Domain switching and indentation crack propagating in BaTiO3 single crystal induced by etching
WANG Ruimin; CHU Wuyang; SU Yanjing; GAO Kewei; QIAO Lijie
Department of Materials Physics; University of Science & Technology Beijing; Beijing 100083
Cite this article:
WANG Ruimin; CHU Wuyang; SU Yanjing; GAO Kewei; QIAO Lijie. Domain switching and indentation crack propagating in BaTiO3 single crystal induced by etching. Acta Metall Sin, 2005, 41(3): 297-301 .
Abstract Etching-enhanced 90º domain switching and indentation crack
propagating in BaTiO3 single crystal have been investigated using poled and unpoled
samples, respectively. The results show that if the poled direction
[001] lies in the (100) indentation plane, etching in
HCl+HF solution causes the average length of
16 indentation cracks to increase from (140±17)μm to
(211±26)μm, i.e., 50% increment. At the same time,
the 90º domain switching zones surrounded by the
indentation cracks increase also evidently after etching.
The reason is due to chemisorption of etching molecular
decreasing surface energy. If Vicker's indention is
carried out in the pre-etched surface, the average crack
length and the size of the domain switching zones are
the same with those of etching after indentation. If the [001]
poling direction is normal to the indentation plane,
there is no effect of etching on the
domain switching zone and crack length.
For unpoled sample, etching increases the
domain switching zone and the crack length
from (150±21) μm to (182±30)
μm, i.e., about 20% increment.
[1] Busche M J, Hsia K J. Scr Mater, 2001; 44: 207 [2] Fang F, Yang W. Mater Lett, 2002; 57: 198 [3] Yang W. Mechatronic Reliability. Beijing: Tsinghua University Press, 2001: 96 (杨卫.力电失效学.北京:清华大学出版社, 2001:96) [4] Geramita A V, Seberry J. Orthogonal Designs: Quadratic Forms and Hadamard Matrices. New York: Marcel Dekker, 1979 [5] Wang R M, Chu W Y, Gao K W, Su Y J, Qiao L J. Mater Lett, 2004; 58: 1811 [6] Wang Y, Chu W Y , Su Y J, Qiao L J. Mater Sci Eng, 2002; B59: 263 [7] Chantikul P, Anstis G R, Lawn B R, Marshall D B. J Am Ceram Soc, 1981; 64: 539 [8] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Fracture. Beijing: Science Press, 2000: 10 (褚武扬,乔利杰,陈奇志,高克玮.断裂与环境断裂.北京: 科学出版社,2000:10)