Abstract Columnar grain Al samples with 001uv0
orientations were cold rolled to reductions of
10%, 30% and 50%, respectively. The macroscopic subdivision of grains with different orientations was
characterized in detail by using EBSP technique. It is
found that the macroscopic subdivision patterns of
different oriented grains are different. A model
based on dislocation slip was used to analyze
the observed macroscopic subdivision patterns.
|
|
Received: 24 July 2003
|
|
|
[1] Hansen N. Metall Mater Trans A, 2001; 32A: 2917 [2] Hansen N, Juul Jensen D. Proc R Soc Land A, 1999;357:.1447 [3] Wert J, Liu Q, Hansen N. Acta Mater, 1995; 43: 4153 [4] Liu Q, Hansen N. Proc R Soc Land A, 1998; 454: 2555 [5] Liu Q, Wert J, Hansen N. Acta Mater, 2000; 48: 4267 [6] Wert J. Acta Mater, 2002; 50: 3125 [7] Liu Q, Maurice C, Driver D, Hansen N. Metall MaterTrans, 1998; 29A: 2333 [8] Basson F, Driver J H. Acta Mater, 2000; 48: 2101 [9] Li Z J, Godfrey A, Liu Q. Scr Mater, 2001; 45: 847 [10] Kuhlmann-Wilsdorf D, Hansen N. Scr Metall, 1991; 25:1557 [11] Bay B, Hansen N, Hughes D A, Kuhlmann-Wilsdorf D.Acta Metall Mater, 1992; 40: 205 [12] Hughes D A, Hansen N. Metall Trans, 1993; 24A: 2021 [13] Liu Q, Juul Jensen D, Hansen N. Acta Mater, 1997; 46:5819 [14] Liu Q. J Appl Cryst, 1994; 27: 755 [15] Liu Q. Ultramicroscopy, 1995; 60: 81 [16] Delannay L, Mishin O V, Juul Jensen D, Van Houtte P.Acta Mater, 2001; 49: 2441 [17] Hurley P J, Humphrey F J. Acta Mater, 2003; 51: 1087 [18] Wert J, Liu Q, Hansen N. Acta Mater, 1997; 45: 2565 [19] Krieger Lassen N C, Juul Jensen D, Conradsen K. ActaCrystall, 1994; A50: 741 [20] Tucker G E G. Acta Metall, 1964; 12: 1093V |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|