| PREPARATION OF LN_2 TEMPERATURE REGION SUPERCONDUCTOR FILM ON Si(100) SUBSTRATE |
| HU Qingyu;ZHAO Hangwei;WEN Lishi;WANG Yongzhong;QIAO Guiwen Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
HU Qingyu;ZHAO Hangwei;WEN Lishi;WANG Yongzhong;QIAO Guiwen Institute of Metal Research; Academia Sinica; Shenyang. PREPARATION OF LN_2 TEMPERATURE REGION SUPERCONDUCTOR FILM ON Si(100) SUBSTRATE. Acta Metall Sin, 1989, 25(3): 152-154.
|
|
|
Abstract We report the experimental results of the prepartion of YBaCuO superconductorthin film on Si (100) substrate by the method of ion beam sputtering deposition. A ZrO_2 buf-fer layer was applied to Si (100) substrate, and was found to play an important role in resist-ing the diffusion of Si toward the film. The thin film is mainly a 123 phase with strong c-axispreferred orentation. The onset transition temperature of the film is 100 K and the finaltransition temperature 78 K.
|
|
Received: 18 March 1989
|
1 郑家琪,中国真空学会第3届年会学术论文集,沈阳,1988;122 2 Mogro-Campero, A, Hunt B D, Turner L G, Burrell M C, Balz W E. High Temperature Superconductor Ⅱ. Extended Abstracts, Materials Research Society of America, 1988: 113 3 胡倾宇,闻立时,赵航炜,乔桂文,钱声伟,于宝海,杨巧勤,庄育智.材料科学进展,1989;3:233 4 胡倾宇,钱声伟,闻立时,于宝海,赵航炜,杨巧勤,关侃,傅立顺.低温物理学报,1987;9(3) :19 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|