Abstract The directionally solidified microstructures of peritectic alloys are affected
markedly by the nucleation and growth conditions. By using nucleation and constitutionalsupercooling criterion and assuming that the maximum interface growth temperature of phase growth is more stability in the directional solidification process, the composition range is theoretically developed for predicting the nucleation at the plane-front growth of properitectic and peritectic phases in an initial transient zone. The band--like microstructure occurs as a function of
solidification distance and composition range is described on the basis of the purely diffusivemodel. The calculated results of Fe--Ni and Pb--Bi peritectic alloys are in agreement with their experimental data.
|
|
Received: 01 January 1900
|
|
|
[1] Kerr H W, Kurz W. Inter Mater Rev, 1996; 41:129 [2] Barker N J W, Hellawell A. Metal Sci, 1974; 8:353 [3] Brody H D, David S A. Int Conf on Solidification and Casting, Institute of Metals, London, 1977:144 [4] Tichener A P, Spittle J A. Acta Metall, 1975; 23:497 [5] Ostowski A, Langer E W. Int Conf on Solidification and Casting, Institute of Metals, London, 1977:139 [6] Boettinger W J. Metall Trans, 1974; 5:2203 [7] Trivedi R. Metall Mater Trans, 1995; 26A: 1583 [8] Zeissler M K, Lograsso T. Metall Mater Trans, 1997; 28A: 1543 [9] Kurz W, Trivedi R. Metall Mater Trans, 1996; 27A: 625 [10] Tokieda K, Yasuda H, Ohnaka I. Mater Sci Eng, 1999; A262:241 [11] Karma A, Rappel W J, Fuh B C, Trivedi R. Metall Mater Trans, 1998; 29A: 1457 [12] Trivedi R, Park J S. J Cryst Growth, 2002; 235:572 [13] Hunziker O, Vandyoussefi M. Kurz W. Acta Mater, 1998; 46:6325 [14] Tiller W A. The Science of Crystallization: Macroscopic Phenomena and Defect Generation. Cambribge: Cambridge University Press, 1991:143 [15] Hu H Q. Solidification Principle of Metals. The 2nd edition. Beijing: Machinary Industry Press, 2000:114(胡汉起.金属凝固原理.第2版,北京:机械工业出版社,2000:114) [16] Umeda T. Okane T, Kurz W. Acta Mater, 1996; 44:4214 [17] Umeda T, Okane T. Sci Technol Adv Mater, 2001; 2:239 |