| Polythermal Projection Of Primary Al--Cu--Fe Icosahedral Quasicrystal Phase And The Related Crystal Phase |
| ZHAO Dongshan; QU Wenbang; WANG Renhui |
| Materials Engineering College; Zhengzhou University |
|
Cite this article:
ZHAO Dongshan; QU Wenbang; WANG Renhui. Polythermal Projection Of Primary Al--Cu--Fe Icosahedral Quasicrystal Phase And The Related Crystal Phase. Acta Metall Sin, 2004, 40(1): 14-19 .
|
|
|
Abstract A series of Al--Cu--Fe alloys with compositions ofAl48-60Cu33-50Fe0-10 was prepared and the phase constituents in thesealloys quenched from various temperatures were identified by using XRD, SEM, EDXS and EBSD attached to SEM, and TEM (including HRTEM). Compared with the polythermal projection proposed by Gayle et al, a main amendment is to divide the previous φ--region into β+φ two regions. A new ternary reaction is the quasiperitectic at U8: L+βIQC+φ.EDXS reveals that the composition of φ phase with Ni2Al3 structure is in Al47.3-50.6Cu45.4-48.1Fe4.5-5.2,and its center composition is Al47.9Cu47.1Fe5.0.
|
|
Received: 17 December 2002
|
|
|
[1] Bradley A J, Goldschmidt H J. J Inst Met, 1939; 65:403 [2] Gayle F W, Shapiro A J, Biancaniello F S, Boettinger W J. Metall Trans, 1992; 23A: 2409 [3] Tsai A P, Inoue A, Masumoto A. J Mater Sci Lett, 1987; 6:1403 [4] Calvayrac Y, Quivy A, Bessiere M, Lefebvre S, Quiquandon M C, Gratias D. J Phys I France, 1990; 51:417 [5] Faudot F. Ann Chim Fr, 1993; 18:445 [6] Grushko B, Wittenberg R, Holland-Moritz D. J Mater Res, 1996; 11:2177 [7] Gui J, Wang J, Wang R, Wang D, Liu J, Chen F. J Mater Res, 2001; 16:1037 [8] Dong C. Quasicrystal Materials. Beijing: China National Defence Industry Press, 1998:47(董闯.准晶材料.北京:国防工业出版社,1998:47) [9] Zhang R K, Wang J B, Wang D H, Liu J, Chen F Y, Chen X M, Gui J N, Wang R H. Acta Metall Sin, 1999; 35:463(张瑞康,王建波,汪大海,刘静,陈方玉,陈小梅,桂嘉年,王仁卉.金属学报,1999;35:463) [10] Lee S M, Jeon H J, Kim B H, Kim W T, Kin D H. Mater Sci Eng, 2001; (304-306) A: 871 [11] Zhao D S, Wang R H, Gui J N, Shen N F, Qu W B, Guo X Y, Wu Z S, Zhang Z J, Sun L H. J Chin Electron Microscopy Soc, 2002; 21:455(赵东山,王仁卉,桂嘉年,沈宁福,瞿文榜,郭新勇,吴志申,张治军,孙丽虹.电子显微学报,2002;21:455) [12] Zhang L M, Luck R. J Alloys Compd, 2001; 342:53 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|