Influence Of Zinc Content And Surface Contamination On The Electrochemical Behaviors Of Epoxy Zinc--Rich Primer
XIE Deming;HU Jiming; TONG Shaoping
Institute for Thermal Power Engineering; Zhejiang University
Cite this article: 

XIE Deming; HU Jiming; TONG Shaoping. Influence Of Zinc Content And Surface Contamination On The Electrochemical Behaviors Of Epoxy Zinc--Rich Primer. Acta Metall Sin, 2004, 40(1): 103-108 .

Download:  PDF(191KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of zinc powder content and contamination of epoxy zinc--rich primer/substrate interface on the protective performance of the zinc--rich coatings was investigated by means of electrochemical impedance spectroscopy (EIS) and corrosion potential monitoring.The degradation mechanism of the zinc—rich coatings was elucidated.It was shown that effective barrier can not be formed in the coatings with low zinc content. The attack of zinc particles in zinc--rich coatings is explained in terms of diffusion control through the film of zinc corrosion products around the zinc particles. The surface contamination of the substrate is vital to the performance of the organic coatings protecting the substrate steel. The surface contamination will lead to not only the impairment of the performance of the zinc—rich coatings but also the acceleration of the degradation processes of the steel substrate.
Key words:  epoxy zinc--rich primer      electrochemical impedance spectroscopy      
Received:  01 January 1900     
ZTFLH:  TG174  
  O646  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I1/103

[1] Du C S. Corros Protect, 1999; 20(4) : 168, 153 (杜存山.腐蚀与防护.1999;20(4) :168,153)
[2] Kendig M K, Jeanjaquet S L, White J, Momsfeld F. Corrosion Protection by Organic Coatings. Vol. 87-2, Thousand Oaks, CA USA: The Electrochemical Society, 1987: 253
[3] Hare C H. J Protect Coat Linings, 1998; 15(8) : 29
[4] Zhang J Q, Cao C N. Corros Protect, 1998; 19(3) : 99 (张鉴清,曹楚南.腐蚀与防护,1998;19(3) :99)
[5] Feliu S, Barajas R, Bastidas J M, Morcillo M. J Coat Technol, 1989; 61(775) : 63
[6] Feliu S, Barajas R, Bastidas J M, Morcilto M. J Coat Technol, 1989; 61(775) : 71
[7] Uhlig H H, Revie R W. Corrosion and Corrosion Control. 3rd ed., New York: Wiley, 1985: 227
[8] Almeida E, Pereira D, Cabral A M, Morcillo M. J Oil Color Chem Associat, 1991; 21
[9] Faidi S E, Scantlebury J D, Bullivant P. Corros Sci, 1993; 35: 1319
[10] Feliu S Jr, Morcillo M, Feliu S. Corrosion, 2001; 57: 591
[11] Frydrych P J, Farrington G C, Townsend H E. Proc Electrochem Soc, 1987; 87(2) : 240
[12] Novoa X R, Izquierdo M, Merino P, Espada L, Mater Sci Forum, 1989; 44-45: 223
[13] Gervasi C A, Di Sarli A R, Cavalcanti E, Ferraz P. Bucharsky E C, Real S G, Vilche J R. Corros Sci, 1994; 36: 1963
[14] Izquierdo M, Novoa X R, Pena G, Espada L. Mater Sci Forum, 1992; 111-112: 257
[15] Zhang J Q. J Chin Soc Corros Protect, 1996; 16: 175 (张鉴清.中国腐蚀与防护学报, 1996: 16: 175)
[16] Hare Clive H. Paint Coat, 1982; (4) : 48
[17] Hare Clive H. Wright S J. J Coat Technol, 1982; 54(693) : 65
[18] Giudice C B, Linares M M. Surf Coat Int, 1997; (6) : 279
[19] Feliu S Jr, Morcillo M, Bastidas J M, Feliu S. J Coat Technol, 1991; 63(793) : 31
[20] Abreu C M, Izquierdo M, Keddam M, Novoa X R, Takenouti H. Electrochim Acta, 1996; 41: 2405
[21] Morcillo M, Barajas R, Feliu S, Bastidas J M. J Mater Sci, 1990; 25: 2441
[22] Xie D M. Ph D Thesis, Zhejiang University, Hangzhou, 2002: 32(谢德明.浙江大学博士学位论文,杭州,2002:32)
[1] BAI Yang, WANG Zhenhua, LI Xiangbo, LI Yan. Corrosion Behavior of Al(Y)-30%Al2O3 Coating Fabricated by Low Pressure Cold Spray Technology[J]. 金属学报, 2019, 55(10): 1338-1348.
[2] WEI Renchao, XU Fengling, LIN Cunguo, TANG Xiao, LI Yan. CORROSION BEHAVIOR OF B10 ALLOY EXPOSED TO SEAWATER CONTAINING VIBRIO AZUREUS, SULFATE-REDUCING BACTERIA, AND THEIR MIXTURE[J]. 金属学报, 2014, 50(12): 1461-1470.
[3] FU Xinxin, DONG Junhua, HAN En-hou, KE Wei. ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY MONITORING ON MILD STEEL Q235 IN SIMULATED INDUSTRIAL ATMOSPHERIC CORROSION ENVIORNMENT[J]. 金属学报, 2014, 50(1): 57-63.
[4] ZHOU Xiaowei,SHEN Yifu. CORROSION BEHAVIOR AND EIS STUDY OF NANOCRYSTALLINE Ni-CeO2 COATINGS IN AN ACID NaCl SOLUTION[J]. 金属学报, 2013, 49(9): 1121-1130.
[5] ZHAO Bo DU Cuiwei LIU Zhiyong LI Xiaogang YANG Jike LI Yueqiang. CORROSION BEHAVIOR OF X80 STEEL IN YINGTAN SOIL SIMULATED SOLUTION UNDER DISBONDED COATING[J]. 金属学报, 2012, 48(12): 1530-1536.
[6] ZHANG Jie SONG Xiuxia LUAN Xin SUN Caixia DUAN Jizhou HOU Baorong . EFFECTS OF SHEWANELLA ALGAE ON CORROSION OF Zn–Al–Cd ANODE[J]. 金属学报, 2012, 48(12): 1495-1502.
[7] ZHU Xuemei CAO Xuemei LIU Ming LEI Mingkai ZHANG Yansheng. AN ANTIFERROMAGNETIC Fe24Mn4Al5Cr COVAR ALLOY IMPULSE--PASSIVATED BY AN ALTERNATING CURRENT VOLTAGE OVERLAPPING A DIRECT CURRENT VOLTAGE AND ITS CORROSION RESISTANCE[J]. 金属学报, 2012, 48(11): 1357-1364.
[8] WANG Changgang DONG Junhua KE Wei CHEN Nan. EFFCTS OF pH AND Cl− CONCENTRATION ON THE CORROSION BEHAVIOR OF COPPER IN BORIC ACID BUFFER SOLUTION[J]. 金属学报, 2011, 47(3): 354-360.
[9] SONG Lixiao ZHANG Zhao ZHANG Jianqing CAO Chunan. ELECTROPLATING MECHANISM OF NANOSTRUCTURED BLACK Ni FILMS[J]. 金属学报, 2011, 47(1): 123-128.
[10] SHI Jinjie SUN Wei GENG Guoqing. INFLUENCE OF CARBONATION ON THE CORROSION PERFORMANCE OF STEEL HRB335 IN SIMULATED CONCRETE PORE SOLUTION[J]. 金属学报, 2011, 47(1): 17-24.
[11] YANG Bo LI Moucheng YAO Meiyi ZHOU Bangxin SHEN Jianian. IN SITU IMPEDANCE CHARACTERISTICS OF ZIRCONIUM ALLOY CORROSION IN HIGH TEMPERATURE AND PRESSURE WATER ENVIRONMENT[J]. 金属学报, 2010, 46(8): 946-950.
[12] ZHOU Jianlong LI Xiaogang DU Cuiwei LI Yunling LI Tao PAN Ying. ANODIC ELECTROCHEMICAL BEHAVIOR OF X80 PIPELINE STEEL IN NaHCO3 SOLUTION[J]. 金属学报, 2010, 46(2): 251-256.
[13] ZHANG Jie LIU Fengling LI Weihua DUAN Jizhou HOU Baorong. EFFECTS OF SRB ON CORROSION OF Zn–Al–Cd ANODE IN MARINE SEDIMENT[J]. 金属学报, 2010, 46(10): 1250-1257.
[14] . EFFECT OF RE (RARE EARTH) ON THE CORROSION RESISTANCE OF CARBON STEEL IN 0.3 mol/L NACL SOLUTION[J]. 金属学报, 2008, 44(7): 863-866 .
[15] ;. SURFACE MODIFICATION OF 316L STAINLESS STEEL BY HIGH CURRENT PULSED ELECTRON BEAM Part II Corrosion behaviors in the simulated body fluid[J]. 金属学报, 2007, 42(1): 71-76 .
No Suggested Reading articles found!