Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (2): 221-222    DOI:
Current Issue | Archive | Adv Search |
POSITRON ANNIHILATION STUDY OF HEAT TREATMENT PROCESS IN Fe-22 at.-% Al
WANG Jingcheng;LIU Dajun Shanghai Iron and Steel Research Institute
Cite this article: 

WANG Jingcheng;LIU Dajun Shanghai Iron and Steel Research Institute. POSITRON ANNIHILATION STUDY OF HEAT TREATMENT PROCESS IN Fe-22 at.-% Al. Acta Metall Sin, 1988, 24(2): 221-222.

Download:  PDF(207KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Specimens of Fe-22 at-%Al subjected to different heat treatment process have beenstudied using Doppler broadening measurements. The calculated data according to the trappingmodel was shown to be in good agreement with the measured, shape parameter. The microstruc-tural change during each stage of heating and cooling has been discussed in relation to the shapeparameter, which indicates that positron annihilation data is valuable for establishing the prac-tical heat treatment process of the alloy.
Key words:  positron annihilation      Fe-Al alloy      heat treatment process     
Received:  18 February 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I2/221

1 Bergersen B, Stott M I. Solid State Commun 969; 7: 1208
2 Oki K, Hasaka M, Eguchi T. Jpn J Appl Phys, 1973; 12: 1522
3 Liu Dajun. J Magn Magn Mater, 1982; 26: 217
4 山中和夫,井野博满.日本金属学会志,1971;35,(6) :566
[1] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
[2] TIAN Xuefen, LIU Xiang, GONG Min, ZHANG Peiyuan, WANG Kang, DENG Aihong. Defect Evolution in H/He Neutral Beam Irradiated W-ZrC Alloy Using Positron Annihilation Spectroscopy[J]. 金属学报, 2021, 57(1): 121-128.
[3] WAN Xiangliang, HU Feng, CHENG Lin, HUANG Gang, ZHANG Guohong, WU Kaiming. Influence of Two-Step Bainite Transformation on Toughness in Medium-Carbon Micro/Nano-Structured Steel[J]. 金属学报, 2019, 55(12): 1503-1511.
[4] Tianci ZHANG, Haitao WANG, Zhengcao LI, Henk SCHUT, Zhengming ZHANG, Ming HE, Yuliang SUN. Positron Annihilation Investigation of Embrittlement Behavior in Chinese RPV Steels after Fe-Ion Irradiation[J]. 金属学报, 2018, 54(4): 512-518.
[5] Kang WANG,Aihong DENG,Min GONG,Xiaobo LU,Yuanyuan ZHANG,Xiang LIU. Effect on Microstructure of Tungsten Under Helium Ions Irradiation with Multiple Energy[J]. 金属学报, 2017, 53(1): 70-76.
[6] Changji LI,Liangyin XIONG,Shi LIU. EFFECT OF THE INTERMEDIATE HEAT TREATMENT PROCESSES ON THE OXIDATION CHARACTERIS- TICS OF Zr-1Nb-0.2Y ALLOY IN 420 ℃ AIR[J]. 金属学报, 2016, 52(1): 85-92.
[7] LIU Yang, XIANG Wei, WANG Boyu. EFFECT OF IRRADIATION WITH PULSED ION BEAM ON THE MICROSTRUCTURE OF TiH2[J]. 金属学报, 2013, 49(10): 1269-1274.
[8] WANG Xiaoyong, PAN Tao, WANG Hua, SU Hang,LI Xiangyang, CAO Xingzhong. INVESTIGATION OF THE TOUGHNESS OF LOW CARBON TEMPERED MARTENSITE IN THE SURFACE OF Ni-Cr-Mo-B ULTRA-HEAVY PLATE STEEL[J]. 金属学报, 2012, 48(4): 401-406.
[9] WANG Boyu XIANG Wei TAN Xiaohua DAI Jingyi CHENG Liang QIN Xiubo. EFFECT OF D+ BEAM IRRADIATION ON Ti FILM[J]. 金属学报, 2010, 46(7): 810-813.
[10] WEI Shitong LU Shanping HE Guangzhong ZHAO Xu LI Dianzhong LI Yiyi . EFFECTS OF HEAT TREATMENT ON THE MICROSTRUCTURE AND MECHANICAL PROPERTY OF WELD METAL WITH Nb ADDITION[J]. 金属学报, 2009, 45(9): 1063-1069.
[11] SUN Wei. The internal friction peak correlated to the relaxation of Al antisite atoms in Fe-Al alloys[J]. 金属学报, 2007, 43(3): 311-314 .
[12] ZHANG Lanzhi; WANG Baoyi; WANG Danni; WEI Long; LIN Junpin; WANG Wenjun. STUDIES OF Nb–TiAl ALLOY BY POSITRON ANNIHILATION TECHNIQUES[J]. 金属学报, 2007, 43(3): 269-272 .
[13] Jian Zhang. STUDY OF HYDROGEN EMBRITLLEMENT IN Fe-Ni BASED ALLOY THROUGH POSITRON ANNIHILATION LIFETIME TEST[J]. 金属学报, 2006, 42(5): 469-473 .
[14] DENG Wen; RUAN Xiangdong; HUANG Yuyang; ZHOU Yin'e; ZHU Yingying; ZHU Yingying. Effects Of Twin Size On The Dislocation Configuration During Cyclic Deformation Of Polycrystalline Twin Copper[J]. 金属学报, 2005, 41(1): 33-.
[15] JIA Wei;XIONG Lianggue;ZENG Meiguang;WANG Jiangiang (Department of Materials Science; College of Science; Northeastern University; Shenyang 110006)(International Center for Materials Physics; Institute of Matal Research; The Chinese Academy of Sciences;Shenyang 110015). POSITRON ANNIHILATION STUDY ON THE EFFECT OF MISCH METAL IN Al-Fe-V-Si-Mm ALLOYS[J]. 金属学报, 1998, 34(2): 221-224.
No Suggested Reading articles found!