CONSTRUCTION OF COMPLETE POLE FIGURE FROM AN INCOMPLETE ONE
ZUO Liang;XU Jiazheng;LIANG Zhide Northeast University of Technology; Shenyang
Cite this article:
ZUO Liang;XU Jiazheng;LIANG Zhide Northeast University of Technology; Shenyang. CONSTRUCTION OF COMPLETE POLE FIGURE FROM AN INCOMPLETE ONE. Acta Metall Sin, 1989, 25(3): 149-151.
Abstract Arbitrary incomplete measured pole figure (except that of {100}) of cubic materi-als can be completed by using the fundamental equations of the vector method and employingthe measured data as constraint conditions. The prediction of this method is in good agreementwith experimental results, and the analysing procedure has been proved to be simple and ef-ficient.