AUGER STUDY OF CARBON LAYER ON ION IMPLANTED STEEL SURFACE
YU Zhenjiang;YANG Dequan;XIE Xie;YAN Rongxin;FAN Chuizhen Lanzhou Institute of Physics Ministry of Aeronautical Industry
Cite this article: 

YU Zhenjiang;YANG Dequan;XIE Xie;YAN Rongxin;FAN Chuizhen Lanzhou Institute of Physics Ministry of Aeronautical Industry. AUGER STUDY OF CARBON LAYER ON ION IMPLANTED STEEL SURFACE. Acta Metall Sin, 1989, 25(2): 143-145.

Download:  PDF(236KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The carbon layers on implanted Steel surface have been studied by means of Augerspectra. It is showed that the thickness of the carbon layer is proportional to the dose of implant-ed ions. By comparison with the results of friction and wear tests, we found that the frictioncoefficient is smaller than 0.20 at the first part of the friction coefficient curve. It is consideredthat the graphitic carbon layer on the top of the steel is helpful to reducing the surface frictioncoefficient of the steel.
Key words:  nitrogen ion implantation      carbon layer on surface      GCr15      wear resistance     
Received:  18 February 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I2/143

1 Prabhawalkar P D, Raole P M. Vacuum, 1986; 36 (11--12) : 817
2 余镇江,杨德全,谢燮,阎荣鑫,王珍,范垂祯.真空,1988;(1) :22
3 Singer I L, Barlak T M. Appl Phys Lett, 1983; 43 (5) : 457
3 Ktal J, Zemek J. Vacuum, 1986; 36 (11--12) : 55
[1] WANG Haifeng, ZHANG Zhiming, NIU Yunsong, YANG Yange, DONG Zhihong, ZHU Shenglong, YU Liangmin, WANG Fuhui. Effect of Pre-Oxidation on Microstructure and Wear Resistance of Titanium Alloy by Low Temperature Plasma Oxynitriding[J]. 金属学报, 2023, 59(10): 1355-1364.
[2] ZHANG Yu, LOU Liyan, XU Qinglong, LI Yan, LI Changjiu, LI Chengxin. Microstructure and Wear Resistance of Ni-Based WC Coating by Ultra-High Speed Laser Cladding[J]. 金属学报, 2020, 56(11): 1530-1540.
[3] Hulin DONG,Haiping BAO,Jianhong PENG. Effect of TiC Contents on Mechanical Properties and Wear Resistance of Iron-Based Composites[J]. 金属学报, 2019, 55(8): 1049-1057.
[4] Yuan HOU, Zhongming REN, Jiang WANG, Zhenqiang ZHANG, Xia LI. Effect of Longitudinal Static Magnetic Field on the Columnar to Equiaxed Transition in Directionally Solidified GCr15 Bearing Steel[J]. 金属学报, 2018, 54(5): 801-808.
[5] Shilu ZHAO,Zhen ZHANG,Jun ZHANG,Jianming WANG,Zhenggui ZHANG. MICROSTRUCTURE AND WEAR RESISTANCE OF TiAlZrCr/(Ti, Al, Zr, Cr)N GRADIENT FILMS DEPOSITED BY MULTI-ARC ION PLATING[J]. 金属学报, 2016, 52(6): 747-754.
[6] Wenfang CUI,Dong CAO,Gaowu QIN. MICROSTRUCTURE AND WEAR RESISTANCE OF Ti/TiN MULTILAYER FILMS DEPOSITED BY MAGNETRON SPUTTERING[J]. 金属学报, 2015, 51(12): 1531-1537.
[7] LIU Xiaobo, ZHAO Yuguang. MICROSTRUCTURE EVOLUTION AND WEAR RESISTANCE OF IN SITU Mg2Si/Al COMPOSITES UNDER DIFFERENT PREPARATION CONDITIONS[J]. 金属学报, 2014, 50(6): 753-761.
[8] LIU Hongji, SUN Junjie, JIANG Tao, GUO Shengwu, LIU Yongning, LIN Xin. ROLLING CONTACT FATIGUE BEHAVIOR OF AN ULTRAHIGH CARBON STEEL[J]. 金属学报, 2014, 50(12): 1446-1452.
[9] NIU Yunsong, WEI Jie, ZHAO Jian, HU Jiaxiu, YU Zhiming. PREPARATION AND PROPERTIES OF NANOSIZED MUL-TILAYERED Ni COATINGS BY ULTRASOUND-ASSISTED ELECTRODEPOSITION[J]. 金属学报, 2013, 49(12): 1617-1622.
[10] YU Yipeng HUANG Jinfeng CUI Hua CAI Yuanhua ZHANG Jishan. EFFECT OF Nb ON THE MICROSTRUCTURE AND PROPERTIES OF SPRAY FORMED M3 HIGH SPEED STEEL[J]. 金属学报, 2012, 48(8): 935-940.
[11] ZHANG Fenggang ZHU Xiaopeng WANG Mingyang LEI Mingkai. SURFACE MODIFICATION OF WC-Ni CEMENTED CARBIDE FOR SEALS BY HIGH-INTENSITY PULSED ION BEAM IRRADIATION[J]. 金属学报, 2011, 47(7): 958-964.
[12] WANG Yanqiu WANG Yue CHEN Paiming SHAO Yawei WANG Fuhui. MICROSTRUCTURE, CORROSION AND WEAR RESISTANCES OF MICROARC OXIDATION COATING ON Al ALLOY 7075[J]. 金属学报, 2011, 47(4): 455-461.
[13] LEI Mingkai WANG Kesheng OU Yi Xiang ZHANG Lei. PLASMA–BASED LOW–ENERGY NITROGEN ION IMPLANTATION OF 2Cr13 MARTENSITIC STAINLESS STEEL USED IN PUMPS AND VALVES[J]. 金属学报, 2011, 47(12): 1490-1494.
[14] LU Liantao LI Wei ZHANG Jiwang SHIOZAWA Kazuaki ZHANG Weihua. ANALYSIS OF ROTARY BENDING GIGACYCLE FATIGUE PROPERTIES OF BEARING STEEL GCr15[J]. 金属学报, 2009, 45(1): 73-78.
[15] LI Jian; MAO Dongsheng; HUANG Liping; GUO Shaoyi; MAO Zhiyuan(Department of Materials Science and Engineering; Zhejiang University Hangzhou 310027Ion Beam Laboratory; Shanghai Institute of Metallurgy The Chinese Academy of Sciences; Shanghai 200050). PROPERTIES AND ABRASION WEAR RESISTANCE OF AN Al_2O_3-TiC-Co MODIFIED CERAMIC[J]. 金属学报, 1998, 34(3): 332-336.
No Suggested Reading articles found!