| CONSTITUTIVE RELATIONSHIPS OF Nb MICROALLOYED STEEL DURING HIGH TEMPERATURE DEFORMATION |
| JIA Bin, PENG Yan |
| State Key Laboratory of Metastable Materials Science and Technology, Engineering Research Center of Rolling Equipment and Complete Technology of Ministry of Education, Yanshan University, Qinhuangdao 066004 |
|
Cite this article:
JIA Bin PENG Yan. CONSTITUTIVE RELATIONSHIPS OF Nb MICROALLOYED STEEL DURING HIGH TEMPERATURE DEFORMATION. Acta Metall Sin, 2011, 47(4): 507-512.
|
|
|
Abstract The flow stress curves of Nb microalloyed steel Q345B during hot compression deformation were obtained on Gleeble-3500 thermo-simulation machine. Based on the experimental results, the constitutive model of Nb microalloyed steel during high temperature deformation was established to describe the stress-strain relationship during dynamic softening (dynamic recovery and dynamic recrystallization) and in the steady flow state, in which the influences of the thermal deformation parameters (strain rate and deformation temperature) and dynamic softening mechanism (dynamic recovery and dynamic recrystallization) on the flow stress were considered. A method was provided to solve constitutive equation and establish the mathematic expressions of the correlation coefficients. It is shown that the predicted results by the model are in good agreement with the experimental ones.
|
|
Received: 13 January 2011
|
| Fund: Supported by High Technology Research and Development Program of China (No.2009AA04Z143) and Program for New Century Excellent Talents in
University (No.NCET-09-0117) |
| [1] Qi J J. Microalloyed Steels. Beijing: Metallurgy Industry Press, 2006: 1(齐俊杰. 微合金化钢. 北京: 冶金工业出版社, 2006: 1)[2] Tamura I, translated byWang G D. Controlled Rolling and Controlled Cooling of HSLA Steels. Beijing: Metallurgy Industry Press, 1992: 4(田村今男, 王国栋译. 高强度低合金钢的控制轧制与控制冷却. 北京: 冶金工业出版社, 1992: 4)[3] Ebranimi R, Zahiri S H, Najafizadeh A. J Mater Process Technol, 2006; 171: 301[4] Wang M, Hong H P, Wang X M. J Wuhan Univ Sci Technol, 1999; 33: 134(王孟, 洪慧平, 王晓明. 武汉科技大学学报, 1999; 33: 134)[5] Lin Y C, Chen M S, Zhong J. J Cent South Univ (Sci Technol), 2008; 39: 549(蔺永诚, 陈明松, 钟掘. 中南大学学报(自然科学版), 2008; 39: 549)[6] Xu G, Xu C S, Zhao J R. ISIJ Int, 2006; 46: 166[7] Nakata N, Militzer M. ISIJ Int, 2005; 45: 82[8] Najafizadeh A, Jonas J J. ISIJ Int, 2005; 46: 1679[9] Lin W, Li H Y, Zeng C T, Bin J, Wei D D. J Cent South Univ (Sci Technol), 2010; 41: 940(林武, 李红英, 曾翠婷, 宾杰, 魏冬冬. 中南大学学报(自然科学版), 2010; 41: 940)[10] Zhang H Y, Zhang H B, Chen H S. Mater Mech Eng, 2007; 31: 92(张红英, 张鸿冰, 陈浩时. 机械工程材料, 2007; 31: 92)[11] Pu Z J. Mater Sci Eng, 1995; A192: 780[12] Laasraoui A, Jonas J J. Metall Trans, 1991; 22A: 1545[13] He Y Z, Chen D H, Lei T Q. Iron Steel, 1999; 34: 29(何宜柱, 陈大宏, 雷廷权. 钢铁, 1999; 34 : 29)[14] Suh D W, Cho J Y, Oh K H, Lee H C. ISIJ Int, 2002; 42: 564[15] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. Oxford: Pergamon Press, 1995: 363[16] Yoshie A, Fujita T, Fujioka M, Okamoto K, Morikawa H. ISIJ Int, 1996; 36: 474[17] Minami K, Siciliano Jr F, Maccagno, T M, Jonas J J. ISIJ Int, 1996; 36: 1507[18] Hodgson P D, Gibbs R K. ISIJ Int, 1992; 32: 1329[19] Manohar P A, Kyuhwan L, Rollett A D, Youngseog L. ISIJ Int, 2003; 43: 1421[20] Ma B, Peng Y, Liu Y F, Jia B. Trans Mater Heat Treat, 2010; 31: 141(马博, 彭艳, 刘云飞, 贾斌. 材料热处理学报, 2010; 31: 141) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|