Intelligent Expert System Used in Gear Material Selection and its Heat Treatment |
LI Xincheng; CHEN Guang; ZHU Weixing; WANG Yun; ZHANG KAihua; WANG Jianmin |
School of Mechanical Engineering; Jiangsu Univercity; Zhenjiang 212013 |
|
Cite this article:
LI Xincheng; CHEN Guang; ZHU Weixing; WANG Yun; ZHANG KAihua; WANG Jianmin. Intelligent Expert System Used in Gear Material Selection and its Heat Treatment. Acta Metall Sin, 2004, 40(10): 1051-1054 .
|
Abstract The characters and weakness of expert system (ES) and artificial neural
networks (ANN) have been analyzed. The ANN were led into gear materials
selection and heat treatment ES, and 2-grades back propagation (BP)
ANN model which has conquered the weakness of traditional ES has been
established. This system contains large quantity of knowledge of gear
materials and heat treatment process.
|
Received: 22 October 2003
|
|
[1] Zakarian V I, Kaiser M J. Expert System Appl, 1999; 16: 233 [2] Mizoguchi R. IEEE Expert, 1995; 8: 23 [3] Kim H S, Im Y T. Mater Proc Technol, 1999; 95: 262 [4] Chan Y W. Computer Appl Technol, 1998; 11: 66 [5] Sonar R M. Expert System Appl, 1999; 17: 45 [6] Phillip W G. Eng Appl Artificial Intelligence, 1996; 2: 163 [7] Lucas W. Weld World, 1994; 34: 9 [8] Andrew R G, Paul S R. Artificial Intelligence, 1996; 87:215 [9] ASM Handbook Committee. Metal Handbook (Vol.6) .New York: McGraw-Hill, 1996: 158 [10] Lange K. Handbook of Metal Forming. New York:McGraw-Hill, 1995: 116 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|