DIFFUSION OF HYDROGEN IN (α+γ) DUPLEX STAINLESS STEEL
HE Jianhong;TANG Xiangyun;CHEN Nanping Tsinghua University; Beijing
Cite this article: 

HE Jianhong;TANG Xiangyun;CHEN Nanping Tsinghua University; Beijing. DIFFUSION OF HYDROGEN IN (α+γ) DUPLEX STAINLESS STEEL. Acta Metall Sin, 1989, 25(1): 42-47.

Download:  PDF(410KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The permeation curves of hydrogen in (α+γ) duplex stainless steelhave been electrochemically determined. The apparent diffusivity of hydrogen de-pends on the austenite content (fγ) at room temperature, D=(0.27+0.9/f_γ~2) (10~(-10)cm~2/s). It is simply verified that hydrogen in (α+γ) duplex stainless steel diffusesin "series-connection" form through both ferrite and austenite, the apparent diffu-sivity is D≈D_αD_γ/(f_α~2D_γ+f_γ~2D_α), where D_αD_γare respectively diffusivity of hydrogenin ferrite and austenite, f_α,f_γare volume fraction, in turn, of ferrite and aus-tenite.
Key words:  hydrogen      diffusion      duplex stainless steel     
Received:  18 January 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I1/42

1 McNabb A. Foster P K. TMS-AIME. 1963; 227: 618
2 何建宏,唐祥云,陈南平.金属学报,1989;25:A39
3 姚录安,周仲柏,陶映初.武汉大学学报(自然科学版),1980;(1) :76
4 Crank J. The Mathematics of Diffusion Oxford: Clarendon Press, 1956: 51
5 Sakamoto Y. Trans Jpn Inst Met, 1984: 25: 244
6 Gonzalez O D. TMS-AIME, 1969; 245: 607
7 Thomas G J. In: Bernstein I M, Thompson A W eds., Hydrogen Effects in Metals, New York: TMS AIME, 1980: 77
8 Oriani R A. Acta Met, 1970; 18: 147
9 何建宏,唐祥云,马莒生.稀有金属,1987;6:8
10 McLellan R B. Acta Met, 1979; 27: 1655
11 McLellan R B. Scr Met, 1981; 15: 1251
12 Yoshihara M, McLellan R B. Acta Met, 1982; 30: 1605
13 胡赓祥,钱苗根,金属学,上海科学技术出版社,1980:112
14 Namboodhiri T K G, Nanis L. Acta Met. 1973; 21: 663
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] LI Qian, SUN Xuan, LUO Qun, LIU Bin, WU Chengzhang, PAN Fusheng. Regulation of Hydrogen Storage Phase and Its Interface in Magnesium-Based Materials for Hydrogen Storage Performance[J]. 金属学报, 2023, 59(3): 349-370.
[3] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[4] LIU Lujun, LIU Zheng, LIU Renhui, LIU Yong. Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process[J]. 金属学报, 2023, 59(11): 1457-1465.
[5] DU Zonggang, XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng. Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine[J]. 金属学报, 2023, 59(10): 1335-1345.
[6] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
[7] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[8] LI Xifeng, LI Tianle, AN Dayong, WU Huiping, CHEN Jieshi, CHEN Jun. Research Progress of Titanium Alloys and Their Diffusion Bonding Fatigue Characteristics[J]. 金属学报, 2022, 58(4): 473-485.
[9] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[10] HUA Yu, CHEN Jianguo, YU Liming, SI Yonghong, LIU Chenxi, LI Huijun, LIU Yongchang. Microstructure Evolution and Mechanical Properties of Dissimilar Material Diffusion-Bonded Joint for High Cr Ferrite Heat-Resistant Steel and Austenitic Heat-Resistant Steel[J]. 金属学报, 2022, 58(2): 141-154.
[11] LIU Zhongwu, HE Jiayi. Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets[J]. 金属学报, 2021, 57(9): 1155-1170.
[12] XIAO Na, HUI Weijun, ZHANG Yongjian, ZHAO Xiaoli. Hydrogen Embrittlement Behavior of a Vacuum-Carburized Gear Steel[J]. 金属学报, 2021, 57(8): 977-988.
[13] CHEN Shenghu, RONG Lijian. Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic[J]. 金属学报, 2021, 57(8): 989-999.
[14] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
[15] LAN Liangyun, KONG Xiangwei, QIU Chunlin, DU Linxiu. A Review of Recent Advance on Hydrogen Embrittlement Phenomenon Based on Multiscale Mechanical Experiments[J]. 金属学报, 2021, 57(7): 845-859.
No Suggested Reading articles found!