| EFFECT OF MICROSTRUCTURES ON THE YIELD STRENGTH AND SCR OF 7075 ALUMINIUM ALLOY |
| HUA Mingjian Institute of Aeronoutical Materials;Beijing;Post Box NO.81;LI Chunzhi;WANG Hongjian Institute of Aeronautical Materials; Beijing |
|
Cite this article:
HUA Mingjian Institute of Aeronoutical Materials;Beijing;Post Box NO.81;LI Chunzhi;WANG Hongjian Institute of Aeronautical Materials; Beijing. EFFECT OF MICROSTRUCTURES ON THE YIELD STRENGTH AND SCR OF 7075 ALUMINIUM ALLOY. Acta Metall Sin, 1988, 24(1): 41-46.
|
|
|
Abstract The microstructures of T6, CgS3 and T73 aged 7075 aluminiumalloy have been investigated using TEM and related to the yield strength and thestress-corrosion resistance (SCR) of the alloy, which were shown to be affectedmainly by the type, size and density of matrix precipitates (MPt). After aged bythe newlydeveloped CgS3 process, the majority of MPt is η' transition phase withabout 5×10~(16)/cm~3 in volume density and 5-7nm in size. The alloy subsequentlyshows an optimum combination of yield strength and SCR, which has been attributed to the increased tendency of dislocations by-passing MPt particles.
|
|
Received: 18 January 1988
|
1 李春志.金属学报,1985;21:B233 2 Allen S M. Phil. Mag., 1981; 43: 325 3 Adler P, DeIasi R, Geschwind G. AD732321. Nov. 1971 4 Speidel M O. In: Scully J C ed. The Theory of SCC in Alloys, Erussel: NATC Sci, Affairs Division. 1971: 289 5 Hirsch P B, Humphreys F J. Physics of Strength and Plasticity. MIT Press, 1969: 189 6 Gerold V, Haberkorn V. Phys. Status Solidi, 1960; 16: 675 7 Park J K, Ardell A J. Metall Trans, 1983; 14A: 1957 8 Hua Mingjian, Li Chunzhi, Yan Minggao. In: the Secretariate of BCEIA ed. Froc. of Beijing Conf. and Exhibition on Instrumental Analysis, Beijing, Nov. 1985: Vol. 1, 102r |