Abstract Specimens of Fe-22 at-%Al subjected to different heat treatment process have beenstudied using Doppler broadening measurements. The calculated data according to the trappingmodel was shown to be in good agreement with the measured, shape parameter. The microstruc-tural change during each stage of heating and cooling has been discussed in relation to the shapeparameter, which indicates that positron annihilation data is valuable for establishing the prac-tical heat treatment process of the alloy.
|
|
Received: 18 February 1988
|
1 Bergersen B, Stott M I. Solid State Commun 969; 7: 1208 2 Oki K, Hasaka M, Eguchi T. Jpn J Appl Phys, 1973; 12: 1522 3 Liu Dajun. J Magn Magn Mater, 1982; 26: 217 4 山中和夫,井野博满.日本金属学会志,1971;35,(6) :566 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|