| SPALLING OF NITRIDED LAYER OF AUSTENITIC STEEL 4Cr14Ni14W2Mo |
| LI Jian;Professor;Northeast University of Technotogy;Shenyang;SUN Xudong;LI Zaixian;LI Chunsheng Northeast University of Technology |
|
Cite this article:
LI Jian;Professor;Northeast University of Technotogy;Shenyang;SUN Xudong;LI Zaixian;LI Chunsheng Northeast University of Technology. SPALLING OF NITRIDED LAYER OF AUSTENITIC STEEL 4Cr14Ni14W2Mo. Acta Metall Sin, 1988, 24(1): 47-50.
|
|
|
Abstract The tendency of spalling of nitrided layer of an austenitic heatresistant steel 4Cr14Ni14W2Mo has been studied experimentally. It was found thatthe residual deformation retained in the rolled steel is the root that causes thespalling of nitrided layer of the steel. If the work hardening state is removed by asuitable heat treatment before nitriding, the spalling of nitrided layer can be com-pletely avoided.
|
|
Received: 18 January 1988
|
1 Unthank D C, Driver J H. Jack K H. Met Sci, 1974; 8: 209 2 Kindlimann L E. Ansell G S. Metall Trans, 1970; 1: 163 3 高濑孝夫.多属,1958; 28 (6) : 424 4 Briant C L, Banerji S K. Int Metall Rev, 1978; 23 (4) : 164l |
| No Suggested Reading articles found! |
|
|