| As--Cast Microstructure and its Formation Mechanism in Mg-Based Alloys Containing Ca And Si |
| AI Yanling; LUO Chengping; LIU Jiangwen; HUANG Yanfei |
| College of Mechanical Engineering; South China University of Technology; Guangzhou 510641 |
|
Cite this article:
AI Yanling; LUO Chengping; LIU Jiangwen; HUANG Yanfei. As--Cast Microstructure and its Formation Mechanism in Mg-Based Alloys Containing Ca And Si. Acta Metall Sin, 2005, 41(1): 49-.
|
|
|
Abstract The as--cast microstructure of Mg-based alloys containing Ca and Si was investigated
using optical microscopy, XRD, SEM/EDS and TEM. It was found that the alloy containing low Si
consisted of Mg-rich matrix and CaMgSi phase, while the alloy containing higher Si consisted of
Mg2Si besides the Mg-rich matrix and CaMgSi. The phase CaMgSi existed in three different
morphologies, namely discrete large angular, dispersive dot-like, and
needle-like, while the Mg2Si,
also needle-like, existed in the “Chinese-script” colonies. The
formation mechanism of the as-cast
microstructure was discussed in details based on a proposed
pseudo-ternary Mg-Mg2Si-CaMgSi phase
diagram.
|
|
Received: 09 August 2004
|
|
|
[1] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37 [2] Carbonneau Y, Couture A, van Neste A, Tremblay R. Metall Mater Trans, 1998; 29A: 1759 [3] You B S, Park W W, Chung I S. Scr Mater, 2000; 42:1089 [4] Kim J J, Kim D H, Skin K S , Kim N J. Scr Mater, 1999;41: 333 [5] Yuan G Y, Liu Z L, Wang Q D, Ding W J. Mater Lett,2002; 56: 53 [6] Yuan G Y, Liu M P, Ding W J, Akihisa I. Mater Sci Eng,2003; A357: 314 [7] Nie J F, Muddle B C. Scr Mater, 1997; 37: 1475 [8] Bronfin B, Katsir M, Aghion E. Mater Sci Eng, 2001;A302: 46 [9] Villars P, Prince A, Okumoto H. Handbook of TernaryAlloy Phase Diagram. ASM International, 1995: 66 [10] Matsui H, Kuramoto M, Ono T, Nose Y, Tatsuoka H, Ki-wabara H. J Cryst Growth, 2002; 237-239: 2121 [11] Hosono J, Kuramoto M. Appl Surf Sci, 2003; 216: 620 [12] Luo C P, Weatherly G C. Acta Metall, 1963; 35: 1987 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|