| PREDICTION OF GRAIN GROWTH IN HYBRID WELDING HAZ OF TCS STAINLESS STEEL |
| ZHANG Zhuanzhuan, WU Chuansong, Gao Jinqiang |
| Key Lab for Liquid–Solid Structure Evolution and Materials Processing (Ministry of Education), Shandong University, Jinan 250061 |
|
Cite this article:
ZHANG Zhuanzhuan WU Chuansong Gao Jinqiang. PREDICTION OF GRAIN GROWTH IN HYBRID WELDING HAZ OF TCS STAINLESS STEEL. Acta Metall Sin, 2012, 48(2): 199-204.
|
|
|
Abstract According to the formula of grain growth under isothermal condition, the kinetics equation of ferritic grain growth in heat affected zone (HAZ) was obtained, which was combined with the calculated thermal cycles to predict the grain growth in HAZ of TCS stainless steel under the new–type welding procedure–hybrid welding. The grain sizes in HAZ of TCS stainless steel have been calculated for three welding conditions. Simulation results are validated by the average grain sizes measured on the metallographic images of the welding joint of TCS stainless steel. Preliminary discussion has been made on correlation of the grain growth with the thermal cycles and the effect of local variation in thermal cycles on the grain growth.
|
|
Received: 15 September 2011
|
| Fund: Supported by National Natural Science Foundation of China (No.51074098) |
| [1] Du B, Sun J T, Xu Y J, Mao H, Jia Y L, Wang L X, Wang Z B, Zhang X B, Yu W, Liu Z C,Chen Z Y, Zhang Z C. Weld Join, 2009; (1): 1(杜兵, 孙静涛, 徐玉军, 毛 辉, 贾玉力, 王立新, 王志斌, 张心保, 于 维, 刘志臣, 陈增有, 张志昌. 焊接, 2009; (1): 1)[2] Li J L, Li J Q, Wu Y L, Huo L X, Zhang Y F. Weld Join, 2007; (7): 17(李加良, 李践桥, 武永亮, 霍立兴, 张玉风. 焊接, 2007; (7): 17)[3] Dilthey U. Proc 8th Int Symposium on Innovations in Welding and Joining for a New Era in Manufacturing, Kyoto, Japan, 2008: 1[4] Defalco J. Weld J, 2007; 86: 47[5] Mo C L, Qian B N, Li D Z, Li J L. Chin J Mater Res, 2001; 15: 343(莫春立, 钱百年, 李殿中, 李晶丽. 材料研究学报, 2001; 15: 343)[6] Mo C L, Li D Z, Qian B N, Guo X M. Acta Metall Sin, 2001; 37: 307(莫春立, 李殿中, 钱百年, 国旭明. 金属学报, 2001; 37: 307)[7] Wu C S. Welding Thermal Processes and Weld Pool Behaviors. New York: CRC Press, 2011; 47[8] Cho J H, Na S J. J Phys, 2006; 39D: 5372[9] Kaplan A. J Phys, 1994; 27D: 1805[10] Xu G X, Wu C S, Qin G L, Wang X Y, Lin S Y. Acta Metall Sin, 2008; 44: 641(胥国祥, 武传松, 秦国梁, 王旭友, 林尚扬. 金属学报, 2008; 44: 641)[11] Xu G X, Wu C S, Qin G L, Wang X Y, Lin S Y. Acta Metall Sin, 2009; 45: 107(胥国祥, 武传松, 秦国梁, 王旭友, 林尚扬. 金属学报, 2009; 45: 107)[12] Zhang Z Z, Xu G X, Wu C S. Acta Metall Sin, 2011; 47: 1450(张转转, 胥国祥, 武传松. 金属学报, 2011; 47: 1450)[13] Wang L X, Song C J. Iron Steel, 2008; 43: 71(王立新, 宋长江. 钢铁, 2008; 43: 71) |