Abstract The effect of heating temperature and holding time on the phase transformation from (Fe, Mn)Al6 to α-Al12(Fe, Mn)3Si in AA3104 aluminum alloy during homogenization was studied by BSE and EDS in SEM. The 3D morphology of the eutectic phases heated at 600 ℃ for different holding times was reconstructed by a novel serial sectioning method. Evolution of the microstructure could be revealed in 3D for the first time. Al spots were observed within the α-Al12(Fe, Mn)3Si phase and counted during different transformation stages. Large number of Al spots disappeared by diffusing into the neighboring matrix after extended heating times, while the volume of the α phase was also decreased at the same time. The microstructure of the α phase after transformation was analyzed, showing ‘duplex interfaces’created by partly transformed particles. The dense holes within α phase particles are believed to promote particle break up during hot rolling of the omogenized material.
|
|
Received: 07 November 2011
|
|
|
| Fund: Supported by Fundamental Research Funds for the Central Universities No.CDJRC10130008) |
| [1] Engler O, Kong X W, Yang P. Scr Mater, 1997; 37: 1665[2] Humphreys F J. Acta Metall, 1977; 25: 1323[3] Vatne H E, Engler O, Nes E. Mater Sci Technol, 1997; 13: 3[4] Yang P, Engler O. Acta Metall Sin, 1998; 34: 785(杨平, Engler O. 金属学报, 1998; 34: 785)[5] Alexander D T L, Greer A L. Philos Mag, 2004; 84: 3051[6] Hamerton R, Cama H, Meredith M W. Mater Sci Forum, 000; 331–337: 143[7] Alexander D T L, Greer A L. Mater Sci Technol, 2005; 1: 955[8] Gandhi C. Master Dissertation, Vancouver: The University f British Columbia, 1999[9] Li Y J, Arnberg L. Mater Sci Eng, 2003; A347: 130[10] Moulin N, Parra–Denis E, Jeulin D, Ducottet C, Bigot A, Boller E, Maire E, Barat C, Kl¨ocker H. Adv Eng Mater, 2010; 12: 20[11] Skjerpe P. Metall Mater Trans, 1987; 18A: 189[12] Li Y J, Johansen A, Benum S, Simensen C J, Dons A L, Hakonsen A, Arnberg L. Aluminium, 2004; 80: 578[13] Sun D L, Kang S B, Koo H S. Mater Chem Phys, 2000; 63: 37[14] Alexander D T L, Greer A L. Acta Mater, 2002; 50: 2571[15] Alexander D T L, Greer A L. Philos Mag, 2004; 84: 3071[16] Fiala J C. J Microsc, 2005; 218: 52[17] Li Y J, Arnberg L. Acta Mater, 2003; 51: 3415[18] Sun D L, Kang S B, Koo H S. Chinese J Nonferr Met, 1999; 9: 556(孙东立, 姜石峰, 高兴锡. 中国有色金属学报, 1999; 9: 556)[19] Dehmas M, Weisbecker P, Geandier G, Archambault P, Aeby–Gautier E. J Alloys Compd, 2005; 400: 116[20] Li Y J, Arnberg L. Acta Mater, 2004; 52: 2945 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|