Research Of The Equaxied Dendritic Growth In The Undercooled Melt Of The Pure Metal By Phase--Field Method
LI Xinzhong; GUO Jingjie; SU Yanqing; JIA Jun
Cite this article:
LI Xinzhong; GUO Jingjie; SU Yanqing; JIA Jun. Research Of The Equaxied Dendritic Growth In The Undercooled Melt Of The Pure Metal By Phase--Field Method. Acta Metall Sin, 2004, 40(1): 31-35 .
Abstract A new way to improve computational efficiency of phase field is used to simulate the evolution of the equiaxed dendritic growth morphology in pure metal melt with initial dimensionless supercooling of 0.55. Much information about equiaxed dendritic growth has been got, which is in good agreement with experimental observation. The births of second arms and third arms have been simulated successfully by adding appropriate thermal noise. Furthermore, the dimensionless velocity and radius of the equiaxed dendritic axis' tip, and the Peclet number are computed, and the computational results by phase--field method are in good agreement with the ones by the microsolvability theory and the Ivantsov theory.
[1] Chen W C, Chien L C. J Synthetic Cryst, 2002; 31:245(陈万春,简来成.人工晶体学报.2002;31:245) [2] Wheeler A A, Murray B T, Schaefer R J. Physica, 1993; 66D: 243 [3] Wang S L, Sekerka R F, Wheeler A A, Murray B T, Coriell S R, Rraun R J, McFadden G B. Physica, 1993; 69D: 189 [4] Warren J A, Boettinger W I. Acta Metal Mater, 1995; 43: 689 [5] McCarthy J F. Acta Mater, 1997; 45:4077 [6] Wheeler A A, Boettinger W J, McFadden G B. Phys Rev, 1992; 47E: 1893 [7] Kobayashi R. Physica, 1993; 63D: 410 [8] Karma A, Rappel W-J. Phys Rev, 1997; 57E: 4323 [9] Beckermann C, Diepers H J, Steinbach I, Karma A, Tong X. J Computat Phys, 1999; 154 [10] Karma A, Rappel W J. Phys Rev, 1999; 60E: 3614 [11] Provatas N, Goldendeld N, Jonathan D. Phys Rev Lett, 1998; 80:3308 [12] Zhao D P, Jing T. Acta Metall Sin, 2002; 38:1238(赵代平,荆涛.金属学报,2002;12:1238) [13] Tong X, Beckermann C, Karma A. Weld Adv Solidific Processes. 1998:613 [14] Ivantsov G P, Dokl. Akada Nank USSR, 1974; 58:567 [15] Karma A, Rappel W J. Phys Rev, 1996; 53E: 3017 [16] Glicksman. Metal Mater Sci Eng, 1984; 65:45 [17] Hu H Q. Principle of Metal Solidification. Beijing: Machinery Press, 2000:127(胡汉起.金属凝固原理.北京:机械工业出版社.2000:127)h