Please wait a minute...
Acta Metall Sin  2012, Vol. 48 Issue (2): 205-210    DOI: 10.3724/SP.J.1037.2011.00577
论文 Current Issue | Archive | Adv Search |
EXPERIMENTAL RESEARCH ON LASER SHOCK WAVE LOADING MECHANISM OF 2024 ALUMINUM ALLOY SHEET
FENG Aixin 1,2, NIE Guifeng 1, XUE Wei 2, CAO Yupeng 1,3, XU Xiaoxiang 1, LI Bin 1, SHI Fen 1
1. School of Mechanical Engineering, Jiangsu University, Zhenjiang 212013
2. School of Mechanical Engineering, Wenzhou University, Wenzhou 325035
3. School of Mechanical Engineering, Nantong University, Nantong 226019
Cite this article: 

FENG Aixin NIE Guifeng XUE Wei CAO Yupeng XU Xiaoxiang LI Bin SHI Fen . EXPERIMENTAL RESEARCH ON LASER SHOCK WAVE LOADING MECHANISM OF 2024 ALUMINUM ALLOY SHEET. Acta Metall Sin, 2012, 48(2): 205-210.

Download:  PDF(706KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  2024 aluminum alloy sheets with three different thicknesses were shocked by means of a single laser shock processing. Static and dynamic strain signals from the strain gauges on the back of the target were measured by STSS–1 stress test module. Residual stresses of target surfaces were measured by XRD. The loading model by the laser shock waves in 2024 aluminium alloy sheets was established, the stress wave propagations and stress wave structures inside the targets were described, and the reasons of generating residual tensile stress in the impact areas were explained. The results indicate that laser shock waves reflected and transmitted have different properties and intensities at the different places of target surfaces. When the laser power density is far beyond the best power density range of 2024 aluminum alloy and the target material is thin enough, the tensile residual stresses are generated.
Key words:  laser shock wave      stress wave      dynamic strain      2024 aluminum alloy     
Received:  15 September 2011     
ZTFLH: 

TN249

 
Fund: 

Supported by National Science Foundation of China (No.51175237), China Postdoctoral ScienceFoundation (No.20100481096), Postdoctoral Science Foundation of Jiangsu Province (No.1002029C) and Senior Start Funds of Jiangsu University (No.09JDG090)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2011.00577     OR     https://www.ams.org.cn/EN/Y2012/V48/I2/205

[1] Zhang Y K, Hu C L, Cai L, Yang J C, Zhang X R. Appl Phys, 2001; 72A: 113

[2] Zhang Y K, Lu J Z, Ren X D, Yao H B, Yao H X. Mater Des, 2009; 30: 1697

[3] Zhang Y K, You J, Lu J Z, Cui C Y, Jiang Y F, Ren X D. Surf Coat Technol, 2010; 204: 3947

[4] Lu J Z, Luo K Y, Feng A X, Zhong J W, Sun G F, Zhang L, Qian Xi M. Chin J Lasers, 2010; 37: 2664

(鲁金忠, 罗开玉, 冯爱新, 钟俊伟, 孙桂芳, 张 磊, 钱晓明. 中国激光, 2010; 37: 2664)

[5] Yang X, Zou H C, Dai S J. Appl Laser, 1998; 18(4): 179

(杨 晓, 邹鸿承, 戴蜀娟. 应用激光, 1998; 18(4): 179)

[6] Huang S, Zhou J Z, Jiang S Q, Zhu Y B, Hu L L. Chin J Lasers, 2010; 37: 256

(黄舒, 周建忠, 蒋素琴, 朱银波, 胡玲玲. 中国激光, 2010; 37: 256)

[7] Gu Y Y, Zhang L F, Lu J Z, Zhang Y K. Chin J Lasers, 2009; 36: 3318

(顾永玉, 张凌峰, 鲁金忠, 张永康. 中国激光, 2009; 36: 3318)

[8] Montross C S, Ye L. Int Fatigue, 2002; 24: 1021

[9] Li Z Y, Zhu W H, Cheng J Y, Guo D H, Wu H X. Chin J Lasers, 1997; 24: 259.

(李志勇, 朱文辉, 程经毅, 郭大浩, 吴鸿兴. 中国激光, 1997; 24: 259)

[10] Liu L, Wang S B, Wu H X, Guo D H, Liao P Y. Laser Technol, 2007; 31: 134

(刘丽, 王声波, 吴鸿兴, 郭大浩, 廖培育. 激光技术, 2007; 31: 134)

[11] Tang T M, Zhang Y K. Nantong Inst Technol, 1999; 15(1): 26

(唐通鸣, 张永康. 南通工学院学报, 1999; 15(1): 26)

[12] Yu S S, Xiao H B, Wang F, Yuan B, Zhang Y K. Chin J Lasers, 2010; 37: 1386

(于水生, 姚红兵, 王飞, 袁 蓓, 张永康. 中国激光, 2010; 37: 1386)

[13] Liao P Y, Wang S B, Sheng J J, Liu L, Xia X P. Appl Laser, 2007; 27(2): 110

(廖培育, 王声波, 盛晶晶, 刘 丽, 夏小平. 应用激光, 2007; 27(2): 110)

[14] Tang Y X, Zhang Y K, Zhang H, Yu C Y. Trans Met Heat Treat, 1997; 18(4): 22

(唐亚新, 张永康, 张宏, 余承业. 金属热处理学报, 1997; 18(4): 22)

[15] Zhang L F, Zhang Y K, Ren X D, Feng A X. Trans Chin Soc Agric Machine, 2007; 38(1): 127

(张凌峰, 张永康, 任旭东, 冯爱新. 农业机械学报, 2007; 38(1): 127)

[16] Zhang Y K, Chen J F, Xu R J. Chin J Lasers, 2008; 35: 1067

(张永康, 陈菊芳, 许仁军. 中国激光, 2008; 35: 1067)

[17] Liu H W. Mechanics of Materials. Beijing: Higher Education Press, 2004: 216

(刘鸿文. 材料力学. 北京: 高等教育出版社, 2004: 216)

[18] Luo X M, Ma H, Zhang J W, Zhang Y K. Mater Rev, 2010; 24(3): 11

(罗新民, 马 辉, 张静文, 张永康. 材料导报, 2010; 24(3): 11)

[19] Yang X M. Numerical Simulation for Explosion and Phenomena. Hefei: University of Science and Technology of China Press, 2010: 31

(杨秀敏. 爆炸冲击现象数值模拟. 合肥: 中国科学技术大学出版社, 2010: 31)

[20] Hu Y X. PhD Thesis, Shanghai Jiao Tong University, 2008

(胡永祥. 上海交通大学博士学位论文, 2008)

[21] Gu Y Y, Zhang Y K, Zhang X Q, Shi J G. Acta Phys Sin, 2006; 55: 5885

(顾永玉, 张永康, 张兴权, 史建国. 物理学报, 2006; 55: 5885)

[22] Ma X Q. Impact Dynamics. Beijing: Beijing Institue of Technology Press, 1992: 1

(马晓青. 冲击动力学. 北京:北京理工大学出版社, 1992: 1)
[1] GAO Bowen, WANG Meihan, YAN Maocheng, ZHAO Hongtao, WEI Yinghua, LEI Hao. Electrochemical Preparation and Corrosion Resistance of PEDOT Coatings on Surface of 2024 Aluminum Alloy[J]. 金属学报, 2020, 56(11): 1541-1550.
[2] Dongdong LI, Lihe QIAN, Shuai LIU, Jiangying MENG, Fucheng ZHANG. Effect of Manganese Content on Tensile Deformation Behavior of Fe-Mn-C TWIP Steels[J]. 金属学报, 2018, 54(12): 1777-1784.
[3] GUO Pengcheng, QIAN Lihe, MENG Jiangying, ZHANG Fucheng. MONOTONIC TENSION AND TENSION-COMPRES- SION CYCLIC DEFORMATION BEHAVIORS OF HIGH MANGANESE AUSTENITIC TWIP STEEL[J]. 金属学报, 2014, 50(4): 415-422.
[4] CAI Yulong, FU Shihua, WANG Yuhui, TIAN Chenggang, GAO Yue, CHENG Teng, ZHANG Qingchuan. SERRATED YIELDING OF 5456 ALUMINIUM MAGNE- SIUM ALLOY BASED ON THREE DIMENSIONAL DIGITAL IMAGE CORRELATION[J]. 金属学报, 2014, 50(12): 1491-1497.
[5] HAN Guoming, CUI Chuanyong, GU Yuefeng, HU Zhuangqi, SUN Xiaofeng. INVESTIGATION OF TEMPERATURE DEPENDENCE OF PLC EFFECT IN A NICKEL BASE SUPERALLOY[J]. 金属学报, 2013, 49(10): 1243-1247.
[6] FU Shihua CHENG Teng ZHANG Qingchuan CAO Pengtao HU Qi. STUDY ON TWO CRITICAL MECHANISMS OF PLC EFFECT OF 5456 Al–BASED ALLOY[J]. 金属学报, 2012, 48(12): 1453-1458.
[7] TIAN Chenggang CUI Chuanyong GU Yuefeng SUN Xiaofeng . EFFECT OF SOLUTION TREATMENT ON THE INVERSE DYNAMIC STRAIN AGING OF A Ni–Co BASE SUPERALLOY[J]. 金属学报, 2012, 48(10): 1223-1228.
[8] LIU Shihan CHEN Darong. MECHANICS MECHANISM OF DUPLEX STEEL CAVITATION DAMAGE[J]. 金属学报, 2009, 45(5): 519-526.
[9] JIANG Huifeng CHEN Xuedong FAN Zhichao DONG Jie JIANG Heng LU Shouxiang. EFFECT OF DYNAMIC STRAIN AGING ON FATIGUE--CREEP BEHAVIOR OF 316L AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2009, 45(3): 326-330.
[10] TAN Jun LI Cong SUN Chao YING Shihao LIAN Shanshan KAN Xiwu FENG Keqin. THERMALLY ACTIVATED DEFORMATION AND DYNAMIC STRAIN AGING OF Zr–4 ALLOY DURING STRESS RELAXATION[J]. 金属学报, 2009, 45(2): 173-177.
[11] Cong Wang. PORTEVIN-LE CHATELIER EFFECT OF LA41 MAGNESIUM ALLOYS[J]. 金属学报, 2006, 42(2): 191-194 .
[12] . The Effect of Solute Concentration by Solution Treatment on Portevin-Le Chatelier effect in Al-Cu Alloys[J]. 金属学报, 2006, 42(12): 1248-1252 .
[13] JIANG Huifeng; ZHANG Qingchuan; JIANG Zhenyu; WU Xiaoping. Experimental Investigations on the Temporal and Spatial Behaviors of the PLC Effect in Al--Cu Alloys[J]. 金属学报, 2005, 41(7): 727-732 .
[14] CHAI Huifen;RUAN Zheng;FAN Quncheng (Xi'an Jiaotong University)(Manuscript received 7 December; 1993; in revised form 10 June; 1994). SLIP BANDS OF PRESTRAINED AND CYCLED Cu AND Cu-Zn ALLOY[J]. 金属学报, 1994, 30(11): 502-506.
[15] CHEN Wenzhe;QIAN Kuangwu Fuzhou UniversityPENG Kaiping;assistant;Department of Mechanical Engineering;Fuzhou University Fuzhou 350002. EFFECT OF DYNAMIC STRAIN AGING ON LOW CYCLE FATIGUE BEHAVIOUR OF 18--8 AUSTENITIC STAINLESS STEEL[J]. 金属学报, 1993, 29(6): 43-48.
No Suggested Reading articles found!