SPALLING OF NITRIDED LAYER OF AUSTENITIC STEEL 4Cr14Ni14W2Mo
LI Jian;Professor;Northeast University of Technotogy;Shenyang;SUN Xudong;LI Zaixian;LI Chunsheng Northeast University of Technology
Cite this article: 

LI Jian;Professor;Northeast University of Technotogy;Shenyang;SUN Xudong;LI Zaixian;LI Chunsheng Northeast University of Technology. SPALLING OF NITRIDED LAYER OF AUSTENITIC STEEL 4Cr14Ni14W2Mo. Acta Metall Sin, 1988, 24(1): 47-50.

Download:  PDF(1700KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The tendency of spalling of nitrided layer of an austenitic heatresistant steel 4Cr14Ni14W2Mo has been studied experimentally. It was found thatthe residual deformation retained in the rolled steel is the root that causes thespalling of nitrided layer of the steel. If the work hardening state is removed by asuitable heat treatment before nitriding, the spalling of nitrided layer can be com-pletely avoided.
Key words:  nitriding      spalling      heat resistant steel     
Received:  18 January 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I1/47

1 Unthank D C, Driver J H. Jack K H. Met Sci, 1974; 8: 209
2 Kindlimann L E. Ansell G S. Metall Trans, 1970; 1: 163
3 高濑孝夫.多属,1958; 28 (6) : 424
4 Briant C L, Banerji S K. Int Metall Rev, 1978; 23 (4) : 164l
[1] WANG Haifeng, ZHANG Zhiming, NIU Yunsong, YANG Yange, DONG Zhihong, ZHU Shenglong, YU Liangmin, WANG Fuhui. Effect of Pre-Oxidation on Microstructure and Wear Resistance of Titanium Alloy by Low Temperature Plasma Oxynitriding[J]. 金属学报, 2023, 59(10): 1355-1364.
[2] QIU Longshi, ZHAO Jing, PAN Xiaolong, TIAN Feng. Interfacial Fatigue Spalling Behavior of TiN Films on High Speed Steel[J]. 金属学报, 2021, 57(8): 1039-1047.
[3] ZHAO Manman, QIN Sen, FENG Jie, DAI Yongjuan, GUO Dong. Effect of Al and Ni on Hot Deformation Behavior of 1Cr9Al(1~3)Ni(1~7)WVNbB Steel[J]. 金属学报, 2020, 56(7): 960-968.
[4] LI Kejian, ZHANG Yu, CAI Zhipeng. Fracture Location Shift of Dissimilar Metal Welds Under Coupled Thermal-Stress Effect[J]. 金属学报, 2020, 56(11): 1463-1473.
[5] YANG Ke,LIANG Ye,YAN Wei,SHAN Yiyin. Preferential Distribution of Boron and its Effect on Microstructure and Mechanical Properties of (9~12)%Cr Martensitic Heat Resistant Steels[J]. 金属学报, 2020, 56(1): 53-65.
[6] Guimin ZENG,Haiwen LUO,Jun LI,Jian GONG,Xianhao LI,Xianhui WANG. Experimental Studies and Numerical Simulation on the Nitriding Process of Grain-Oriented Silicon Steel[J]. 金属学报, 2017, 53(6): 743-750.
[7] CAO Tieshan, FANG Xudong, CHENG Congqian, ZHAO Jie. CREEP BEHAVIOR OF TWO KINDS OF HR3C HEAT RESISTANT STEELS BASED ON STRESS RELAXATION TESTS[J]. 金属学报, 2014, 50(11): 1343-1349.
[8] ZHENG Leigang, HU Xiaoqiang, KANG Xiuhong, LI Dianzhong. PRECIPITATION BEHAVIOR OF M23C6 AND ITS EFFECTS ON DUCTILITY AND TOUGHNESS OF A NOVEL Cr-Mn-N AUSTENITIC HEAT RESISTANT STEEL[J]. 金属学报, 2013, 49(9): 1081-1088.
[9] LI Xunping ZHOU Minbo XIA Jianmin MA Xiao ZHANG Xinping. EFFECT OF THE CROSS-INTERACTION ON THE FORMATION AND EVOLUTION OF INTERMETALLIC COMPOUNDS IN Cu(Ni)/Sn-Ag-Cu/Cu(Ni) BGA STRUCTURE SOLDER JOINTS[J]. 金属学报, 2011, 47(5): 611-619.
[10] CHI Chengyu DONG Jianxin LIU Wenqing XIE Xishan. 3DAP INVESTIGATION OF PRECIPITATION BEHAVIOR OF Cu-RICH PHASE IN SUPER304H HEAT RESISTANT STEEL[J]. 金属学报, 2010, 46(9): 1141-1146.
[11] ;. Preparation of Ti(CxN1-x) thick films on titanium by plasma electrolytic carbonitriding[J]. 金属学报, 2008, 44(9): 1105-1110 .
[12] Cao Jin-Rong. The influence of strain rate and temperature on flow stress and critical dynamic recrystallisation of T122 steel[J]. 金属学报, 2007, 42(1): 35-40 .
[13] SU Hang; JI Huaizhong; ZHANG Yongquan; YANG Caifu; LIU Tong. Simulation of Friction Heat Induced Phase Transformation in High Speed Train Wheel[J]. 金属学报, 2004, 40(9): 909-914 .
[14] LI Fengzhao;DAI Jiyan;LI Douxing Shandong Polytechnic University; Jinan; Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinica; Shenyang Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Academia Sinica; ShenyangSUN Dongsheng;assoeiate professor.Institute of Materials Engineering.Shandong Polytechnic University ;Jinan 250014. CRYSTAL DEFECTS AND INTERFACE STRUCTURE OF ION-NITRIDED LAYERS[J]. 金属学报, 1993, 29(5): 11-15.
[15] LIU Wei;WANG Qun;ZHAO Xinguo;ZHAO Tong;ZHANG Zhidong;SUN Xiaokai Institute of Metal Research; Academia Sinica; Shenyang research assistant; Institute of Metal Research; Academia Sinica; Shenyang 110015. PREPARATION OF HIGH COERCIVE Sm-Fe-N PERMANENT MAGNET[J]. 金属学报, 1993, 29(3): 80-83.
No Suggested Reading articles found!