Nucleation At Plane Front In Directionally Solidified Peritectic Alloys
LI Shuangming; LIU Lin; LI Xiaoli; FU Hengzhi
State Key Laboratory of Solidification Processing; Northwestern Polytechnical University
Cite this article: 

LI Shuangming; LIU Lin; LI Xiaoli; FU Hengzhi. Nucleation At Plane Front In Directionally Solidified Peritectic Alloys. Acta Metall Sin, 2004, 40(1): 20-26 .

Download:  PDF(185KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The directionally solidified microstructures of peritectic alloys are affected markedly by the nucleation and growth conditions. By using nucleation and constitutionalsupercooling criterion and assuming that the maximum interface growth temperature of phase growth is more stability in the directional solidification process, the composition range is theoretically developed for predicting the nucleation at the plane-front growth of properitectic and peritectic phases in an initial transient zone. The band--like microstructure occurs as a function of solidification distance and composition range is described on the basis of the purely diffusivemodel. The calculated results of Fe--Ni and Pb--Bi peritectic alloys are in agreement with their experimental data.
Key words:  constitutional supercooling      directional solidification      
Received:  01 January 1900     
ZTFLH:  TG111.4  
  TG132.32  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I1/20

[1] Kerr H W, Kurz W. Inter Mater Rev, 1996; 41:129
[2] Barker N J W, Hellawell A. Metal Sci, 1974; 8:353
[3] Brody H D, David S A. Int Conf on Solidification and Casting, Institute of Metals, London, 1977:144
[4] Tichener A P, Spittle J A. Acta Metall, 1975; 23:497
[5] Ostowski A, Langer E W. Int Conf on Solidification and Casting, Institute of Metals, London, 1977:139
[6] Boettinger W J. Metall Trans, 1974; 5:2203
[7] Trivedi R. Metall Mater Trans, 1995; 26A: 1583
[8] Zeissler M K, Lograsso T. Metall Mater Trans, 1997; 28A: 1543
[9] Kurz W, Trivedi R. Metall Mater Trans, 1996; 27A: 625
[10] Tokieda K, Yasuda H, Ohnaka I. Mater Sci Eng, 1999; A262:241
[11] Karma A, Rappel W J, Fuh B C, Trivedi R. Metall Mater Trans, 1998; 29A: 1457
[12] Trivedi R, Park J S. J Cryst Growth, 2002; 235:572
[13] Hunziker O, Vandyoussefi M. Kurz W. Acta Mater, 1998; 46:6325
[14] Tiller W A. The Science of Crystallization: Macroscopic Phenomena and Defect Generation. Cambribge: Cambridge University Press, 1991:143
[15] Hu H Q. Solidification Principle of Metals. The 2nd edition. Beijing: Machinary Industry Press, 2000:114(胡汉起.金属凝固原理.第2版,北京:机械工业出版社,2000:114)
[16] Umeda T. Okane T, Kurz W. Acta Mater, 1996; 44:4214
[17] Umeda T, Okane T. Sci Technol Adv Mater, 2001; 2:239
[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[4] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[5] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[6] ZHANG Xiaoli, FENG Li, YANG Yanhong, ZHOU Yizhou, LIU Guiqun. Influence of Secondary Orientation on Competitive Grain Growth of Nickel-Based Superalloys[J]. 金属学报, 2020, 56(7): 969-978.
[7] ZHANG Jian,WANG Li,WANG Dong,XIE Guang,LU Yuzhang,SHEN Jian,LOU Langhong. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2019, 55(9): 1077-1094.
[8] XU Qingyan,YANG Cong,YAN Xuewei,LIU Baicheng. Development of Numerical Simulation in Nickel-Based Superalloy Turbine Blade Directional Solidification[J]. 金属学报, 2019, 55(9): 1175-1184.
[9] Hui FANG,Hua XUE,Qianyu TANG,Qingyu ZHANG,Shiyan PAN,Mingfang ZHU. Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification:[J]. 金属学报, 2019, 55(5): 664-672.
[10] Yan YANG, Guangyu YANG, Shifeng LUO, Lei XIAO, Wanqi JIE. Microstructures and Growth Orientation of Directionally Solidification Mg-14.61Gd Alloy[J]. 金属学报, 2019, 55(2): 202-212.
[11] JIN Hao, JIA Qing, LIU Ronghua, XIAN Quangang, CUI Yuyou, XU Dongsheng, YANG Rui. Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy[J]. 金属学报, 2019, 55(12): 1519-1526.
[12] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[13] Jincheng WANG, Chunwen GUO, Junjie LI, Zhijun WANG. Recent Progresses in Competitive Grain Growth During Directional Solidification[J]. 金属学报, 2018, 54(5): 657-668.
[14] Guang CHEN, Gong ZHENG, Zhixiang QI, Jinpeng ZHANG, Pei LI, Jialin CHENG, Zhongwu ZHANG. Research Progress on Controlled Solidificationand Its Applications[J]. 金属学报, 2018, 54(5): 669-681.
[15] Huijun KANG, Jinling LI, Tongmin WANG, Jingjie GUO. Growth Behavior of Primary Intermetallic Phases and Mechanical Properties for Directionally Solidified Al-Mn-Be Alloy[J]. 金属学报, 2018, 54(5): 809-823.
No Suggested Reading articles found!