Acta Metall Sin  2020, Vol. 56 Issue (4): 411-428    DOI: 10.11900/0412.1961.2019.00381
Current Issue | Archive | Adv Search |
A Review of Current State and Prospect of the Manufacturing and Application of Advanced Hot Stamping Automobile Steels
JIN Xuejun1(),GONG Yu1,HAN Xianhong1,DU Hao1,DING Wei1,ZHU Bin2,ZHANG Yisheng2,FENG Yi3,MA Mingtu3,LIANG Bin3,ZHAO Yan3,LI Yong4,ZHENG Jinghua4,SHI Zhusheng4
1.School of Materials Science and Engineering, Shanghai Jiaotong University, Shanghai 200240, China
2.School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan 430074, China
3.China Automotive Engineering Research Institute Co. , Ltd. , Chongqing 401122, China
4.Department of Mechanical Engineering, Imperial College London, London SW7 2AZ, UK
Cite this article: 

JIN Xuejun,GONG Yu,HAN Xianhong,DU Hao,DING Wei,ZHU Bin,ZHANG Yisheng,FENG Yi,MA Mingtu,LIANG Bin,ZHAO Yan,LI Yong,ZHENG Jinghua,SHI Zhusheng. A Review of Current State and Prospect of the Manufacturing and Application of Advanced Hot Stamping Automobile Steels. Acta Metall Sin, 2020, 56(4): 411-428.

Download:  HTML  PDF(2537KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Ultrahigh strength steels are highly competitive materials for vehicles to concurrently meet the increasing demand of the weight reduction and passenger safety. Hot stamping is the key forming technology to manufacture automobile components with high strength. Hot stamping steel and its manufacturing technology experienced a fast development in the past decade. This paper reviewed the state of the art of the manufacturing and applications of hot stamping steels/components in the following aspects: (1) hot stamping steels (from traditional MnB steels to recently newly developed hot stamping steels); (2) forming technologies (from traditional hot stamping process to industry 4.0 intelligent production); (3) novel hot stamping + quenching & partitioning (Q&P) process and fundamentals of deformation assisted heat treatments; (4) simulation techniques for hot stamping process (modeling of the temperature-stress field, microstructure field and simulation of the manufacturing process); (5) the assessments of in-service performance of hot stamped components. Finally, the trends of the development of hot stamping steels and related forming technologies in the future will be discussed.

Key words:  hot stamping steel      hot stamping technology      hot stamping+Q&P process      modeling      in-service performance     
Received:  11 November 2019     
ZTFLH:  TG142  
Fund: National Natural Science Foundation of China(U1564203);National Natural Science Foundation of China(51901128);National Key Research and Development Program of China(2017YFB0304401);Funds for International Cooperation and Exchange of the National Natural Science Foundation of China(51911530204);The Royal Society International Exchanges Cost Share 2018 China (No.IEC\NSFC\181414), Outstanding Academic Leaders Program of Shanghai(18XD1402200);Startup Fund for Youngman Research at SJTU

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2019.00381     OR     https://www.ams.org.cn/EN/Y2020/V56/I4/411

Commercial nameSteelmakerCSiMnPSCrTiBFeRef.
USIBOR 1500ArcelorMittal0.220.251.230.0250.0080.20.0370.004Bal.[4]
MBW 1500ThyssenKrupp0.250.41.40.0250.010.50.050.005Bal.[5]
Docol Boron02SSAB0.20~0.250.20~0.351.0~1.30.0190.010.14~0.26-0.005Bal.[6]
HPF1470POSCO0.250.31.40.020.010.250.050.0035Bal.[5]
PH1500Baosteel0.230.251.350.0150.0060.19-0.0032Bal.[7]
AC1500 HSAnsteel0.240.381.270.0140.0040.270.0420.0022Bal.[8]
Table 1  Compositions of 22MnB5 steels produced by different steel companies in the world[4,5,6,7,8]

Steel

Composition (mass fraction / %)

YS

MPa

UTS

MPa

CSiMnCrTiBNNiAlFe
27MnCrB50.250.211.240.340.0420.0020.0040.010.03Bal.10971611
28MnB50.280.401.30--0.005---Bal.11351740
34MnB50.340.401.30--0.005---Bal.12251919
37MnB40.370.310.810.190.0460.0010.0060.020.03Bal.13782040
Table 2  Compositions and mechanical properties after quenching of hot stamping steels with two strength grades of 1800 MPa and 2000 MPa[9,10]
Commercial nameSteelmakerCSiMnPSAlNbFe
Ductibor 500ArcelorMittal0.05~0.08<0.5<1.4<0.03<0.010.02~0.040.03~0.07Bal.
MBW 500ThyssenKrupp<0.10<0.35<1.0<0.03<0.025>0.015<0.1Bal.
PHS-Ultraform 490Voestalpine<0.11<0.5<1.4<0.03<0.025<0.015<0.1Bal.
Table 3  Grades and compositions of low strength high ductility and toughness steels with strength of 500 MPa[9]
Fig.1  Schematics of hot stamping, quenching and partitioning (HS-Q&P) process and microstructural evolution (Ac3—temperature of all ferrite transform into austenite, Ms—onset of temperature of martensitic transformation, γ—austenite, α'—martensite, αs'—second martensite, f—volume fraction of each phase, C—carbon content of each phase)Color online
Fig.2  Schematics of deformation induced ferrite transformation-Q&P (DIFT-Q&P) process and microstructural evolution (Ae3—equilibrium critical temperature of full austenitization,αD—deformation-induced martensite, ΔT—the difference of temperature of all ferrite transform into austenite and paraequilibrium temperature)Color online
[1] http://www.caam.org.cn/chn/4/cate_39/con_5225478.html
[2] Li J. Lightweight of Passenger Car and Niobium-Microalloying Steel [M]. Beijing: Beijing Institute of Technology Press, 2015: 258
[2] 李 军. 乘用车轻量化及微合金化钢板的应用 [M]. 北京: 北京理工大学出版社, 2015: 258
[3] Galindo-Nava E I, Rainforth W M, Rivera-Díaz-del-Castillo P E J. Predicting microstructure and strength of maraging steels: Elemental optimization [J]. Acta Mater., 2016, 117: 270
[4] Shi C, Daun K J, Wells M A. Evolution of the spectral emissivity and phase transformations of the Al-Si coating on Usibor? 1500P steel during austenitization [J]. Metall. Mater. Trans., 2016, 47B: 3301
[5] Liang J T. Strengthen-toughening mechanism and application technology of 2000 MPa grade hot stamping steel [D]. Beijing: University of Science and Technology Beijing, 2019
[5] 梁江涛. 2000 MPa级热成形钢的强韧化机制及应用技术研究 [D]. 北京: 北京科技大学, 2019
[6] Hu P, Ying L, He B. Hot Stamping Advanced Manufacturing Technology of Lightweight Car Body [M]. Singapore: Springer Singapore, 2017: 45
[7] Han X H, Zhong Y Y, Yang K, et al. Application of hot stamping process by integrating quenching & partitioning heat treatment to improve mechanical properties [J]. Procedia Eng., 2014, 81: 1737
[8] Shi X G, Dong Y, Han B, et al. Influence of parameters of hot stamping technology on properties of AC1500HS steel sheet [J]. Angang Technol., 2013, (5): 24
[8] 时晓光, 董 毅, 韩 斌等. 热成形工艺参数对AC1500HS钢板性能的影响 [J]. 鞍钢技术, 2013, (5): 24
[9] Rana R, Singh S B. Automotive Steels: Design, Metallurgy, Processing and Applications [M]. Sawston Cambridge: Woodhead Publishing, 2017: 387
[10] Karbasian H, Tekkaya A E. A review on hot stamping [J]. J. Mater. Process. Technol., 2010, 210: 2103
[11] Linke B M, Gerber T, Hatscher A, et al. Impact of Si on microstructure and mechanical properties of 22MnB5 hot stamping steel treated by quenching & partitioning (Q&P) [J]. Metall. Mater. Trans., 2018, 49A: 54
[12] Bansal G K, Rajinikanth V, Ghosh C, et al. Microstructure-property correlation in low-Si steel processed through quenching and nonisothermal partitioning [J]. Metall. Mater. Trans., 2018, 49A: 3501
[13] Suzuki T, Ono Y, Miyamoto G, et al. Effects of Si and Cr on bainite microstructure of medium carbon steels [J]. ISIJ Int., 2010, 50: 1476
[14] Li X T. Study on cracks propagation mechanism and control technology of Zn-coated press hardened steel [D]. Beijing: Central Iron & Steel Research Institute, 2018
[14] 李学涛. 镀锌热冲压钢成形过程中裂纹扩展机理及控制工艺研究 [D]. 北京: 钢铁研究总院, 2018
[15] Speer J, Matlock D K, De Cooman B C, et al. Carbon partitioning into austenite after martensite transformation [J]. Acta Mater., 2003, 51: 2611
[16] Liu H P, Lu X W, Jin X J, et al. Enhanced mechanical properties of a hot stamped advanced high-strength steel treated by quenching and partitioning process [J]. Scr. Mater., 2011, 64: 749
[17] Seo E J, Cho L, Cooman B C D. Application of quenching and partitioning (Q&P) processing to press hardening steel [J]. Metall. Mater. Trans., 2014, 45A: 4022
[18] Ariza E A, Poplawsky J, Guo W, et al. Evaluation of carbon partitioning in new generation of quench and partitioning (Q&P) steels [J]. Metall. Mater. Trans., 2018, 49A: 4809
[19] Technology and product development of high performance cold rolled automobile steel [EB/OL]. World Metals, (2019-06-15). http://www.sohu.com/a/320778124_313737
[19] (高性能冷轧汽车用钢工艺与产品研发 [EB/OL]. 世界金属导报, (2019-06-15). http://www.sohu.com/a/320778124_313737)
[20] Liu A M, Feng Y, Zhao Y, et al. Effect of niobium and vanadium micro-aalloying on microstructure and property of 22MnB5 hot press forming steel [J]. Mech. Eng. Mater., 2019, 43(5): 34
[20] 刘安民, 冯 毅, 赵 岩等. 铌钒微合金化对22MnB5热成形钢显微组织与性能的影响 [J]. 机械工程材料, 2019, 43(5): 34
[21] Hidalgo J, Santofimia M J. Effect of prior austenite grain size refinement by thermal cycling on the microstructural features of as-quenched lath martensite [J]. Metall. Mater. Trans., 2016, 47A: 5288
[22] Chen Y S, Haley D, Gerstl S S A, et al. Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel [J]. Science, 2017, 355: 1196
[23] Takahashi J, Kawakami K, Kobayashi Y. Origin of hydrogen trapping site in vanadium carbide precipitation strengthening steel [J]. Acta Mater., 2018, 153: 193
[24] Wang L, Zhu B, Wang Q, et al. Modeling of hot stamping process procedure based on finite state machine (FSM) [J]. Int. J. Adv. Manuf. Technol., 2017, 89: 857
[25] Zhang Y S, Wang Z J, Wang L. Progress in hot stamping process and equipment for high strength steel sheet [J]. J. Plast. Eng., 2018, 25(5): 11
[25] 张宜生, 王子健, 王 梁. 高强钢热冲压成形工艺及装备进展 [J]. 塑性工程学报, 2018, 25(5): 11
[26] Wang L, Zhu B, Zhang Y S, et al. A smart process control strategy for press hardening production [A]. 6th International Conference on Hot Sheet Metal Forming of High Performance Steel [C]. Atlanta, GA: Lule? University of Technology, 2017: 515
[27] Wang L, Zhu B, Zhang Y S. Production control and optimization of hot stamping line [A]. 5th International Conference on Hot Sheet Metal Forming of High-Performance Steel [C]. Toronto, Canada: Lule? University of Technology, 2015: 189
[28] Wang L, Zhu B, Zhang Y S. A runtime intelligent iterative manufacturing system (RIIMS) for hot stamping [A]. Advanced High Strength Steel and Press Hardening: Proceedings of the 2nd International Conference (ICHSU2015 [C]. Xi'an: World Scientific, 2016: 647
[29] Mori K, Maki S, Tanaka Y. Warm and hot stamping of ultra tensile strength steel sheets using resistance heating [J]. CIRP Ann.-Manuf. Technol., 2009, 54(1): 209
[30] Mori K, Bariani P F, Behrens B A, et al. Hot stamping of ultra-high strength steel parts [J]. CIRP Ann., 2017, 66: 755
[31] Merklein M, Wieland M, Lechner M, et al. Hot stamping of boron steel sheets with tailored properties: A review [J]. J. Mater. Process. Technol., 2016, 228: 11
[32] George R, Bardelcik A, Worswick M. Hot forming of boron steels using heated and cooled tooling for tailored properties [J]. J. Mater. Process. Technol., 2012, 212: 2386
[33] Karbasian H, Tekkaya A E. A review on hot stamping [J]. J. Mater. Process. Technol., 2010, 210: 2103
[34] Liu H P, Jin X J, Dong H, et al. Martensitic microstructural transformations from the hot stamping, quenching and partitioning process [J]. Mater. Charact., 2011, 62: 223
[35] Liu H P. Study on high strength and elongtaion steels treated by hot deformation & QP process [D]. Shanghai: Shanghai Jiaotong University, 2011
[35] 刘和平. 高强塑积热变形淬火碳分配钢的研究 [D]. 上海: 上海交通大学, 2011
[36] Porter D A, Easterling K E, Sherif M. Phase Transformations in Metals and Alloys [M]. Revised reprint, Boca Raton: CRC Press, 2009: 99
[37] Liu H P, Sun H E, Liu B, et al. An ultrahigh strength steel with ultrafine-grained microstructure produced through intercritical deformation and partitioning process [J]. Mater. Des., 2015, 83: 760
[38] Chen H C, Era H, Shimizu M. Effect of phosphorus on the formation of retained austenite and mechanical properties in Si-containing low-carbon steel sheet [J]. Metall. Trans., 1989, 20A: 437
[39] Matsumura Y, Yada H. Evolution of ultrafine-grained ferrite in hot successive deformation [J]. Trans. Iron Steel Inst. Jpn., 1987, 27: 492
[40] Hodgson P D, Hickson M R, Gibbs R K. Ultrafine ferrite in low carbon steel [J]. Scr. Mater., 1999, 40: 1179
[41] Wong Y Q. Physical metallurgy for ultra-fine grain steels [A]. Proceedings on HIPERS-21 [C]. Posco, Korea, 2000: 9
[42] Dong H, Sun X J. Deformation induced ferrite transformation in low carbon steels [J]. Curr. Opin. Solid State Mater. Sci., 2005, 9: 269
[43] Sun X J, Dong H, Liu Q Y, et al. Dynamically transformed ferrite fraction inferred from dilatometry measurements after deformation [J]. Mater. Sci. Eng., 2008, A487: 93
[44] Hong S C, Lee K S. Influence of deformation induced ferrite transformation on grain refinement of dual phase steel [J]. Mater. Sci. Eng., 2002, A323: 148
[45] Enomoto M, Aaronson H I. Nucleation kinetics of proeutectoid ferrite at austenite grain boundaries in Fe-C-X alloys [J]. Metall. Trans., 1986, 17A: 1385
[46] Ying C, Li G Z, Wang C Y, et al. Effect of quenching and partitioning with hot stamping on martensite transformation and mechanical properties of AHSS [J]. J. Mater. Eng. Perform., 2015, 24: 3194
[47] Ariza E, Nishikawa A S, Goldenstein H, et al. Characterization and methodology for calculating the mechanical properties of a TRIP-steel submitted to hot stamping and quenching and partitioning (Q&P) [J]. Mater. Sci. Eng., 2016, A671: 54
[48] Ariza E A, Masoumi M, Tschiptschin A P. Improvement of tensile mechanical properties in a TRIP-assisted steel by controlling of crystallographic orientation via HSQ&P processes [J]. Mater. Sci. Eng., 2018, A713: 223
[49] Ariza E A, Poplawsky J, Guo W, et al. Hot straining and quenching and partitioning of a TRIP-assisted steel: Microstructural characterization and mechanical properties [J]. Mater. Sci. Forum., 2018, 941: 704
[50] Khedr M, Li W, Zhu X, et al. Improving hydrogen embrittlement resistance of Hadfield steel by thermo-mechanical flash-treatment [J]. Mater. Sci. Eng., 2018, A712: 133
[51] Zhu B, Zhu J, Wang Y N, et al. Combined hot stamping and Q&P processing with a hot air partitioning device [J]. J. Mater. Process. Technol., 2018, 262: 392
[52] Han X H, Cui Z S, Xin P S, et al. A U-shape tool design for one-step Q&P hot stamping process [P]. Chin Pat, ZL 201310335789.1, 2015
[53] Han X H, Zhong Y Y, Tan S L, et al. Microstructure and performance evaluations on Q&P hot stamping parts of several UHSS sheet metals [J]. Sci. China Technol. Sci., 2017, 60: 1692
[54] Zhang F B, Song H W, Cheng M, et al. Microstructure development and mechanical properties of a hot stamped low-carbon advanced high strength steel treated by a novel dynamic carbon partitioning process [J]. Adv. Mater. Res., 2015, 1063: 42
[55] Hochholdinger B, Grass H, Lipp A, et al. Modeling and determination of flow curves for the simulation of hot forming [A]. Conference on the International Deep Drawing Research Group [C]. Berndyr: International Deep Drawing Research Group, 2009: 659
[56] Li F F, Fu M W, Lin J P, et al. Experimental and theoretical study on the hot forming limit of 22MnB5 steel [J]. Int. J. Adv. Manuf. Technol., 2014, 71: 297
[57] Hu P, Liu W Q, Ying L, et al. A thermal forming limit prediction method considering material damage for 22MnB5 sheet [J]. Int. J. Adv. Manuf. Technol., 2017, 92: 627
[58] Li N, Lin J, Balint D S, et al. Modelling of austenite formation during heating in boron steel hot stamping processes [J]. J. Mater. Process. Technol., 2016, 237: 394
[59] Li N, Lin J G, Dean T A, et al. Materials modelling for selective heating and press hardening of boron steel panels with graded microstructures [J]. Procedia Eng., 2014, 81: 1675
[60] Li N, Sun C Y, Guo N, et al. Damage investigation of boron steel at hot stamping conditions [J]. Procedia Eng., 2014, 81: 1744
[61] Lin J, Mohamed M, Balint D, et al. The development of continuum damage mechanics-based theories for predicting forming limit diagrams for hot stamping applications [J]. Int. J. Damage Mech., 2014, 23: 684
[62] Geiger M, Merklein M, Hoff C. Basic investigations on the hot stamping steel 22MnB5 [J]. Adv. Mater. Res., 2005, 6-8: 795
[63] Zhao K M, Wang B, Chang Y, et al. Comparison of the methods for calculating the interfacial heat transfer coefficient in hot stamping [J]. Appl. Therm. Eng., 2015, 79: 17
[64] Li Y F, Li S H, He J, et al. Identification methods on blank-die interfacial heat transfer coefficient in press hardening [J]. Appl. Therm. Eng., 2019, 152: 865
[65] Han X H, Hao X, Yang K, et al. Theoretical and experimental study of the rule for heat transfer coefficient in hot stamping of high strength steels [J]. AIP Conf. Proc., 2013, 1567: 958
[66] Kirkaldy J S, Venugopalan D. Prediction of microstructure and hardenability in low alloy steels [A]. Proceedings of the International Conference on Phase Transformations in Ferrous Alloys [C]. Warrendale, PA: Metallurgical Soc of AIME, 1984: 125
[67] Li M V, Niebuhr D V, Meekisho L L, et al. A computational model for the prediction of steel hardenability [J]. Metall. Mater. Trans., 1998, 29B: 661
[68] ?kerstr?m P, Oldenburg M. Austenite decomposition during press hardening of a boron steel—Computer simulation and test [J]. J. Mater. Process. Technol., 2006, 174: 399
[69] Koistinen D P, Marburger R E. A general equation prescribing the extent of the austenite-martensite transformation in pure iron-carbon alloys and plain carbon steels [J]. Acta Metall., 1959, 7: 59
[70] Lee S J, Lee Y K. Erratum to "Finite element simulation of quench distortion in a low alloy steel incorporating transformation kinetics" [Acta Mater 2008;56: 1482-90] [J]. Acta Mater., 2009, 57: 2605
[71] Zhu L J, Gu Z W, Xu H, et al. Modeling of microstructure evolution in 22MnB5 steel during hot stamping [J]. J. Iron Steel Res. Int., 2014, 21: 197
[72] Wang Z J, Wang K, Liu Y, et al. Multi-scale simulation for hot stamping quenching & partitioning process of high-strength steel [J]. J. Mater. Process. Technol., 2019, 269: 150
[73] Han X H, Wang C L, Ding Y N, et al. Properties prediction modelling for hot stamping products and its validation in a U-cap part [J]. J. Phys. Conf. Ser., 2018, 1063: 012036
[74] Malik A, Amberg G, Borgenstam A, et al. Effect of external loading on the martensitic transformation—A phase field study [J]. Acta Mater., 2013, 61: 7868
[75] Yang H, Wu C, Li H W, et al. Review on cellular automata simulations of microstructure evolution during metal forming process: Grain coarsening, recrystallization and phase transformation [J]. Sci. China Technol. Sci., 2011, 54: 2107
[76] Tan W D, Bailey N S, Shin Y C. A novel integrated model combining cellular automata and phase field methods for microstructure evolution during solidification of multi-component and multi-phase alloys [J]. Comput. Mater. Sci., 2011, 50: 2573
[77] Zheng C W, Xiao N M, Li D Z, et al. Mesoscopic modeling of austenite static recrystallization in a low carbon steel using a coupled simulation method [J]. Comput. Mater. Sci., 2009, 45: 568
[78] Hutchinson B, Bate P, Lindell D, et al. Plastic yielding in lath martensites—An alternative viewpoint [J]. Acta Mater., 2018, 152: 239
[79] Sun M X, Zhang W N, Liu Z Y, et al. Effect of cooling mode on microstructure and mechanical properties in an extremely low carbon Cu bearing steel [J]. Mater. Charact., 2016, 120: 38
[80] Naderi M, Uthaisangsuk V, Prahl U, et al. A numerical and experimental investigation into hot stamping of boron alloyed heat treated steels [J]. Steel Res., 2008, 79: 77
[81] Tang B T, Wang Q L, Wei Z H, et al. FE simulation models for hot stamping an automobile component with tailor-welded high-strength steels [J]. J. Mater. Eng. Perform., 2016, 25: 1709
[82] Liu B G, Li W, Lu X W, et al. The effect of retained austenite stability on impact-abrasion wear resistance in carbide-free bainitic steels [J]. Wear, 2019, 428-429: 127
[83] Morales-Palma D, Vallellano C, García-Lomas F J. Assessment of the effect of the through-thickness strain/stress gradient on the formability of stretch-bend metal sheets [J]. Mater. Des., 2013, 50: 798
[84] Akeret R. Failure mechanisms in the bending of aluminum sheets and limits of bendability [J]. Aluminium, 1978, 54: 117
[85] Kaupper M, Merklein M. Bendability of advanced high strength steels—A new evaluation procedure [J]. CIRP Ann., 2013, 62: 247
[86] Kaijalainen A J, Suikkanen P, Karjalainen L P, et al. Effect of austenite pancaking on the microstructure, texture, and bendability of an ultrahigh-strength strip steel [J]. Metall. Mater. Trans., 2014, 45A: 1273
[87] Yamazaki K O M, Yasuda H. Recent advances in ultrahigh-strength sheet steels for automotive structural use [J]. Nippon Steel Tech. Rep., 1995, 64: 37
[88] Larour P, Hackl B, Leomann F. Sensitivity analysis on the calculated bending angle in the instrumented bending test [J]. Proc. Int. Conf. IDDRG, 2013, C/52/13: 317
[89] Arola A M, Kaijalainen A, Kesti V, et al. Digital image correlation and optical strain measuring in bendability assessment of ultra-high strength structural steels [J]. Procedia Manuf., 2019, 29: 398
[90] Cheong K, Omer K, Cliff B, et al. Evaluation of the VDA 238-100 tight radius bending test using digital image correlation strain measurement [A]. 36th IDDRG Conference—Materials Modelling and Testing for Sheet Metal Forming [C]. J. Phys.Conf. Ser., 2017, 896: 012075
[91] Ma N, Shen G Z, Zhang Z H, et al. Material performance of hot-forming high strength steel and its application in vehicle body [J]. J. Mech. Eng., 2011, 47(8): 60
[91] 马 宁, 申国哲, 张宗华等. 高强度钢板热冲压材料性能研究及在车身设计中的应用 [J]. 机械工程学报, 2011, 47(8): 60
[92] Yang J K, Xu W, Wan X M. Development and validation of a head-neck finite element model for the study of neck dynamic responses in car impacts [J]. J. Hunan Univ. (Nat. Sci.), 2005, 32(2): 6
[92] 杨济匡, 许 伟, 万鑫铭. 研究汽车碰撞中头颈部动态响应的有限元模型的建立和验证 [J]. 湖南大学学报(自然科学版), 2005, 32(2): 6
[93] Wan X M, Yue Z Y, Yang J K. Simulation study of the Hybrid Ⅲ 50th head-neck response under low severity rear impact [J]. Automobile Technol., 2006, (Suppl.1): 60
[93] 万鑫铭, 乐中耀, 杨济匡. Hybrid Ⅲ 50th颈部模型低速后碰撞响应的仿真分析 [J]. 汽车技术, 2006, (增刊1): 60
[94] Smerd R, Winkler S, Salisbury C, et al. High strain rate tensile testing of automotive aluminum alloy sheet [J]. Int. J. Impact Eng., 2005, 32: 541
[95] Cho L, Sulistiyo D H, Seo E J, et al. Hydrogen absorption and embrittlement of ultra-high strength aluminized press hardening steel [J]. Mater. Sci. Eng., 2018, A734: 416
[96] Takagi S, Toji Y, Yoshino M, et al. Hydrogen embrittlement resistance evaluation of ultra high strength steel sheets for automobiles [J]. ISIJ Int., 2012, 52: 316
[97] Toji Y, Takagi S, Yoshino M, et al. Evaluation of hydrogen embrittlement for high strength steel sheets [J]. Mater. Sci. Forum, 2010, 638-642: 3537
[98] Akiyama E, Wang M Q, Li S J, et al. Studies of evaluation of hydrogen embrittlement property of high-strength steels with consideration of the effect of atmospheric corrosion [J]. Metall. Mater. Trans., 2013, 44A: 1290
[99] Chin K G, Kang C Y, Sang Y S, et al. Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels [J]. Mater. Sci. Eng., 2011, A528: 2922
[100] Zhang Y J, Zhou C, Hui W J, et al. Hydrogen induced delayed fracture behavior of a low-carbon Mn-B type ultra-high strength steel sheet [J]. Trans. Mater. Heat Treat., 2013, 34(10): 96
[100] 张永健, 周 超, 惠卫军等. 一种低碳Mn-B系超高强度钢板的氢致延迟断裂行为 [J]. 材料热处理学报, 2013, 34(10): 96
[101] Toribio J, Ayaso F J. Optimization of round-notched specimen for hydrogen embrittlement testing of materials [J]. J. Mater. Sci., 2004, 39: 4675
[102] Yamasaki S, Takahashi T. Evaluation method of delayed fracture property of high strength steels [J]. Tetsu Hagané, 1997, 83: 454
[102] 山崎 真吾, 高橋 稔彦. 高強度鋼の耐遅れ破壊特性の定量的評価方法 [J]. 鉄と鋼, 1997, 83: 454
[103] Development progress of green and low cost automobile board in WISCO [EB/OL]. (2017-07-24). https://www.sohu.com/a/159496432_378896
[104] https://www.xianjichina.com/news/details_86038
[105] Lu Q. New high performance hot forming steel for automobile [A]. The 13th Automobile Lightweight Congress and Exhibition Automobile Lightweight Congress [C]. 2019
[105] 卢 琦. 新型高性能汽车用热成形钢 [A]. (第十三届)汽车轻量化大会暨展览汽车轻量化大会 [C]. 2019
[106] http://www.magang.org.cn/D3/Xwzx/Jtzx/380517/Index
[1] CHEN Huabin, CHEN Shanben. Key Information Perception and Control Strategy of Intellignet Welding Under Complex Scene[J]. 金属学报, 2022, 58(4): 541-550.
[2] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[3] YANG Yong, HE Quanfeng. Lattice Distortion in High-Entropy Alloys[J]. 金属学报, 2021, 57(4): 385-392.
[4] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[5] YI Hongliang,CHANG Zhiyuan,CAI Helong,DU Pengju,YANG Dapeng. Strength, Ductility and Fracture Strain ofPress-Hardening Steels[J]. 金属学报, 2020, 56(4): 429-443.
[6] Houfa SHEN, Kangxin CHEN, Baicheng LIU. Numerical Simulation of Macrosegregation inSteel Ingot Casting[J]. 金属学报, 2018, 54(2): 151-160.
[7] Rui CHEN, Qingyan XU, Huiting GUO, Zhiyuan XIA, Qinfang WU, Baicheng LIU. Modeling of Strain Hardening Behavior and Mechanical Properties of Al-7Si-Mg Cast Aluminum AlloysDuring Tensile Process[J]. 金属学报, 2017, 53(9): 1110-1124.
[8] Xunhua YUAN, Qifu ZHANG. Microstructure Evolution of Hot-Dip Al-10%Si Coating During the Austenitization of 22MnB5 Hot Stamping Steel[J]. 金属学报, 2017, 53(11): 1495-1503.
[9] Mingfang ZHU, Qianyu TANG, Qingyu ZHANG, Shiyan PAN, Dongke SUN. CELLULAR AUTOMATON MODELING OF MICRO-STRUCTURE EVOLUTION DURING ALLOY SOLIDIFICATION[J]. 金属学报, 2016, 52(10): 1297-1310.
[10] Lei ZHAO,Hongxiang JIANG,Tauseef AHMAD,Jiuzhou ZHAO. STUDY OF SOLIDIFICATION FOR GAS-ATOMIZED DROPLET OF Cu-Co-Fe ALLOY[J]. 金属学报, 2015, 51(7): 883-888.
[11] ZHANG Lei, ZHAO Honglei, ZHU Mingfang. SIMULATION OF SOLIDIFICATION MICROSTRUC-TURE OF SPHEROIDAL GRAPHITE CAST IRON USING A CELLULAR AUTOMATON METHOD[J]. 金属学报, 2015, 51(2): 148-158.
[12] YANG Qianqian, LIU Yuan, LI Yanxiang. MODELING AND SIMULATION OF STRUCTURAL FORMATION OF POROUS ALUMINUM IN GASAR SOLIDIFICATION[J]. 金属学报, 2014, 50(11): 1403-1412.
[13] LI Zhengyang, ZHU Mingfang, DAI Ting. MODELING OF MICROPOROSITY FORMATION IN AN Al-7%Si ALLOY[J]. 金属学报, 2013, 49(9): 1032-1040.
[14] CAO Lingyong, GUO Mingxing, CUI Hua, CAI Yuanhua,ZHANG Qiaoxia,HU Xiaoqian,ZHANG Jishan. STUDY ON THE KINETICS OF PHASE TRANSFORMATION β→α IN THE HOMOGENEOUS HEAT TREATMENT OF Al-Mg-Si SERIES ALLOYS[J]. 金属学报, 2013, 29(4): 428-434.
[15] CHENG Junye, ZHAO Aimin, CHEN Yinli, DONG Rui, HUANG Yao. EBSD STUDIES OF 30MnB5 HOT STAMPING STEEL TEMPERED AT DIFFERENT TEMPERATURE[J]. 金属学报, 2013, 49(2): 137-145.
No Suggested Reading articles found!