A THEORETICAL ANALYSIS ON EFFECT OF DEFORMATION ABOVE Ae3 TO THE NUCLEATION OF PROEUTECTOID FERRITE TRANSFORMATION
Zhi-Gang YANG;Chao WANG Qi
清华大学材料科学与工程系
Cite this article: 

Zhi-Gang YANG; Chao WANG Qi. A THEORETICAL ANALYSIS ON EFFECT OF DEFORMATION ABOVE Ae3 TO THE NUCLEATION OF PROEUTECTOID FERRITE TRANSFORMATION. Acta Metall Sin, 2007, 43(4): 344-348 .

Download:  PDF(449KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A theoretical analysis has been made on the effect of deformation above Ae3 temperature to the nucleation of proeutectioid ferrite transformation in low carbon steel. There are two types of influence differentiated by strain, here mainly focuses on one that ε<0.36. The influence of deformation parameters to deformation energy is discussed. The calculation results show that transformation starting temperature and maximum nucleation temperature raises when adding deformation, nucleation rate increases at the same temperature, incubation time becomes shorter, and with increased nucleation rate, finer ferrite can be obtained if grain growth is controlled.
Key words:  low carbon steel      deformation energy      nucleation rate      
Received:  18 July 2006     
ZTFLH:  TG142.3  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I4/344

[1]Umemoto M,Tamura I,Otsuka H.Tetsu Hagané,1982; 68(Suppl.):1384 (梅本实,田村今男,大冢秀幸.铁钢,1982;68(增刊): 1384)
[2]Ouchi C,Sampei T,Kozasu I.Trans ISIJ,1982;22:214
[3]Lange W F III,Enomoto M,Aaraonson H I.Metall Trans, 1988;19A:427
[4]Bergstrom Y.Rev Powder Metall Phys Ceram,1983;(2): 79
[5]Bodin A,Seitsma J,van der Zwaag S.Scr Mater.2001; 45:875
[6]Cahn J W.Acta Metall,1956;4:449
[7]Yang Z G.Enomoto M.In:Howe J M,Laughlin D E, Lee J K.eds.,Int Conf on Solid-Solid Phase Transfor- mation in Inorganic Materials,Phoenix,Arizona,USA: TMS,2005:47
[8]Enomoto M.Lange III W F.Aaronson H I.Metall Trans, 1986;17A:1399
[9]Ungar T.Scr Mater,2004;51:777
[10]Godfrey A,Hughes D A.Acta Mater,2000;48:1897
[11]Humphreys F J.Scr Mater,2004:51:771
[12]Yu Y N.Principle of Metallurgy.Beijing:Metallurgical Industry Press,2000 (余永宁.金属学,北京;冶金工业出版社,2000)
[13]Leeuwen Y.Sietsma J.In:Howe J M,Laughlin D E,Lee J K,eds.,Int Conf on Solid-Solid Phase Transformation in Inorganic Materials,Phoenix,Arizona,USA:TMS,2005: 855
[1] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[2] Canshuai LIU,Zhaohui TIAN,Zhiming ZHANG,Jianqiu WANG,En-Hou HAN. Corrosion Behaivour of X65 Low Carbon Steel During Redox State Transition Process of High LevelNuclear Waste Disposal[J]. 金属学报, 2019, 55(7): 849-858.
[3] WEN Huailiang, DONG Junhua, KE Wei, CHEN Wenjuan, YANG Jingfeng, CHEN Nan. ACTIVE/PASSIVE BEHAVIOR OF LOW CARBON STEEL IN DEAERATED BICARBONATE SOLUTION[J]. 金属学报, 2014, 50(3): 275-284.
[4] GAO Zhongtang, HU Rui, WANG Jun, YANG Jieren, LI Jinshan. EFFECT OF ELECTROMAGNETIC MELT TREATMENT NEAR LIQUIDUS ON THE FORMATION OF NON-DENDRITE MICROSTRUCTURE OF SUPERALLOY[J]. 金属学报, 2014, 50(12): 1471-1477.
[5] ZHANG Ruihui, ZHANG Chi, XIA Zhixin, YANG Zhigang. OPTIMIZING CONTROL OF PRECIPITATES IN T91 FERRITIC HEAT-RESISTAN STEEL[J]. 金属学报, 2013, 49(9): 1075-1080.
[6] HOU Ziyong XU Yunbo WU Di. RECRYSTALLIZATION OF ULTRA-LOW CARBON STEEL SHEET AFTER ULTRA-RAPID ANNEALING[J]. 金属学报, 2012, 48(9): 1057-1066.
[7] REN Yongqiang XIE Zhenjia SHANG Chengjia. REGULATION OF RETAINED AUSTENITE AND ITS EFFECT ON THE MECHANICAL PROPERTIES OF LOW CARBON STEEL[J]. 金属学报, 2012, 48(9): 1074-1080.
[8] XU Hengdong ZHAO Haiyan S¨orn Ocylok Igor Kelbassa. STUDY ON CRACKS IN LASER DIRECT–CLADDED TITANIUM LAYER ON LOW CARBON STEEL[J]. 金属学报, 2012, 48(2): 142-147.
[9] ZHANG Peng ZHANG Fucheng WANG Tiansheng. PREPARATION AND MICROSTRUCTURE OF HARD BAINITE IN SURFACE LAYER OF CARBURIZED 20CrMnMoAl STEEL[J]. 金属学报, 2011, 47(8): 1038-1045.
[10] YANG Jingfeng DONG Junhua KE Wei CHEN Nan. INFLUENCE OF pH VALUES AND CORROSION PRODUCTS ON LOW CARBON STEEL CORROSION SUSCEPTIBILITY IN BORATE BUFFER SOLUTION[J]. 金属学报, 2011, 47(2): 152-156.
[11] YANG Jingfeng DONG Junhua KE Wei. EFFECTS OF SO42− AND Cl− ON ACTIVE/PASSIVE CORROSION BEHAVIORS OF LOW CARBON STEEL IN DEAERATED BICARBONATE SOLUTION[J]. 金属学报, 2011, 47(10): 1321-1326.
[12] LIU Guangzhou WANG Jianming ZHANG Jianqing CAO Chunan. EFFECT OF ELECTROLYTIC TREATMENT OF BALLAST WATER ON CORROSION BEHAVIOR OF TANK STEEL[J]. 金属学报, 2010, 46(9): 1093-1097.
[13] ZHANG Changli Michel Bellet Manuel Bobadilla SHEN Houfa LIU Baicheng. FINITE ELEMENT MODELLING OF TENSILE TEST FOR MICRO–ALLOYED LOW CARBON STEEL AT HIGH TEMPERATURE[J]. 金属学报, 2010, 46(10): 1206-1214.
[14] CUI Guibin GUO Hui YANG Shanwu HE Xinlai. INFLUENCE OF INTERFACE BETWEEN GRAIN BOUNDARY FERRITE AND PRIOR AUSTENITE ON BAINITE TRANSFORMATION IN A LOW CARBON STEEL[J]. 金属学报, 2009, 45(6): 680-686.
[15] ZHAO Heshan; LI Dianzhong; LIU Zhaoxia; LI Yiyi. INVESTIGATION ON DIFFUSION OF CARBON ATOMS AND STABILITY OF DEFORMATION INDUCED FERRITE IN A LOW CARBON STEEL[J]. 金属学报, 2007, 43(3): 286-290 .
No Suggested Reading articles found!