]Ouchi C,Sampei T,Kozasu I.Trans ISIJ,1982;22:214 [3]Lange W F III,Enomoto M,Aaraonson H I.Metall Trans, 1988;19A:427 [4]Bergstrom Y.Rev Powder Metall Phys Ceram,1983;(2): 79 [5]Bodin A,Seitsma J,van der Zwaag S.Scr Mater.2001; 45:875 [6]Cahn J W.Acta Metall,1956;4:449 [7]Yang Z G.Enomoto M.In:Howe J M,Laughlin D E, Lee J K.eds.,Int Conf on Solid-Solid Phase Transfor- mation in Inorganic Materials,Phoenix,Arizona,USA: TMS,2005:47 [8]Enomoto M.Lange III W F.Aaronson H I.Metall Trans, 1986;17A:1399 [9]Ungar T.Scr Mater,2004;51:777 [10]Godfrey A,Hughes D A.Acta Mater,2000;48:1897 [11]Humphreys F J.Scr Mater,2004:51:771 [12]Yu Y N.Principle of Metallurgy.Beijing:Metallurgical Industry Press,2000 (余永宁.金属学,北京;冶金工业出版社,2000) [13]Leeuwen Y.Sietsma J.In:Howe J M,Laughlin D E,Lee J K,eds.,Int Conf on Solid-Solid Phase Transformation in Inorganic Materials,Phoenix,Arizona,USA:TMS,2005: 855 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|