Acta Metall Sin  2011, Vol. 47 Issue (9): 1216-1220    DOI: 10.3724/SP.J.1037.2011.00211
论文 Current Issue | Archive | Adv Search |
HIGH TEMPERATURE OXIDATION BEHAVIOURS OF THREE ZIRCONIUM ALLOYS
QIU Jun, ZHAO Wenjin Thomas Guilbert  Jean-Luc Bechade
1) Science and Technology on Reactor Fuel and Materials Laboratory, Nuclear Power Institute of China, Chengdu 610041
2) French Atomic Energy and Alternative Energies Commission, Gif-sur-Yvette cedex 91191, France
Cite this article: 

QIU Jun ZHAO Wenjin Thomas Guilbert Jean-Luc Bechade. HIGH TEMPERATURE OXIDATION BEHAVIOURS OF THREE ZIRCONIUM ALLOYS. Acta Metall Sin, 2011, 47(9): 1216-1220.

Download:  PDF(2309KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Isothermal oxidation behaviors of Zr-alloys Zr-A and Zr-B cladding tubes in flowing oxygen were measured and compared to Zr-4 cladding tube over a wide temperature range from 700 ℃ to 1200 ℃. The results show that the kinetics oxidation curves of all the alloys basically obey the parabolic rate law at the temperature range from 700 ℃ to 1200 ℃. In 700 ℃ oxidation of alloy Zr-B, a rate transition occurrs at about 1200 s. The rate transitions in 800 ℃ curves of alloys Zr-A and Zr-B occurr at about 600 s. The oxidation kinetics curves are changed for all the alloys at 1000 ℃, which is resulted from the crack in the oxide layer due to the ZrO2 phase transformation from a monoclinic structure to a tetragonal structure. At the temperature above 1100 ℃, the oxidation kinetics curves of all the alloys obey the parabolic rate law, and no kinetics changes were observed. The results also show that the alloy composition has a negligible effect on the oxidation resistance at the temperature above 1100 ℃. The parabolic rate constant Kp of the oxidation reaction was get through calculating weight gain due to oxidation.
Key words:  zirconium alloy      high-temperature oxidation      oxidation kinetics     
Received:  06 April 2011     

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2011.00211     OR     https://www.ams.org.cn/EN/Y2011/V47/I9/1216

[1] Baker L, Just L C. ANL–6548, AEC Research and Development Report, Argonne National Laboratory, 1962

[2] Pawel K E, Cathcart J V, Mckee R A. Electrochem Sci Techol, 1979; 126: 1105

[3] Leistikow S, Schanze G. Nucl Eng Des, 1987; 103: 65

[4] Nagase F. Otomo T, Uetsuka H. Nucl Sci Technol, 2003; 40: 213

[5] Sabol G P, Comstock R J, Weiner R, Larouere A P, Stanutz R N. In: Bradly E R, Sabol G P eds., Zirconium in the Nuclear Industry Tenth International Symposiu. ASTM STP 1245, Philadelphia: ASTM International, 1994: 724

[6] Etoh Y, Shimada S, Yasuda T, Ikeda T, Adamson R B, Chen J F, Ishii Y, Takai K. In: Paul D B, Davidson R R eds., Zirconium in the Nuclear Industry Nineth International Symposium, ASTM STP 1129, West Conshohocken, PA: ASTM International, 1992,: 825

[7] Choo K N, Kim Y S. J Nucl Mater, 2001; 297: 5247

[8] Kim J M, Jeong Y H. J Nucl Mater, 1999; 275: 74

[9] Billone M, Yan C, Burtseva Y, Chung H M. In: Fuketa T ed., Summary of Fuel Safety Research Meeting 2005, Tokyo: Japan Atomic Energy Agency, 2006: 168

[10] Asmolov V, Yegorova L, Lioutov K, Konoveyev A, Smirnov V, Goryachev A, Chesanov V, Prokhorov V. In: Monteleone S, Nesmith S eds., Proceeding of the 2002 Nuclear

Safety Research Conference, Washingdon D. C.: Nuclear Regulation Commission, 2003: 109

[11] Baek J H, Park K B, Jeong Y H. J Nucl Mater, 2004; 335: 443

[12] Zhao W J. Rare Met Lett, 2004; 23(5): 15

(赵文金. 稀有金属快报, 2004; 23(5): 15)

[13] Li C, Zhou B X, Zhao W J, Li P, Peng Q, Ying S H, Shen B L. J Nucl Mater, 2002; 304: 134

[14] Peng J H, Li W F, Bechade J L, Maury R. Chin J Rare Met, 2008; 32(1): 1

(彭继华, 李文芳, Bechade J L, Maury R. 稀有金属, 2008; 32(1): 1)

[15] Xue X Y, Bai X D, Tan Z Y, Zhou Q S, Liu J Z. Rare Met Mater Eng, 2004; 33(9): 902

(薛祥义, 白新德, 田振业, 周青山, 刘建章. 稀有金属材料与工程, 2004; 33(9): 902)

[16] American Society for Metals, Metals Handbook Vol.8. 8th Ed., Materials Park: ASM International, 1971: 327
[1] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[2] LIAO Jingjing, ZHANG Wei, ZHANG Junsong, WU Jun, YANG Zhongbo, PENG Qian, QIU Shaoyu. Periodic Densification-Transition Behavior of Zr-Sn-Nb-Fe-V Alloys During Uniform Corrosion in Superheated Steam[J]. 金属学报, 2023, 59(2): 289-296.
[3] CONG Hongda, WANG Jinlong, WANG Cheng, NING Shen, GAO Ruoheng, DU Yao, CHEN Minghui, ZHU Shenglong, WANG Fuhui. A New Design Inorganic Silicate Composite Coating and Its Oxidation Behavior at High Temperature in Steam Atmosphere[J]. 金属学报, 2022, 58(8): 1083-1092.
[4] YAO Meiyi,ZHANG Xingwang,HOU Keke,ZHANG Jinlong,HU Pengfei,PENG Jianchao,ZHOU Bangxin. The Initial Corrosion Behavior of Zr-0.75Sn-0.35Fe-0.15Cr Alloy in Deionized Water at 250 ℃[J]. 金属学报, 2020, 56(2): 221-230.
[5] YAO Meiyi, LIN Yuchen, HOU Keke, LIANG Xue, HU Pengfei, ZHANG Jinlong, ZHOU Bangxin. Effect of Sn on Initial Corrosion Behavior of Zirconium Alloy in 280 ℃ LiOH Aqueous Solution[J]. 金属学报, 2019, 55(12): 1551-1560.
[6] Yin BAI, Zhengdong LIU, Jianxin XIE, Hansheng BAO, Zhengzong CHEN. Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel[J]. 金属学报, 2018, 54(6): 895-904.
[7] Bing CHEN,Changyuan GAO,Jiao HUANG,Yajing MAO,Meiyi YAO,Jinlong ZHANG,Bangxin ZHOU,Qiang LI. Corrosion Behavior of Second Phase Alloys of β-(Nb, Zr) in Deionized Water at 360 ℃[J]. 金属学报, 2017, 53(4): 447-454.
[8] Hongxi LIU,Zhengxue LI,Xiaowei ZHANG,Jun TAN,Yehua JIANG. Effect of Heat Treatment on High-Temperature Oxidation Resistance of High Niobium Ti-Al Intermetallic Coating Fabricated by Laser In Situ Synthesis on Titanium Alloy[J]. 金属学报, 2017, 53(2): 201-210.
[9] Wenying ZHANG, Jun LI, Bo ZHOU. OXIDATION KINETICS BEHAVIOR AND ELECTRICAL PROPERTY OF MnCO2O4 SPINEL AS A COATING MATERIAL FOR METALLIC INTERCONNECTS[J]. 金属学报, 2016, 52(3): 355-360.
[10] Boyang WANG,Bangxin ZHOU,Zhen WANG,Jiao HUANG,Meiyi YAO,Jun ZHOU. CORROSION RESISTANCE OF Zr-0.72Sn-0.32Fe- 0.14Cr-xNb ALLOYS IN 500 ℃ SUPERHEATED STEAM[J]. 金属学报, 2015, 51(12): 1545-1552.
[11] ZHANG Haixia, LI Zhongkui, ZHOU Lian, XU Bingshe, WANG Yongzhen. EFFECTS OF STRUCTURE AND INTERNAL STRESSES IN OXIDE FILMS ON CORROSION MECHANISM OF NEW ZIRCONIUM ALLOY[J]. 金属学报, 2014, 50(12): 1529-1537.
[12] LUO Lei, SHEN Yifu, LI Bo, HU Weiye. PREPARATION AND OXIDATION BEHAVIOR OF ALUMINIZED COATING ON TC4 TITANIUM ALLOY VIA FRICTION STIR LAP WELDING METHOD[J]. 金属学报, 2013, 49(8): 996-1002.
[13] WEI Tianguo, LONG Chongsheng, MIAO Zhi, LIU Yunming,LUAN Baifeng. CORROSION BEHAVIOR OF Zr-0.4Fe-1.0Cr-x Mo ALLOYS IN 500℃ and 10.3 MPa STEAM[J]. 金属学报, 2013, 49(6): 717-724.
[14] ZHANG Jinlong, XIE Xingfei, YAO Meiyi, ZHOU Bangxin,PENG Jianchao,LIANG Xue. STUDY ON THE CORROSION RESISTANCE OF Zr-1Nb-0.7Sn-0.03Fe-xGe ALLOY IN LITHIATED WATER AT 360 ℃[J]. 金属学报, 2013, 29(4): 443-450.
[15] YAO Meiyi ZOU Linghong XIE Xingfei ZHANG Jinlong PENG Jianchao ZHOU Bangxin. EFFECT OF Bi ADDITION ON THE CORROSION RESISTANCE OF Zr-4 IN SUPERHEATED STEAM AT 400 ℃/10.3 MPa[J]. 金属学报, 2012, 48(9): 1097-1102.
No Suggested Reading articles found!